Bridging plugging slurry and preparation method thereof

The invention provides bridging plugging slurry and a preparation method thereof. The novel plugging slurry with good flowback capability is formed by bridging the shape memory alloy with the two-way effect in the plugging slurry and utilizing the characteristic that the shape of the shape memory al...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: CHEN ZENGWEI, SONG BITAO, LI DAQI, OU BIAO, LI FAN, LIU JINHUA, CHEN ZHIHUI, REN MAO, ZHANG DUJIE
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator CHEN ZENGWEI
SONG BITAO
LI DAQI
OU BIAO
LI FAN
LIU JINHUA
CHEN ZHIHUI
REN MAO
ZHANG DUJIE
description The invention provides bridging plugging slurry and a preparation method thereof. The novel plugging slurry with good flowback capability is formed by bridging the shape memory alloy with the two-way effect in the plugging slurry and utilizing the characteristic that the shape of the shape memory alloy is changed under the influence of temperature, is used for reservoir plugging construction, can expand to form a plugging layer at the reservoir temperature, and can be used for reducing the temperature of a near-shaft reservoir by adopting a clear water circulation mode in the later period. The plugging material shrinks, the plugging layer is damaged, the plugging material in the oil-gas seepage channel flows back, the oil-gas seepage channel is liberated, the later oil-gas yield is not affected, and the yield and development efficiency are improved. 本发明提出了一种桥接堵漏浆及制备方法。通过桥接堵漏浆中的具有双程效应的形状记忆合金,利用其受温度影响形状发生变化的特点,组成具有良好返排能力的新型堵漏浆,用于储层堵漏施工,在储层温度下能够膨胀形成封堵层,后期采用清水循环的方式降低近井筒储层温度时,堵漏材料收缩,封堵层破坏,油气渗透通道内的堵漏材料返排出来,解放油气渗流通道
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116064009A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116064009A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116064009A3</originalsourceid><addsrcrecordid>eNrjZDB3KspMSc_MS1coyClNBzOKc0qLiioVEvNSFAqKUgsSixJLMvPzFHJTSzLyUxRKMlKLUvPTeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoaGZgZmJgYGlozExagACfS5O</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Bridging plugging slurry and preparation method thereof</title><source>esp@cenet</source><creator>CHEN ZENGWEI ; SONG BITAO ; LI DAQI ; OU BIAO ; LI FAN ; LIU JINHUA ; CHEN ZHIHUI ; REN MAO ; ZHANG DUJIE</creator><creatorcontrib>CHEN ZENGWEI ; SONG BITAO ; LI DAQI ; OU BIAO ; LI FAN ; LIU JINHUA ; CHEN ZHIHUI ; REN MAO ; ZHANG DUJIE</creatorcontrib><description>The invention provides bridging plugging slurry and a preparation method thereof. The novel plugging slurry with good flowback capability is formed by bridging the shape memory alloy with the two-way effect in the plugging slurry and utilizing the characteristic that the shape of the shape memory alloy is changed under the influence of temperature, is used for reservoir plugging construction, can expand to form a plugging layer at the reservoir temperature, and can be used for reducing the temperature of a near-shaft reservoir by adopting a clear water circulation mode in the later period. The plugging material shrinks, the plugging layer is damaged, the plugging material in the oil-gas seepage channel flows back, the oil-gas seepage channel is liberated, the later oil-gas yield is not affected, and the yield and development efficiency are improved. 本发明提出了一种桥接堵漏浆及制备方法。通过桥接堵漏浆中的具有双程效应的形状记忆合金,利用其受温度影响形状发生变化的特点,组成具有良好返排能力的新型堵漏浆,用于储层堵漏施工,在储层温度下能够膨胀形成封堵层,后期采用清水循环的方式降低近井筒储层温度时,堵漏材料收缩,封堵层破坏,油气渗透通道内的堵漏材料返排出来,解放油气渗流通道</description><language>chi ; eng</language><subject>ADHESIVES ; CHEMISTRY ; DYES ; MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; PAINTS ; POLISHES</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230505&amp;DB=EPODOC&amp;CC=CN&amp;NR=116064009A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230505&amp;DB=EPODOC&amp;CC=CN&amp;NR=116064009A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CHEN ZENGWEI</creatorcontrib><creatorcontrib>SONG BITAO</creatorcontrib><creatorcontrib>LI DAQI</creatorcontrib><creatorcontrib>OU BIAO</creatorcontrib><creatorcontrib>LI FAN</creatorcontrib><creatorcontrib>LIU JINHUA</creatorcontrib><creatorcontrib>CHEN ZHIHUI</creatorcontrib><creatorcontrib>REN MAO</creatorcontrib><creatorcontrib>ZHANG DUJIE</creatorcontrib><title>Bridging plugging slurry and preparation method thereof</title><description>The invention provides bridging plugging slurry and a preparation method thereof. The novel plugging slurry with good flowback capability is formed by bridging the shape memory alloy with the two-way effect in the plugging slurry and utilizing the characteristic that the shape of the shape memory alloy is changed under the influence of temperature, is used for reservoir plugging construction, can expand to form a plugging layer at the reservoir temperature, and can be used for reducing the temperature of a near-shaft reservoir by adopting a clear water circulation mode in the later period. The plugging material shrinks, the plugging layer is damaged, the plugging material in the oil-gas seepage channel flows back, the oil-gas seepage channel is liberated, the later oil-gas yield is not affected, and the yield and development efficiency are improved. 本发明提出了一种桥接堵漏浆及制备方法。通过桥接堵漏浆中的具有双程效应的形状记忆合金,利用其受温度影响形状发生变化的特点,组成具有良好返排能力的新型堵漏浆,用于储层堵漏施工,在储层温度下能够膨胀形成封堵层,后期采用清水循环的方式降低近井筒储层温度时,堵漏材料收缩,封堵层破坏,油气渗透通道内的堵漏材料返排出来,解放油气渗流通道</description><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>DYES</subject><subject>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>PAINTS</subject><subject>POLISHES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDB3KspMSc_MS1coyClNBzOKc0qLiioVEvNSFAqKUgsSixJLMvPzFHJTSzLyUxRKMlKLUvPTeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoaGZgZmJgYGlozExagACfS5O</recordid><startdate>20230505</startdate><enddate>20230505</enddate><creator>CHEN ZENGWEI</creator><creator>SONG BITAO</creator><creator>LI DAQI</creator><creator>OU BIAO</creator><creator>LI FAN</creator><creator>LIU JINHUA</creator><creator>CHEN ZHIHUI</creator><creator>REN MAO</creator><creator>ZHANG DUJIE</creator><scope>EVB</scope></search><sort><creationdate>20230505</creationdate><title>Bridging plugging slurry and preparation method thereof</title><author>CHEN ZENGWEI ; SONG BITAO ; LI DAQI ; OU BIAO ; LI FAN ; LIU JINHUA ; CHEN ZHIHUI ; REN MAO ; ZHANG DUJIE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116064009A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>DYES</topic><topic>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>PAINTS</topic><topic>POLISHES</topic><toplevel>online_resources</toplevel><creatorcontrib>CHEN ZENGWEI</creatorcontrib><creatorcontrib>SONG BITAO</creatorcontrib><creatorcontrib>LI DAQI</creatorcontrib><creatorcontrib>OU BIAO</creatorcontrib><creatorcontrib>LI FAN</creatorcontrib><creatorcontrib>LIU JINHUA</creatorcontrib><creatorcontrib>CHEN ZHIHUI</creatorcontrib><creatorcontrib>REN MAO</creatorcontrib><creatorcontrib>ZHANG DUJIE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CHEN ZENGWEI</au><au>SONG BITAO</au><au>LI DAQI</au><au>OU BIAO</au><au>LI FAN</au><au>LIU JINHUA</au><au>CHEN ZHIHUI</au><au>REN MAO</au><au>ZHANG DUJIE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Bridging plugging slurry and preparation method thereof</title><date>2023-05-05</date><risdate>2023</risdate><abstract>The invention provides bridging plugging slurry and a preparation method thereof. The novel plugging slurry with good flowback capability is formed by bridging the shape memory alloy with the two-way effect in the plugging slurry and utilizing the characteristic that the shape of the shape memory alloy is changed under the influence of temperature, is used for reservoir plugging construction, can expand to form a plugging layer at the reservoir temperature, and can be used for reducing the temperature of a near-shaft reservoir by adopting a clear water circulation mode in the later period. The plugging material shrinks, the plugging layer is damaged, the plugging material in the oil-gas seepage channel flows back, the oil-gas seepage channel is liberated, the later oil-gas yield is not affected, and the yield and development efficiency are improved. 本发明提出了一种桥接堵漏浆及制备方法。通过桥接堵漏浆中的具有双程效应的形状记忆合金,利用其受温度影响形状发生变化的特点,组成具有良好返排能力的新型堵漏浆,用于储层堵漏施工,在储层温度下能够膨胀形成封堵层,后期采用清水循环的方式降低近井筒储层温度时,堵漏材料收缩,封堵层破坏,油气渗透通道内的堵漏材料返排出来,解放油气渗流通道</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116064009A
source esp@cenet
subjects ADHESIVES
CHEMISTRY
DYES
MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
PAINTS
POLISHES
title Bridging plugging slurry and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-22T18%3A13%3A34IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CHEN%20ZENGWEI&rft.date=2023-05-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116064009A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true