Preparation method of oxygen-free mirror copper strip

The invention discloses a preparation method of a mirror surface oxygen-free copper strip. The preparation method is characterized in that the technological process of the mirror surface oxygen-free copper strip comprises the steps of smelting, casting, continuous extrusion and stretching; the conti...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG XIONGFENG, CHEN WEIDONG, ZHENG LIANGYU, LIU QUAN, SHUI XINPING, XU CHAO, YUAN LEILEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG XIONGFENG
CHEN WEIDONG
ZHENG LIANGYU
LIU QUAN
SHUI XINPING
XU CHAO
YUAN LEILEI
description The invention discloses a preparation method of a mirror surface oxygen-free copper strip. The preparation method is characterized in that the technological process of the mirror surface oxygen-free copper strip comprises the steps of smelting, casting, continuous extrusion and stretching; the continuous extrusion process comprises the steps that a cast ingot enters an extrusion die after passing through a cavity of a continuous extrusion machine, an extrusion blank is obtained, the cavity comprises an outlet section, the extrusion die is arranged at an outlet of the outlet section, the outlet section is communicated with the extrusion die through a forming piece, and the forming piece is provided with a forming cavity; the forming cavity comprises a middle area and edge areas arranged at the two ends of the middle area in the width direction of the copper strip, and the cross section area ratio of the middle area to the edge areas is 1: (1.5-3). 本发明公开了一种镜面无氧铜带的制备方法,其特征在于:该镜面无氧铜带的工艺流程包括熔炼→铸造→连续挤压→拉伸;所述连续挤压工艺为
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116037687A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116037687A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116037687A3</originalsourceid><addsrcrecordid>eNrjZDANKEotSCxKLMnMz1PITS3JyE9RyE9TyK-oTE_N000rSk1VyM0sKsovUkjOLyhILVIoLinKLOBhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfHOfoaGZgbG5mYW5o7GxKgBAIrULYQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of oxygen-free mirror copper strip</title><source>esp@cenet</source><creator>WANG XIONGFENG ; CHEN WEIDONG ; ZHENG LIANGYU ; LIU QUAN ; SHUI XINPING ; XU CHAO ; YUAN LEILEI</creator><creatorcontrib>WANG XIONGFENG ; CHEN WEIDONG ; ZHENG LIANGYU ; LIU QUAN ; SHUI XINPING ; XU CHAO ; YUAN LEILEI</creatorcontrib><description>The invention discloses a preparation method of a mirror surface oxygen-free copper strip. The preparation method is characterized in that the technological process of the mirror surface oxygen-free copper strip comprises the steps of smelting, casting, continuous extrusion and stretching; the continuous extrusion process comprises the steps that a cast ingot enters an extrusion die after passing through a cavity of a continuous extrusion machine, an extrusion blank is obtained, the cavity comprises an outlet section, the extrusion die is arranged at an outlet of the outlet section, the outlet section is communicated with the extrusion die through a forming piece, and the forming piece is provided with a forming cavity; the forming cavity comprises a middle area and edge areas arranged at the two ends of the middle area in the width direction of the copper strip, and the cross section area ratio of the middle area to the edge areas is 1: (1.5-3). 本发明公开了一种镜面无氧铜带的制备方法,其特征在于:该镜面无氧铜带的工艺流程包括熔炼→铸造→连续挤压→拉伸;所述连续挤压工艺为</description><language>chi ; eng</language><subject>AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL ; MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; PERFORMING OPERATIONS ; PUNCHING METAL ; TRANSPORTING</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230502&amp;DB=EPODOC&amp;CC=CN&amp;NR=116037687A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230502&amp;DB=EPODOC&amp;CC=CN&amp;NR=116037687A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG XIONGFENG</creatorcontrib><creatorcontrib>CHEN WEIDONG</creatorcontrib><creatorcontrib>ZHENG LIANGYU</creatorcontrib><creatorcontrib>LIU QUAN</creatorcontrib><creatorcontrib>SHUI XINPING</creatorcontrib><creatorcontrib>XU CHAO</creatorcontrib><creatorcontrib>YUAN LEILEI</creatorcontrib><title>Preparation method of oxygen-free mirror copper strip</title><description>The invention discloses a preparation method of a mirror surface oxygen-free copper strip. The preparation method is characterized in that the technological process of the mirror surface oxygen-free copper strip comprises the steps of smelting, casting, continuous extrusion and stretching; the continuous extrusion process comprises the steps that a cast ingot enters an extrusion die after passing through a cavity of a continuous extrusion machine, an extrusion blank is obtained, the cavity comprises an outlet section, the extrusion die is arranged at an outlet of the outlet section, the outlet section is communicated with the extrusion die through a forming piece, and the forming piece is provided with a forming cavity; the forming cavity comprises a middle area and edge areas arranged at the two ends of the middle area in the width direction of the copper strip, and the cross section area ratio of the middle area to the edge areas is 1: (1.5-3). 本发明公开了一种镜面无氧铜带的制备方法,其特征在于:该镜面无氧铜带的工艺流程包括熔炼→铸造→连续挤压→拉伸;所述连续挤压工艺为</description><subject>AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL</subject><subject>MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDANKEotSCxKLMnMz1PITS3JyE9RyE9TyK-oTE_N000rSk1VyM0sKsovUkjOLyhILVIoLinKLOBhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfHOfoaGZgbG5mYW5o7GxKgBAIrULYQ</recordid><startdate>20230502</startdate><enddate>20230502</enddate><creator>WANG XIONGFENG</creator><creator>CHEN WEIDONG</creator><creator>ZHENG LIANGYU</creator><creator>LIU QUAN</creator><creator>SHUI XINPING</creator><creator>XU CHAO</creator><creator>YUAN LEILEI</creator><scope>EVB</scope></search><sort><creationdate>20230502</creationdate><title>Preparation method of oxygen-free mirror copper strip</title><author>WANG XIONGFENG ; CHEN WEIDONG ; ZHENG LIANGYU ; LIU QUAN ; SHUI XINPING ; XU CHAO ; YUAN LEILEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116037687A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL</topic><topic>MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG XIONGFENG</creatorcontrib><creatorcontrib>CHEN WEIDONG</creatorcontrib><creatorcontrib>ZHENG LIANGYU</creatorcontrib><creatorcontrib>LIU QUAN</creatorcontrib><creatorcontrib>SHUI XINPING</creatorcontrib><creatorcontrib>XU CHAO</creatorcontrib><creatorcontrib>YUAN LEILEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG XIONGFENG</au><au>CHEN WEIDONG</au><au>ZHENG LIANGYU</au><au>LIU QUAN</au><au>SHUI XINPING</au><au>XU CHAO</au><au>YUAN LEILEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of oxygen-free mirror copper strip</title><date>2023-05-02</date><risdate>2023</risdate><abstract>The invention discloses a preparation method of a mirror surface oxygen-free copper strip. The preparation method is characterized in that the technological process of the mirror surface oxygen-free copper strip comprises the steps of smelting, casting, continuous extrusion and stretching; the continuous extrusion process comprises the steps that a cast ingot enters an extrusion die after passing through a cavity of a continuous extrusion machine, an extrusion blank is obtained, the cavity comprises an outlet section, the extrusion die is arranged at an outlet of the outlet section, the outlet section is communicated with the extrusion die through a forming piece, and the forming piece is provided with a forming cavity; the forming cavity comprises a middle area and edge areas arranged at the two ends of the middle area in the width direction of the copper strip, and the cross section area ratio of the middle area to the edge areas is 1: (1.5-3). 本发明公开了一种镜面无氧铜带的制备方法,其特征在于:该镜面无氧铜带的工艺流程包括熔炼→铸造→连续挤压→拉伸;所述连续挤压工艺为</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116037687A
source esp@cenet
subjects AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL
MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
PERFORMING OPERATIONS
PUNCHING METAL
TRANSPORTING
title Preparation method of oxygen-free mirror copper strip
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T18%3A21%3A16IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20XIONGFENG&rft.date=2023-05-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116037687A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true