Cotton fiber pretreatment process with stepped temperature rise
The invention discloses a step-heating cotton fiber pretreatment process which comprises the following steps: step 1) adding materials at normal temperature: putting cotton fibers into a scouring and bleaching solution, and adding a KA pretreatment agent into the scouring and bleaching solution; (2)...
Gespeichert in:
Hauptverfasser: | , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | DING WENJUN LIAO YALI CHEN DONG OH BYUNG-SEOK XU QINGLIN WANG XIUCHUN CHU WEIFA ZHU SHOUCHENG LIU GUOQING |
description | The invention discloses a step-heating cotton fiber pretreatment process which comprises the following steps: step 1) adding materials at normal temperature: putting cotton fibers into a scouring and bleaching solution, and adding a KA pretreatment agent into the scouring and bleaching solution; (2) primary heating and heat preservation: after the primary heating temperature reaches 45-55 DEG C, heat preservation is conducted for 20 min; 3) secondary charging: adding caustic soda and hydrogen peroxide; 4) carrying out secondary heating and heat preservation; 5) cooling and discharging liquid; 6) washing with hot water; 7) washing with cold water; and 8) acid neutralization. Compared with a traditional direct heating production process, the stepped heating pretreatment process provided by the invention has the advantages that energy is saved, the production efficiency is improved, and the treated cotton fabric is good in whiteness, capillary effect and hand feeling, high in practicability, safe and environment |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115897212A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115897212A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115897212A3</originalsourceid><addsrcrecordid>eNrjZLB3zi8pyc9TSMtMSi1SKChKLSlKTSzJTc0rAXLyk1OLixXKM0syFIpLUgsKUlMUSlJzC1KLEktKi1IVijKLU3kYWNMSc4pTeaE0N4Oim2uIs4duakF-fGpxQWJyal5qSbyzn6GhqYWluZGhkaMxMWoA7QMxuQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Cotton fiber pretreatment process with stepped temperature rise</title><source>esp@cenet</source><creator>DING WENJUN ; LIAO YALI ; CHEN DONG ; OH BYUNG-SEOK ; XU QINGLIN ; WANG XIUCHUN ; CHU WEIFA ; ZHU SHOUCHENG ; LIU GUOQING</creator><creatorcontrib>DING WENJUN ; LIAO YALI ; CHEN DONG ; OH BYUNG-SEOK ; XU QINGLIN ; WANG XIUCHUN ; CHU WEIFA ; ZHU SHOUCHENG ; LIU GUOQING</creatorcontrib><description>The invention discloses a step-heating cotton fiber pretreatment process which comprises the following steps: step 1) adding materials at normal temperature: putting cotton fibers into a scouring and bleaching solution, and adding a KA pretreatment agent into the scouring and bleaching solution; (2) primary heating and heat preservation: after the primary heating temperature reaches 45-55 DEG C, heat preservation is conducted for 20 min; 3) secondary charging: adding caustic soda and hydrogen peroxide; 4) carrying out secondary heating and heat preservation; 5) cooling and discharging liquid; 6) washing with hot water; 7) washing with cold water; and 8) acid neutralization. Compared with a traditional direct heating production process, the stepped heating pretreatment process provided by the invention has the advantages that energy is saved, the production efficiency is improved, and the treated cotton fabric is good in whiteness, capillary effect and hand feeling, high in practicability, safe and environment</description><language>chi ; eng</language><subject>BLEACHING LEATHER OR FURS ; DRY-CLEANING, WASHING OR BLEACHING FIBRES, FILAMENTS, THREADS,YARNS, FABRICS, FEATHERS OR MADE-UP FIBROUS GOODS ; FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR ; LAUNDERING ; TEXTILES ; TREATMENT OF TEXTILES OR THE LIKE</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230404&DB=EPODOC&CC=CN&NR=115897212A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230404&DB=EPODOC&CC=CN&NR=115897212A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DING WENJUN</creatorcontrib><creatorcontrib>LIAO YALI</creatorcontrib><creatorcontrib>CHEN DONG</creatorcontrib><creatorcontrib>OH BYUNG-SEOK</creatorcontrib><creatorcontrib>XU QINGLIN</creatorcontrib><creatorcontrib>WANG XIUCHUN</creatorcontrib><creatorcontrib>CHU WEIFA</creatorcontrib><creatorcontrib>ZHU SHOUCHENG</creatorcontrib><creatorcontrib>LIU GUOQING</creatorcontrib><title>Cotton fiber pretreatment process with stepped temperature rise</title><description>The invention discloses a step-heating cotton fiber pretreatment process which comprises the following steps: step 1) adding materials at normal temperature: putting cotton fibers into a scouring and bleaching solution, and adding a KA pretreatment agent into the scouring and bleaching solution; (2) primary heating and heat preservation: after the primary heating temperature reaches 45-55 DEG C, heat preservation is conducted for 20 min; 3) secondary charging: adding caustic soda and hydrogen peroxide; 4) carrying out secondary heating and heat preservation; 5) cooling and discharging liquid; 6) washing with hot water; 7) washing with cold water; and 8) acid neutralization. Compared with a traditional direct heating production process, the stepped heating pretreatment process provided by the invention has the advantages that energy is saved, the production efficiency is improved, and the treated cotton fabric is good in whiteness, capillary effect and hand feeling, high in practicability, safe and environment</description><subject>BLEACHING LEATHER OR FURS</subject><subject>DRY-CLEANING, WASHING OR BLEACHING FIBRES, FILAMENTS, THREADS,YARNS, FABRICS, FEATHERS OR MADE-UP FIBROUS GOODS</subject><subject>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</subject><subject>LAUNDERING</subject><subject>TEXTILES</subject><subject>TREATMENT OF TEXTILES OR THE LIKE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLB3zi8pyc9TSMtMSi1SKChKLSlKTSzJTc0rAXLyk1OLixXKM0syFIpLUgsKUlMUSlJzC1KLEktKi1IVijKLU3kYWNMSc4pTeaE0N4Oim2uIs4duakF-fGpxQWJyal5qSbyzn6GhqYWluZGhkaMxMWoA7QMxuQ</recordid><startdate>20230404</startdate><enddate>20230404</enddate><creator>DING WENJUN</creator><creator>LIAO YALI</creator><creator>CHEN DONG</creator><creator>OH BYUNG-SEOK</creator><creator>XU QINGLIN</creator><creator>WANG XIUCHUN</creator><creator>CHU WEIFA</creator><creator>ZHU SHOUCHENG</creator><creator>LIU GUOQING</creator><scope>EVB</scope></search><sort><creationdate>20230404</creationdate><title>Cotton fiber pretreatment process with stepped temperature rise</title><author>DING WENJUN ; LIAO YALI ; CHEN DONG ; OH BYUNG-SEOK ; XU QINGLIN ; WANG XIUCHUN ; CHU WEIFA ; ZHU SHOUCHENG ; LIU GUOQING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115897212A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>BLEACHING LEATHER OR FURS</topic><topic>DRY-CLEANING, WASHING OR BLEACHING FIBRES, FILAMENTS, THREADS,YARNS, FABRICS, FEATHERS OR MADE-UP FIBROUS GOODS</topic><topic>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</topic><topic>LAUNDERING</topic><topic>TEXTILES</topic><topic>TREATMENT OF TEXTILES OR THE LIKE</topic><toplevel>online_resources</toplevel><creatorcontrib>DING WENJUN</creatorcontrib><creatorcontrib>LIAO YALI</creatorcontrib><creatorcontrib>CHEN DONG</creatorcontrib><creatorcontrib>OH BYUNG-SEOK</creatorcontrib><creatorcontrib>XU QINGLIN</creatorcontrib><creatorcontrib>WANG XIUCHUN</creatorcontrib><creatorcontrib>CHU WEIFA</creatorcontrib><creatorcontrib>ZHU SHOUCHENG</creatorcontrib><creatorcontrib>LIU GUOQING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DING WENJUN</au><au>LIAO YALI</au><au>CHEN DONG</au><au>OH BYUNG-SEOK</au><au>XU QINGLIN</au><au>WANG XIUCHUN</au><au>CHU WEIFA</au><au>ZHU SHOUCHENG</au><au>LIU GUOQING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Cotton fiber pretreatment process with stepped temperature rise</title><date>2023-04-04</date><risdate>2023</risdate><abstract>The invention discloses a step-heating cotton fiber pretreatment process which comprises the following steps: step 1) adding materials at normal temperature: putting cotton fibers into a scouring and bleaching solution, and adding a KA pretreatment agent into the scouring and bleaching solution; (2) primary heating and heat preservation: after the primary heating temperature reaches 45-55 DEG C, heat preservation is conducted for 20 min; 3) secondary charging: adding caustic soda and hydrogen peroxide; 4) carrying out secondary heating and heat preservation; 5) cooling and discharging liquid; 6) washing with hot water; 7) washing with cold water; and 8) acid neutralization. Compared with a traditional direct heating production process, the stepped heating pretreatment process provided by the invention has the advantages that energy is saved, the production efficiency is improved, and the treated cotton fabric is good in whiteness, capillary effect and hand feeling, high in practicability, safe and environment</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN115897212A |
source | esp@cenet |
subjects | BLEACHING LEATHER OR FURS DRY-CLEANING, WASHING OR BLEACHING FIBRES, FILAMENTS, THREADS,YARNS, FABRICS, FEATHERS OR MADE-UP FIBROUS GOODS FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR LAUNDERING TEXTILES TREATMENT OF TEXTILES OR THE LIKE |
title | Cotton fiber pretreatment process with stepped temperature rise |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T20%3A13%3A23IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DING%20WENJUN&rft.date=2023-04-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115897212A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |