Low-relaxation high-strength prestressed steel and production method thereof

The invention discloses low-relaxation high-strength prestressed steel which comprises the following components in percentage by weight: 0.29 to 0.36 percent of C, 0.80 to 1.20 percent of Si, 0.60 to 0.80 percent of Mn, 0.10 to 0.15 percent of Cr, 0.010 to 0.020 percent of V, less than or equal to 0...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHANG XIANZHONG, LU XIUYU, LIAO YANGBIAO, ZHENG CHUANYU, XU ZHIDONG, XIA YANHUA, ZHANG FAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHANG XIANZHONG
LU XIUYU
LIAO YANGBIAO
ZHENG CHUANYU
XU ZHIDONG
XIA YANHUA
ZHANG FAN
description The invention discloses low-relaxation high-strength prestressed steel which comprises the following components in percentage by weight: 0.29 to 0.36 percent of C, 0.80 to 1.20 percent of Si, 0.60 to 0.80 percent of Mn, 0.10 to 0.15 percent of Cr, 0.010 to 0.020 percent of V, less than or equal to 0.020 percent of P, less than or equal to 0.015 percent of S and the balance of iron and inevitable impurities. The production method comprises the following steps: pre-desulfurizing blast furnace molten iron by adopting a magnesium spraying desulfurization method, smelting in a top-bottom combined blown converter, and deoxidizing and alloying in a tapping process after smelting is completed; refining in an LF furnace, wherein the LF furnace adopts a whole-course argon bottom blowing mode; active lime and fluorite are added in the refining process to prepare refining slag; the LF refining time is not less than 40 minutes; carrying out soft argon blowing on the molten steel after LF; argon sealing protection pouring
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116179963A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116179963A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116179963A3</originalsourceid><addsrcrecordid>eNrjZPDxyS_XLUrNSaxILMnMz1PIyEzP0C0uKUrNSy_JUCgoSgWxi4tTUxSKS1JTcxQS81KAovkppclg5bmpJRn5KQolGalFqflpPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3tnP0NDM0NzS0szY0ZgYNQAF7za0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Low-relaxation high-strength prestressed steel and production method thereof</title><source>esp@cenet</source><creator>ZHANG XIANZHONG ; LU XIUYU ; LIAO YANGBIAO ; ZHENG CHUANYU ; XU ZHIDONG ; XIA YANHUA ; ZHANG FAN</creator><creatorcontrib>ZHANG XIANZHONG ; LU XIUYU ; LIAO YANGBIAO ; ZHENG CHUANYU ; XU ZHIDONG ; XIA YANHUA ; ZHANG FAN</creatorcontrib><description>The invention discloses low-relaxation high-strength prestressed steel which comprises the following components in percentage by weight: 0.29 to 0.36 percent of C, 0.80 to 1.20 percent of Si, 0.60 to 0.80 percent of Mn, 0.10 to 0.15 percent of Cr, 0.010 to 0.020 percent of V, less than or equal to 0.020 percent of P, less than or equal to 0.015 percent of S and the balance of iron and inevitable impurities. The production method comprises the following steps: pre-desulfurizing blast furnace molten iron by adopting a magnesium spraying desulfurization method, smelting in a top-bottom combined blown converter, and deoxidizing and alloying in a tapping process after smelting is completed; refining in an LF furnace, wherein the LF furnace adopts a whole-course argon bottom blowing mode; active lime and fluorite are added in the refining process to prepare refining slag; the LF refining time is not less than 40 minutes; carrying out soft argon blowing on the molten steel after LF; argon sealing protection pouring</description><language>chi ; eng</language><subject>ALLOYS ; CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; METALLURGY OF IRON ; PERFORMING OPERATIONS ; POWDER METALLURGY ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; TRANSPORTING ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230530&amp;DB=EPODOC&amp;CC=CN&amp;NR=116179963A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230530&amp;DB=EPODOC&amp;CC=CN&amp;NR=116179963A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHANG XIANZHONG</creatorcontrib><creatorcontrib>LU XIUYU</creatorcontrib><creatorcontrib>LIAO YANGBIAO</creatorcontrib><creatorcontrib>ZHENG CHUANYU</creatorcontrib><creatorcontrib>XU ZHIDONG</creatorcontrib><creatorcontrib>XIA YANHUA</creatorcontrib><creatorcontrib>ZHANG FAN</creatorcontrib><title>Low-relaxation high-strength prestressed steel and production method thereof</title><description>The invention discloses low-relaxation high-strength prestressed steel which comprises the following components in percentage by weight: 0.29 to 0.36 percent of C, 0.80 to 1.20 percent of Si, 0.60 to 0.80 percent of Mn, 0.10 to 0.15 percent of Cr, 0.010 to 0.020 percent of V, less than or equal to 0.020 percent of P, less than or equal to 0.015 percent of S and the balance of iron and inevitable impurities. The production method comprises the following steps: pre-desulfurizing blast furnace molten iron by adopting a magnesium spraying desulfurization method, smelting in a top-bottom combined blown converter, and deoxidizing and alloying in a tapping process after smelting is completed; refining in an LF furnace, wherein the LF furnace adopts a whole-course argon bottom blowing mode; active lime and fluorite are added in the refining process to prepare refining slag; the LF refining time is not less than 40 minutes; carrying out soft argon blowing on the molten steel after LF; argon sealing protection pouring</description><subject>ALLOYS</subject><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>TRANSPORTING</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPDxyS_XLUrNSaxILMnMz1PIyEzP0C0uKUrNSy_JUCgoSgWxi4tTUxSKS1JTcxQS81KAovkppclg5bmpJRn5KQolGalFqflpPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3tnP0NDM0NzS0szY0ZgYNQAF7za0</recordid><startdate>20230530</startdate><enddate>20230530</enddate><creator>ZHANG XIANZHONG</creator><creator>LU XIUYU</creator><creator>LIAO YANGBIAO</creator><creator>ZHENG CHUANYU</creator><creator>XU ZHIDONG</creator><creator>XIA YANHUA</creator><creator>ZHANG FAN</creator><scope>EVB</scope></search><sort><creationdate>20230530</creationdate><title>Low-relaxation high-strength prestressed steel and production method thereof</title><author>ZHANG XIANZHONG ; LU XIUYU ; LIAO YANGBIAO ; ZHENG CHUANYU ; XU ZHIDONG ; XIA YANHUA ; ZHANG FAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116179963A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>ALLOYS</topic><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>TRANSPORTING</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHANG XIANZHONG</creatorcontrib><creatorcontrib>LU XIUYU</creatorcontrib><creatorcontrib>LIAO YANGBIAO</creatorcontrib><creatorcontrib>ZHENG CHUANYU</creatorcontrib><creatorcontrib>XU ZHIDONG</creatorcontrib><creatorcontrib>XIA YANHUA</creatorcontrib><creatorcontrib>ZHANG FAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHANG XIANZHONG</au><au>LU XIUYU</au><au>LIAO YANGBIAO</au><au>ZHENG CHUANYU</au><au>XU ZHIDONG</au><au>XIA YANHUA</au><au>ZHANG FAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Low-relaxation high-strength prestressed steel and production method thereof</title><date>2023-05-30</date><risdate>2023</risdate><abstract>The invention discloses low-relaxation high-strength prestressed steel which comprises the following components in percentage by weight: 0.29 to 0.36 percent of C, 0.80 to 1.20 percent of Si, 0.60 to 0.80 percent of Mn, 0.10 to 0.15 percent of Cr, 0.010 to 0.020 percent of V, less than or equal to 0.020 percent of P, less than or equal to 0.015 percent of S and the balance of iron and inevitable impurities. The production method comprises the following steps: pre-desulfurizing blast furnace molten iron by adopting a magnesium spraying desulfurization method, smelting in a top-bottom combined blown converter, and deoxidizing and alloying in a tapping process after smelting is completed; refining in an LF furnace, wherein the LF furnace adopts a whole-course argon bottom blowing mode; active lime and fluorite are added in the refining process to prepare refining slag; the LF refining time is not less than 40 minutes; carrying out soft argon blowing on the molten steel after LF; argon sealing protection pouring</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116179963A
source esp@cenet
subjects ALLOYS
CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
METALLURGY OF IRON
PERFORMING OPERATIONS
POWDER METALLURGY
PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL
TRANSPORTING
TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Low-relaxation high-strength prestressed steel and production method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T04%3A10%3A32IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHANG%20XIANZHONG&rft.date=2023-05-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116179963A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true