Ferritic nodular cast iron, casting and preparation method thereof

The invention discloses ferritic nodular cast iron, a casting and a preparation method of the ferritic nodular cast iron, the ferritic nodular cast iron comprises the following elements in percentage by mass: 92.25-94.25% of Fe, 0.09-0.38% of Cu, 2.92-3.35% of C, 2.92-3.35% of Si, 0.09-0.38% of Mn,...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU JIANCE, LIU XIAOLIANG, LIU SHA, YAN CHUNJIAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIU JIANCE
LIU XIAOLIANG
LIU SHA
YAN CHUNJIAN
description The invention discloses ferritic nodular cast iron, a casting and a preparation method of the ferritic nodular cast iron, the ferritic nodular cast iron comprises the following elements in percentage by mass: 92.25-94.25% of Fe, 0.09-0.38% of Cu, 2.92-3.35% of C, 2.92-3.35% of Si, 0.09-0.38% of Mn, less than or equal to 0.04% of P and less than or equal to 0.02% of S. The casting of the ferritic nodular cast iron is formed by pouring the ferritic nodular cast iron material, the core of the ferritic nodular cast iron casting is of a ferritic structure, and the core of the ferritic nodular cast iron casting is of The surface structure of the ferritic nodular cast iron is martensite. The preparation method comprises the following steps: preparing nodular cast iron, pouring a casting, cooling the casting by adopting a staged cooling chill process, and carrying out laser quenching. The ferritic nodular cast iron with the tensile strength of 450 MPa or above, the hardness of 150 HBW or above and the high elongation
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116200647A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116200647A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116200647A3</originalsourceid><addsrcrecordid>eNrjZHBySy0qyizJTFbIy08pzUksUkhOLC5RyCzKz9MBMzPz0hUS81IUCopSCxKLEksy8_MUclNLMvJTFEoyUotS89N4GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8s5-hoZmRgYGZibmjMTFqAD3XMgo</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Ferritic nodular cast iron, casting and preparation method thereof</title><source>esp@cenet</source><creator>LIU JIANCE ; LIU XIAOLIANG ; LIU SHA ; YAN CHUNJIAN</creator><creatorcontrib>LIU JIANCE ; LIU XIAOLIANG ; LIU SHA ; YAN CHUNJIAN</creatorcontrib><description>The invention discloses ferritic nodular cast iron, a casting and a preparation method of the ferritic nodular cast iron, the ferritic nodular cast iron comprises the following elements in percentage by mass: 92.25-94.25% of Fe, 0.09-0.38% of Cu, 2.92-3.35% of C, 2.92-3.35% of Si, 0.09-0.38% of Mn, less than or equal to 0.04% of P and less than or equal to 0.02% of S. The casting of the ferritic nodular cast iron is formed by pouring the ferritic nodular cast iron material, the core of the ferritic nodular cast iron casting is of a ferritic structure, and the core of the ferritic nodular cast iron casting is of The surface structure of the ferritic nodular cast iron is martensite. The preparation method comprises the following steps: preparing nodular cast iron, pouring a casting, cooling the casting by adopting a staged cooling chill process, and carrying out laser quenching. The ferritic nodular cast iron with the tensile strength of 450 MPa or above, the hardness of 150 HBW or above and the high elongation</description><language>chi ; eng</language><subject>ALLOYS ; CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; PERFORMING OPERATIONS ; POWDER METALLURGY ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; TRANSPORTING ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230602&amp;DB=EPODOC&amp;CC=CN&amp;NR=116200647A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230602&amp;DB=EPODOC&amp;CC=CN&amp;NR=116200647A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU JIANCE</creatorcontrib><creatorcontrib>LIU XIAOLIANG</creatorcontrib><creatorcontrib>LIU SHA</creatorcontrib><creatorcontrib>YAN CHUNJIAN</creatorcontrib><title>Ferritic nodular cast iron, casting and preparation method thereof</title><description>The invention discloses ferritic nodular cast iron, a casting and a preparation method of the ferritic nodular cast iron, the ferritic nodular cast iron comprises the following elements in percentage by mass: 92.25-94.25% of Fe, 0.09-0.38% of Cu, 2.92-3.35% of C, 2.92-3.35% of Si, 0.09-0.38% of Mn, less than or equal to 0.04% of P and less than or equal to 0.02% of S. The casting of the ferritic nodular cast iron is formed by pouring the ferritic nodular cast iron material, the core of the ferritic nodular cast iron casting is of a ferritic structure, and the core of the ferritic nodular cast iron casting is of The surface structure of the ferritic nodular cast iron is martensite. The preparation method comprises the following steps: preparing nodular cast iron, pouring a casting, cooling the casting by adopting a staged cooling chill process, and carrying out laser quenching. The ferritic nodular cast iron with the tensile strength of 450 MPa or above, the hardness of 150 HBW or above and the high elongation</description><subject>ALLOYS</subject><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>TRANSPORTING</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHBySy0qyizJTFbIy08pzUksUkhOLC5RyCzKz9MBMzPz0hUS81IUCopSCxKLEksy8_MUclNLMvJTFEoyUotS89N4GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8s5-hoZmRgYGZibmjMTFqAD3XMgo</recordid><startdate>20230602</startdate><enddate>20230602</enddate><creator>LIU JIANCE</creator><creator>LIU XIAOLIANG</creator><creator>LIU SHA</creator><creator>YAN CHUNJIAN</creator><scope>EVB</scope></search><sort><creationdate>20230602</creationdate><title>Ferritic nodular cast iron, casting and preparation method thereof</title><author>LIU JIANCE ; LIU XIAOLIANG ; LIU SHA ; YAN CHUNJIAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116200647A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>ALLOYS</topic><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>TRANSPORTING</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU JIANCE</creatorcontrib><creatorcontrib>LIU XIAOLIANG</creatorcontrib><creatorcontrib>LIU SHA</creatorcontrib><creatorcontrib>YAN CHUNJIAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU JIANCE</au><au>LIU XIAOLIANG</au><au>LIU SHA</au><au>YAN CHUNJIAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Ferritic nodular cast iron, casting and preparation method thereof</title><date>2023-06-02</date><risdate>2023</risdate><abstract>The invention discloses ferritic nodular cast iron, a casting and a preparation method of the ferritic nodular cast iron, the ferritic nodular cast iron comprises the following elements in percentage by mass: 92.25-94.25% of Fe, 0.09-0.38% of Cu, 2.92-3.35% of C, 2.92-3.35% of Si, 0.09-0.38% of Mn, less than or equal to 0.04% of P and less than or equal to 0.02% of S. The casting of the ferritic nodular cast iron is formed by pouring the ferritic nodular cast iron material, the core of the ferritic nodular cast iron casting is of a ferritic structure, and the core of the ferritic nodular cast iron casting is of The surface structure of the ferritic nodular cast iron is martensite. The preparation method comprises the following steps: preparing nodular cast iron, pouring a casting, cooling the casting by adopting a staged cooling chill process, and carrying out laser quenching. The ferritic nodular cast iron with the tensile strength of 450 MPa or above, the hardness of 150 HBW or above and the high elongation</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116200647A
source esp@cenet
subjects ALLOYS
CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
PERFORMING OPERATIONS
POWDER METALLURGY
PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL
TRANSPORTING
TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Ferritic nodular cast iron, casting and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-22T17%3A19%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20JIANCE&rft.date=2023-06-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116200647A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true