Low-relaxation high-strength prestressed steel and production method thereof

The invention discloses low-relaxation high-strength prestressed steel which comprises the following components in percentage by weight: 0.29 to 0.36 percent of C, 0.80 to 1.20 percent of Si, 0.60 to 0.80 percent of Mn, 0.10 to 0.15 percent of Cr, 0.010 to 0.020 percent of V, less than or equal to 0...