Method with welding residual stress control and crack prevention functions

The invention discloses a method with welding residual stress control and crack prevention functions, which comprises the following steps of: before welding, determining preheating temperature and heat preservation time according to the strength of a workpiece material, a stress state, a welding met...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANG XUNLIANG, LI GUANGJUN, MENG XIANGYI, LIN CHANGJIU, LIU JINGANG, ZHAO MAPING, ZHANG XU, WEI SHENG, WANG ZHIQIANG, HU GUOMIN, HUANG CUNCHAO, LI DONG, WANG MINFENG, ZHU HUAXUE
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YANG XUNLIANG
LI GUANGJUN
MENG XIANGYI
LIN CHANGJIU
LIU JINGANG
ZHAO MAPING
ZHANG XU
WEI SHENG
WANG ZHIQIANG
HU GUOMIN
HUANG CUNCHAO
LI DONG
WANG MINFENG
ZHU HUAXUE
description The invention discloses a method with welding residual stress control and crack prevention functions, which comprises the following steps of: before welding, determining preheating temperature and heat preservation time according to the strength of a workpiece material, a stress state, a welding method and welding parameters; the annular large-wall-thickness welding seam of the workpiece material is subjected to segmented welding; repeated multi-pass welding is adopted for midway welding, a final plugging section is reserved, and welding is conducted; in the welding process, real-time temperature monitoring is conducted on a welding area, welding parameters are adjusted according to real-time temperature data, and the welding temperature and the welding speed are controlled; and after welding, a welding joint is cooled. The method is used for solving the technical problems that an existing method for controlling the welding stress and preventing the welding cracks cannot well adapt to the welding requirements
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116372313A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116372313A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116372313A3</originalsourceid><addsrcrecordid>eNqNyrEKwjAQgOEsDqK-w_kAHWJAZylKEXRyL0dytcFwCbmrfX0VfACn_xv-pblcScccYI46wkwpRH5AJYlhwgSiHwr4zFpzAuQAvqJ_Qqn0ItaYGYaJ_ReyNosBk9Dm15XZnk_3tmuo5J6koCcm7dubtXt32Dnrju6f5w1j_jWm</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method with welding residual stress control and crack prevention functions</title><source>esp@cenet</source><creator>YANG XUNLIANG ; LI GUANGJUN ; MENG XIANGYI ; LIN CHANGJIU ; LIU JINGANG ; ZHAO MAPING ; ZHANG XU ; WEI SHENG ; WANG ZHIQIANG ; HU GUOMIN ; HUANG CUNCHAO ; LI DONG ; WANG MINFENG ; ZHU HUAXUE</creator><creatorcontrib>YANG XUNLIANG ; LI GUANGJUN ; MENG XIANGYI ; LIN CHANGJIU ; LIU JINGANG ; ZHAO MAPING ; ZHANG XU ; WEI SHENG ; WANG ZHIQIANG ; HU GUOMIN ; HUANG CUNCHAO ; LI DONG ; WANG MINFENG ; ZHU HUAXUE</creatorcontrib><description>The invention discloses a method with welding residual stress control and crack prevention functions, which comprises the following steps of: before welding, determining preheating temperature and heat preservation time according to the strength of a workpiece material, a stress state, a welding method and welding parameters; the annular large-wall-thickness welding seam of the workpiece material is subjected to segmented welding; repeated multi-pass welding is adopted for midway welding, a final plugging section is reserved, and welding is conducted; in the welding process, real-time temperature monitoring is conducted on a welding area, welding parameters are adjusted according to real-time temperature data, and the welding temperature and the welding speed are controlled; and after welding, a welding joint is cooled. The method is used for solving the technical problems that an existing method for controlling the welding stress and preventing the welding cracks cannot well adapt to the welding requirements</description><language>chi ; eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230704&amp;DB=EPODOC&amp;CC=CN&amp;NR=116372313A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230704&amp;DB=EPODOC&amp;CC=CN&amp;NR=116372313A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YANG XUNLIANG</creatorcontrib><creatorcontrib>LI GUANGJUN</creatorcontrib><creatorcontrib>MENG XIANGYI</creatorcontrib><creatorcontrib>LIN CHANGJIU</creatorcontrib><creatorcontrib>LIU JINGANG</creatorcontrib><creatorcontrib>ZHAO MAPING</creatorcontrib><creatorcontrib>ZHANG XU</creatorcontrib><creatorcontrib>WEI SHENG</creatorcontrib><creatorcontrib>WANG ZHIQIANG</creatorcontrib><creatorcontrib>HU GUOMIN</creatorcontrib><creatorcontrib>HUANG CUNCHAO</creatorcontrib><creatorcontrib>LI DONG</creatorcontrib><creatorcontrib>WANG MINFENG</creatorcontrib><creatorcontrib>ZHU HUAXUE</creatorcontrib><title>Method with welding residual stress control and crack prevention functions</title><description>The invention discloses a method with welding residual stress control and crack prevention functions, which comprises the following steps of: before welding, determining preheating temperature and heat preservation time according to the strength of a workpiece material, a stress state, a welding method and welding parameters; the annular large-wall-thickness welding seam of the workpiece material is subjected to segmented welding; repeated multi-pass welding is adopted for midway welding, a final plugging section is reserved, and welding is conducted; in the welding process, real-time temperature monitoring is conducted on a welding area, welding parameters are adjusted according to real-time temperature data, and the welding temperature and the welding speed are controlled; and after welding, a welding joint is cooled. The method is used for solving the technical problems that an existing method for controlling the welding stress and preventing the welding cracks cannot well adapt to the welding requirements</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEKwjAQgOEsDqK-w_kAHWJAZylKEXRyL0dytcFwCbmrfX0VfACn_xv-pblcScccYI46wkwpRH5AJYlhwgSiHwr4zFpzAuQAvqJ_Qqn0ItaYGYaJ_ReyNosBk9Dm15XZnk_3tmuo5J6koCcm7dubtXt32Dnrju6f5w1j_jWm</recordid><startdate>20230704</startdate><enddate>20230704</enddate><creator>YANG XUNLIANG</creator><creator>LI GUANGJUN</creator><creator>MENG XIANGYI</creator><creator>LIN CHANGJIU</creator><creator>LIU JINGANG</creator><creator>ZHAO MAPING</creator><creator>ZHANG XU</creator><creator>WEI SHENG</creator><creator>WANG ZHIQIANG</creator><creator>HU GUOMIN</creator><creator>HUANG CUNCHAO</creator><creator>LI DONG</creator><creator>WANG MINFENG</creator><creator>ZHU HUAXUE</creator><scope>EVB</scope></search><sort><creationdate>20230704</creationdate><title>Method with welding residual stress control and crack prevention functions</title><author>YANG XUNLIANG ; LI GUANGJUN ; MENG XIANGYI ; LIN CHANGJIU ; LIU JINGANG ; ZHAO MAPING ; ZHANG XU ; WEI SHENG ; WANG ZHIQIANG ; HU GUOMIN ; HUANG CUNCHAO ; LI DONG ; WANG MINFENG ; ZHU HUAXUE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116372313A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>YANG XUNLIANG</creatorcontrib><creatorcontrib>LI GUANGJUN</creatorcontrib><creatorcontrib>MENG XIANGYI</creatorcontrib><creatorcontrib>LIN CHANGJIU</creatorcontrib><creatorcontrib>LIU JINGANG</creatorcontrib><creatorcontrib>ZHAO MAPING</creatorcontrib><creatorcontrib>ZHANG XU</creatorcontrib><creatorcontrib>WEI SHENG</creatorcontrib><creatorcontrib>WANG ZHIQIANG</creatorcontrib><creatorcontrib>HU GUOMIN</creatorcontrib><creatorcontrib>HUANG CUNCHAO</creatorcontrib><creatorcontrib>LI DONG</creatorcontrib><creatorcontrib>WANG MINFENG</creatorcontrib><creatorcontrib>ZHU HUAXUE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YANG XUNLIANG</au><au>LI GUANGJUN</au><au>MENG XIANGYI</au><au>LIN CHANGJIU</au><au>LIU JINGANG</au><au>ZHAO MAPING</au><au>ZHANG XU</au><au>WEI SHENG</au><au>WANG ZHIQIANG</au><au>HU GUOMIN</au><au>HUANG CUNCHAO</au><au>LI DONG</au><au>WANG MINFENG</au><au>ZHU HUAXUE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method with welding residual stress control and crack prevention functions</title><date>2023-07-04</date><risdate>2023</risdate><abstract>The invention discloses a method with welding residual stress control and crack prevention functions, which comprises the following steps of: before welding, determining preheating temperature and heat preservation time according to the strength of a workpiece material, a stress state, a welding method and welding parameters; the annular large-wall-thickness welding seam of the workpiece material is subjected to segmented welding; repeated multi-pass welding is adopted for midway welding, a final plugging section is reserved, and welding is conducted; in the welding process, real-time temperature monitoring is conducted on a welding area, welding parameters are adjusted according to real-time temperature data, and the welding temperature and the welding speed are controlled; and after welding, a welding joint is cooled. The method is used for solving the technical problems that an existing method for controlling the welding stress and preventing the welding cracks cannot well adapt to the welding requirements</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116372313A
source esp@cenet
subjects CLADDING OR PLATING BY SOLDERING OR WELDING
CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
PERFORMING OPERATIONS
SOLDERING OR UNSOLDERING
TRANSPORTING
WELDING
WORKING BY LASER BEAM
title Method with welding residual stress control and crack prevention functions
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T07%3A28%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YANG%20XUNLIANG&rft.date=2023-07-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116372313A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true