Method for improving bowl opening of straightened end of drill collar steel

The invention relates to a method for improving an end bowl opening of straightened drill collar steel, and belongs to the technical field of drill collar steel production processes in the metallurgical industry. According to the technical scheme, seven-roller straightening is adopted, the rolling r...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG XIAOJUN, ZHU YE, ZHAO JINGCUN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG XIAOJUN
ZHU YE
ZHAO JINGCUN
description The invention relates to a method for improving an end bowl opening of straightened drill collar steel, and belongs to the technical field of drill collar steel production processes in the metallurgical industry. According to the technical scheme, seven-roller straightening is adopted, the rolling reduction of 1 # upper and lower rollers and 3 # upper and lower rollers is 4-5 mm, and the rolling reduction of 2 # upper and lower rollers is 1-2 mm; the anti-bending amount is 15 to 16 mm; the angles of the straightening rollers are as follows: the angle of a 1 # upper roller and a 1 # lower roller is 29.5-30 degrees, the angle of a 2 # upper roller is 30-31 degrees, the angle of a 3 # upper roller is 29.5-30 degrees, and the angle of a lower roller is 32-32.5 degrees; and the straightened end of the round steel is chamfered, the chamfering angle ranges from 30 degrees to 45 degrees, and the chamfering length ranges from 1 mm to 2 mm. The method has the beneficial effects that the internal structure stress of the
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116274374A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116274374A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116274374A3</originalsourceid><addsrcrecordid>eNrjZPD2TS3JyE9RSMsvUsjMLSjKL8vMS1dIyi_PUcgvSM0DcfLTFIpLihIz0zNKUvNSUxRS81JAYilFmTk5Csn5OTmJRUAFqak5PAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMRmovyTe2c_Q0MzI3MTY3MTRmBg1AFNRNVM</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for improving bowl opening of straightened end of drill collar steel</title><source>esp@cenet</source><creator>WANG XIAOJUN ; ZHU YE ; ZHAO JINGCUN</creator><creatorcontrib>WANG XIAOJUN ; ZHU YE ; ZHAO JINGCUN</creatorcontrib><description>The invention relates to a method for improving an end bowl opening of straightened drill collar steel, and belongs to the technical field of drill collar steel production processes in the metallurgical industry. According to the technical scheme, seven-roller straightening is adopted, the rolling reduction of 1 # upper and lower rollers and 3 # upper and lower rollers is 4-5 mm, and the rolling reduction of 2 # upper and lower rollers is 1-2 mm; the anti-bending amount is 15 to 16 mm; the angles of the straightening rollers are as follows: the angle of a 1 # upper roller and a 1 # lower roller is 29.5-30 degrees, the angle of a 2 # upper roller is 30-31 degrees, the angle of a 3 # upper roller is 29.5-30 degrees, and the angle of a lower roller is 32-32.5 degrees; and the straightened end of the round steel is chamfered, the chamfering angle ranges from 30 degrees to 45 degrees, and the chamfering length ranges from 1 mm to 2 mm. The method has the beneficial effects that the internal structure stress of the</description><language>chi ; eng</language><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; PERFORMING OPERATIONS ; PUNCHING METAL ; ROLLING OF METAL ; TRANSPORTING ; WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230623&amp;DB=EPODOC&amp;CC=CN&amp;NR=116274374A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230623&amp;DB=EPODOC&amp;CC=CN&amp;NR=116274374A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG XIAOJUN</creatorcontrib><creatorcontrib>ZHU YE</creatorcontrib><creatorcontrib>ZHAO JINGCUN</creatorcontrib><title>Method for improving bowl opening of straightened end of drill collar steel</title><description>The invention relates to a method for improving an end bowl opening of straightened drill collar steel, and belongs to the technical field of drill collar steel production processes in the metallurgical industry. According to the technical scheme, seven-roller straightening is adopted, the rolling reduction of 1 # upper and lower rollers and 3 # upper and lower rollers is 4-5 mm, and the rolling reduction of 2 # upper and lower rollers is 1-2 mm; the anti-bending amount is 15 to 16 mm; the angles of the straightening rollers are as follows: the angle of a 1 # upper roller and a 1 # lower roller is 29.5-30 degrees, the angle of a 2 # upper roller is 30-31 degrees, the angle of a 3 # upper roller is 29.5-30 degrees, and the angle of a lower roller is 32-32.5 degrees; and the straightened end of the round steel is chamfered, the chamfering angle ranges from 30 degrees to 45 degrees, and the chamfering length ranges from 1 mm to 2 mm. The method has the beneficial effects that the internal structure stress of the</description><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>ROLLING OF METAL</subject><subject>TRANSPORTING</subject><subject>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPD2TS3JyE9RSMsvUsjMLSjKL8vMS1dIyi_PUcgvSM0DcfLTFIpLihIz0zNKUvNSUxRS81JAYilFmTk5Csn5OTmJRUAFqak5PAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMRmovyTe2c_Q0MzI3MTY3MTRmBg1AFNRNVM</recordid><startdate>20230623</startdate><enddate>20230623</enddate><creator>WANG XIAOJUN</creator><creator>ZHU YE</creator><creator>ZHAO JINGCUN</creator><scope>EVB</scope></search><sort><creationdate>20230623</creationdate><title>Method for improving bowl opening of straightened end of drill collar steel</title><author>WANG XIAOJUN ; ZHU YE ; ZHAO JINGCUN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116274374A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>ROLLING OF METAL</topic><topic>TRANSPORTING</topic><topic>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG XIAOJUN</creatorcontrib><creatorcontrib>ZHU YE</creatorcontrib><creatorcontrib>ZHAO JINGCUN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG XIAOJUN</au><au>ZHU YE</au><au>ZHAO JINGCUN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for improving bowl opening of straightened end of drill collar steel</title><date>2023-06-23</date><risdate>2023</risdate><abstract>The invention relates to a method for improving an end bowl opening of straightened drill collar steel, and belongs to the technical field of drill collar steel production processes in the metallurgical industry. According to the technical scheme, seven-roller straightening is adopted, the rolling reduction of 1 # upper and lower rollers and 3 # upper and lower rollers is 4-5 mm, and the rolling reduction of 2 # upper and lower rollers is 1-2 mm; the anti-bending amount is 15 to 16 mm; the angles of the straightening rollers are as follows: the angle of a 1 # upper roller and a 1 # lower roller is 29.5-30 degrees, the angle of a 2 # upper roller is 30-31 degrees, the angle of a 3 # upper roller is 29.5-30 degrees, and the angle of a lower roller is 32-32.5 degrees; and the straightened end of the round steel is chamfered, the chamfering angle ranges from 30 degrees to 45 degrees, and the chamfering length ranges from 1 mm to 2 mm. The method has the beneficial effects that the internal structure stress of the</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116274374A
source esp@cenet
subjects MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
PERFORMING OPERATIONS
PUNCHING METAL
ROLLING OF METAL
TRANSPORTING
WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL
title Method for improving bowl opening of straightened end of drill collar steel
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-21T18%3A16%3A37IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20XIAOJUN&rft.date=2023-06-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116274374A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true