Preparation method and application of strip-shaped nano barium sulfate

The invention discloses a preparation method and application of strip-shaped nano barium sulfate, and the preparation method comprises the following steps: S0, adding 0.05-0.6 part by mass of EDTA-2Na and 0.05-0.2 part by mass of phosphate into 10-30 parts by mass of barium sulfide slurry, fully and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FANG SIBO, FANG LIFU, FANG CHANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator FANG SIBO
FANG LIFU
FANG CHANG
description The invention discloses a preparation method and application of strip-shaped nano barium sulfate, and the preparation method comprises the following steps: S0, adding 0.05-0.6 part by mass of EDTA-2Na and 0.05-0.2 part by mass of phosphate into 10-30 parts by mass of barium sulfide slurry, fully and uniformly mixing to obtain a pre-reaction mixture, S1, preparing 3-8 parts by mass of a sodium sulfate solution with the concentration of 3-8 wt% (in parts by mass), and stirring uniformly to obtain a pre-reaction mixture; s2, 0.05-0.7 part by mass of EDTA-2Na and 0.01-0.05 part by mass of sodium octadecyl sulfonate or sodium octadecyl sulfate are added into 500-1000 parts by mass of water to prepare a bottom water mixture, S3, the pre-reaction mixture and a sulfuric acid solution are added into the bottom water mixture, S4, the mixture in the S3 is stirred for full reaction, a post-reaction mixture is obtained, and the pre-reaction mixture is obtained. And S5, filtering, washing and drying the reacted mixture to
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116332218A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116332218A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116332218A3</originalsourceid><addsrcrecordid>eNrjZHALKEotSCxKLMnMz1PITS3JyE9RSMwD4oKCnMxkiHB-mkJxSVFmgW5xRmJBaopCXmJevkJSYlFmaa5CcWlOWmJJKg8Da1piTnEqL5TmZlB0cw1x9tBNLciPTy0uSExOzUstiXf2MzQ0MzY2MjK0cDQmRg0ASVEzuQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method and application of strip-shaped nano barium sulfate</title><source>esp@cenet</source><creator>FANG SIBO ; FANG LIFU ; FANG CHANG</creator><creatorcontrib>FANG SIBO ; FANG LIFU ; FANG CHANG</creatorcontrib><description>The invention discloses a preparation method and application of strip-shaped nano barium sulfate, and the preparation method comprises the following steps: S0, adding 0.05-0.6 part by mass of EDTA-2Na and 0.05-0.2 part by mass of phosphate into 10-30 parts by mass of barium sulfide slurry, fully and uniformly mixing to obtain a pre-reaction mixture, S1, preparing 3-8 parts by mass of a sodium sulfate solution with the concentration of 3-8 wt% (in parts by mass), and stirring uniformly to obtain a pre-reaction mixture; s2, 0.05-0.7 part by mass of EDTA-2Na and 0.01-0.05 part by mass of sodium octadecyl sulfonate or sodium octadecyl sulfate are added into 500-1000 parts by mass of water to prepare a bottom water mixture, S3, the pre-reaction mixture and a sulfuric acid solution are added into the bottom water mixture, S4, the mixture in the S3 is stirred for full reaction, a post-reaction mixture is obtained, and the pre-reaction mixture is obtained. And S5, filtering, washing and drying the reacted mixture to</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS ; INORGANIC CHEMISTRY ; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES ; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES ; METALLURGY ; NANOTECHNOLOGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230627&amp;DB=EPODOC&amp;CC=CN&amp;NR=116332218A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230627&amp;DB=EPODOC&amp;CC=CN&amp;NR=116332218A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>FANG SIBO</creatorcontrib><creatorcontrib>FANG LIFU</creatorcontrib><creatorcontrib>FANG CHANG</creatorcontrib><title>Preparation method and application of strip-shaped nano barium sulfate</title><description>The invention discloses a preparation method and application of strip-shaped nano barium sulfate, and the preparation method comprises the following steps: S0, adding 0.05-0.6 part by mass of EDTA-2Na and 0.05-0.2 part by mass of phosphate into 10-30 parts by mass of barium sulfide slurry, fully and uniformly mixing to obtain a pre-reaction mixture, S1, preparing 3-8 parts by mass of a sodium sulfate solution with the concentration of 3-8 wt% (in parts by mass), and stirring uniformly to obtain a pre-reaction mixture; s2, 0.05-0.7 part by mass of EDTA-2Na and 0.01-0.05 part by mass of sodium octadecyl sulfonate or sodium octadecyl sulfate are added into 500-1000 parts by mass of water to prepare a bottom water mixture, S3, the pre-reaction mixture and a sulfuric acid solution are added into the bottom water mixture, S4, the mixture in the S3 is stirred for full reaction, a post-reaction mixture is obtained, and the pre-reaction mixture is obtained. And S5, filtering, washing and drying the reacted mixture to</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</subject><subject>INORGANIC CHEMISTRY</subject><subject>MANUFACTURE OR TREATMENT OF NANOSTRUCTURES</subject><subject>MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES</subject><subject>METALLURGY</subject><subject>NANOTECHNOLOGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHALKEotSCxKLMnMz1PITS3JyE9RSMwD4oKCnMxkiHB-mkJxSVFmgW5xRmJBaopCXmJevkJSYlFmaa5CcWlOWmJJKg8Da1piTnEqL5TmZlB0cw1x9tBNLciPTy0uSExOzUstiXf2MzQ0MzY2MjK0cDQmRg0ASVEzuQ</recordid><startdate>20230627</startdate><enddate>20230627</enddate><creator>FANG SIBO</creator><creator>FANG LIFU</creator><creator>FANG CHANG</creator><scope>EVB</scope></search><sort><creationdate>20230627</creationdate><title>Preparation method and application of strip-shaped nano barium sulfate</title><author>FANG SIBO ; FANG LIFU ; FANG CHANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116332218A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</topic><topic>INORGANIC CHEMISTRY</topic><topic>MANUFACTURE OR TREATMENT OF NANOSTRUCTURES</topic><topic>MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES</topic><topic>METALLURGY</topic><topic>NANOTECHNOLOGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>FANG SIBO</creatorcontrib><creatorcontrib>FANG LIFU</creatorcontrib><creatorcontrib>FANG CHANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>FANG SIBO</au><au>FANG LIFU</au><au>FANG CHANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method and application of strip-shaped nano barium sulfate</title><date>2023-06-27</date><risdate>2023</risdate><abstract>The invention discloses a preparation method and application of strip-shaped nano barium sulfate, and the preparation method comprises the following steps: S0, adding 0.05-0.6 part by mass of EDTA-2Na and 0.05-0.2 part by mass of phosphate into 10-30 parts by mass of barium sulfide slurry, fully and uniformly mixing to obtain a pre-reaction mixture, S1, preparing 3-8 parts by mass of a sodium sulfate solution with the concentration of 3-8 wt% (in parts by mass), and stirring uniformly to obtain a pre-reaction mixture; s2, 0.05-0.7 part by mass of EDTA-2Na and 0.01-0.05 part by mass of sodium octadecyl sulfonate or sodium octadecyl sulfate are added into 500-1000 parts by mass of water to prepare a bottom water mixture, S3, the pre-reaction mixture and a sulfuric acid solution are added into the bottom water mixture, S4, the mixture in the S3 is stirred for full reaction, a post-reaction mixture is obtained, and the pre-reaction mixture is obtained. And S5, filtering, washing and drying the reacted mixture to</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116332218A
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS
INORGANIC CHEMISTRY
MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES
METALLURGY
NANOTECHNOLOGY
ORGANIC MACROMOLECULAR COMPOUNDS
PERFORMING OPERATIONS
SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES
THEIR PREPARATION OR CHEMICAL WORKING-UP
TRANSPORTING
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS
title Preparation method and application of strip-shaped nano barium sulfate
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T17%3A26%3A07IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=FANG%20SIBO&rft.date=2023-06-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116332218A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true