Implementation method of FRP glue joint maintenance geometric configuration based on laser controllable processing

The invention discloses a laser controllable processing-based FRP (fiber reinforce plastic) glue joint maintenance geometric configuration implementation method, which aims to improve the surface physical and chemical properties of geometric configuration, and comprises the following steps: carrying...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANG WENFENG, WANG LIN, YIN XINGUANG, WANG WENXUAN, WANG DISHENG, LI TIANQUAN, LI SHAOLONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YANG WENFENG
WANG LIN
YIN XINGUANG
WANG WENXUAN
WANG DISHENG
LI TIANQUAN
LI SHAOLONG
description The invention discloses a laser controllable processing-based FRP (fiber reinforce plastic) glue joint maintenance geometric configuration implementation method, which aims to improve the surface physical and chemical properties of geometric configuration, and comprises the following steps: carrying out laser controllable processing on an FRP damaged area by adopting laser, realizing layer-by-layer removal of carbon fibers, and forming geometric configuration and surface properties which are beneficial to glue joint maintenance. The method has the advantages of being easy to operate, good in resin removing effect, high in fiber integrity, high in shape precision and three-dimensional size precision and the like. The problems that in the prior art, the number of resin residues on the surface of the maintained geometric configuration is large, the fiber fracture amount is large, and the shape precision and the three-dimensional size precision are poor can be solved. And therefore, the FRP glue joint maintenance
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116141712A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116141712A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116141712A3</originalsourceid><addsrcrecordid>eNqNi0EKwjAURLtxIeodvgdwERVdS7HoRkTclzROYyT9PyTp_Y3oAdzMDMx70yqeh-AxgLPOTpgG5Kc8SHpqbleyfgS9xHGmQZcEazYgCylcdIaMcO_sGL9ypxOKy-TLiJ8zR_Fedx4Uohik5NjOq0mvfcLi17Nq2Rzv9WmFIC1S0AaM3NYXpXZqq_Zqfdj8w7wBMoNEqQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Implementation method of FRP glue joint maintenance geometric configuration based on laser controllable processing</title><source>esp@cenet</source><creator>YANG WENFENG ; WANG LIN ; YIN XINGUANG ; WANG WENXUAN ; WANG DISHENG ; LI TIANQUAN ; LI SHAOLONG</creator><creatorcontrib>YANG WENFENG ; WANG LIN ; YIN XINGUANG ; WANG WENXUAN ; WANG DISHENG ; LI TIANQUAN ; LI SHAOLONG</creatorcontrib><description>The invention discloses a laser controllable processing-based FRP (fiber reinforce plastic) glue joint maintenance geometric configuration implementation method, which aims to improve the surface physical and chemical properties of geometric configuration, and comprises the following steps: carrying out laser controllable processing on an FRP damaged area by adopting laser, realizing layer-by-layer removal of carbon fibers, and forming geometric configuration and surface properties which are beneficial to glue joint maintenance. The method has the advantages of being easy to operate, good in resin removing effect, high in fiber integrity, high in shape precision and three-dimensional size precision and the like. The problems that in the prior art, the number of resin residues on the surface of the maintained geometric configuration is large, the fiber fracture amount is large, and the shape precision and the three-dimensional size precision are poor can be solved. And therefore, the FRP glue joint maintenance</description><language>chi ; eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; PERFORMING OPERATIONS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230523&amp;DB=EPODOC&amp;CC=CN&amp;NR=116141712A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76419</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230523&amp;DB=EPODOC&amp;CC=CN&amp;NR=116141712A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YANG WENFENG</creatorcontrib><creatorcontrib>WANG LIN</creatorcontrib><creatorcontrib>YIN XINGUANG</creatorcontrib><creatorcontrib>WANG WENXUAN</creatorcontrib><creatorcontrib>WANG DISHENG</creatorcontrib><creatorcontrib>LI TIANQUAN</creatorcontrib><creatorcontrib>LI SHAOLONG</creatorcontrib><title>Implementation method of FRP glue joint maintenance geometric configuration based on laser controllable processing</title><description>The invention discloses a laser controllable processing-based FRP (fiber reinforce plastic) glue joint maintenance geometric configuration implementation method, which aims to improve the surface physical and chemical properties of geometric configuration, and comprises the following steps: carrying out laser controllable processing on an FRP damaged area by adopting laser, realizing layer-by-layer removal of carbon fibers, and forming geometric configuration and surface properties which are beneficial to glue joint maintenance. The method has the advantages of being easy to operate, good in resin removing effect, high in fiber integrity, high in shape precision and three-dimensional size precision and the like. The problems that in the prior art, the number of resin residues on the surface of the maintained geometric configuration is large, the fiber fracture amount is large, and the shape precision and the three-dimensional size precision are poor can be solved. And therefore, the FRP glue joint maintenance</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>PERFORMING OPERATIONS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNi0EKwjAURLtxIeodvgdwERVdS7HoRkTclzROYyT9PyTp_Y3oAdzMDMx70yqeh-AxgLPOTpgG5Kc8SHpqbleyfgS9xHGmQZcEazYgCylcdIaMcO_sGL9ypxOKy-TLiJ8zR_Fedx4Uohik5NjOq0mvfcLi17Nq2Rzv9WmFIC1S0AaM3NYXpXZqq_Zqfdj8w7wBMoNEqQ</recordid><startdate>20230523</startdate><enddate>20230523</enddate><creator>YANG WENFENG</creator><creator>WANG LIN</creator><creator>YIN XINGUANG</creator><creator>WANG WENXUAN</creator><creator>WANG DISHENG</creator><creator>LI TIANQUAN</creator><creator>LI SHAOLONG</creator><scope>EVB</scope></search><sort><creationdate>20230523</creationdate><title>Implementation method of FRP glue joint maintenance geometric configuration based on laser controllable processing</title><author>YANG WENFENG ; WANG LIN ; YIN XINGUANG ; WANG WENXUAN ; WANG DISHENG ; LI TIANQUAN ; LI SHAOLONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116141712A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>PERFORMING OPERATIONS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>YANG WENFENG</creatorcontrib><creatorcontrib>WANG LIN</creatorcontrib><creatorcontrib>YIN XINGUANG</creatorcontrib><creatorcontrib>WANG WENXUAN</creatorcontrib><creatorcontrib>WANG DISHENG</creatorcontrib><creatorcontrib>LI TIANQUAN</creatorcontrib><creatorcontrib>LI SHAOLONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YANG WENFENG</au><au>WANG LIN</au><au>YIN XINGUANG</au><au>WANG WENXUAN</au><au>WANG DISHENG</au><au>LI TIANQUAN</au><au>LI SHAOLONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Implementation method of FRP glue joint maintenance geometric configuration based on laser controllable processing</title><date>2023-05-23</date><risdate>2023</risdate><abstract>The invention discloses a laser controllable processing-based FRP (fiber reinforce plastic) glue joint maintenance geometric configuration implementation method, which aims to improve the surface physical and chemical properties of geometric configuration, and comprises the following steps: carrying out laser controllable processing on an FRP damaged area by adopting laser, realizing layer-by-layer removal of carbon fibers, and forming geometric configuration and surface properties which are beneficial to glue joint maintenance. The method has the advantages of being easy to operate, good in resin removing effect, high in fiber integrity, high in shape precision and three-dimensional size precision and the like. The problems that in the prior art, the number of resin residues on the surface of the maintained geometric configuration is large, the fiber fracture amount is large, and the shape precision and the three-dimensional size precision are poor can be solved. And therefore, the FRP glue joint maintenance</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116141712A
source esp@cenet
subjects AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
PERFORMING OPERATIONS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
title Implementation method of FRP glue joint maintenance geometric configuration based on laser controllable processing
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T19%3A19%3A13IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YANG%20WENFENG&rft.date=2023-05-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116141712A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true