Method for preparing cadmium phosphide from copper-cadmium slag

The invention relates to a method for preparing cadmium phosphide by using copper-cadmium slag, which comprises the following steps: (1) oxidizing and acid leaching: mixing the copper-cadmium slag, ammonium dichromate and water, stirring to react, controlling the pH value at the end point to be 5-5....

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YAO YINGFENG, FANG YANXIA, WU KEFU, WANG YUANRUI, SUN SHUAINAN, WANG YAPING, MA JIANFEI, ZHANG YANCUI, ZHAN ZHIWANG, WANG HONGYAN, GUO YONGHONG, PANG ZHENYE, NIU YONGSHENG, GONG YANFEI, YANG YANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YAO YINGFENG
FANG YANXIA
WU KEFU
WANG YUANRUI
SUN SHUAINAN
WANG YAPING
MA JIANFEI
ZHANG YANCUI
ZHAN ZHIWANG
WANG HONGYAN
GUO YONGHONG
PANG ZHENYE
NIU YONGSHENG
GONG YANFEI
YANG YANG
description The invention relates to a method for preparing cadmium phosphide by using copper-cadmium slag, which comprises the following steps: (1) oxidizing and acid leaching: mixing the copper-cadmium slag, ammonium dichromate and water, stirring to react, controlling the pH value at the end point to be 5-5.2, and performing solid-liquid separation to respectively obtain a mixed solution of zinc sulfate and chromium sulfate and a solid phase; (2) zinc and chromium separation: adding ammonia water into the mixed solution of zinc sulfate and chromium sulfate for chromium precipitation reaction to respectively obtain a [Zn (NH3) 4] (OH) 2 solution and a mixed precipitate of chromium hydroxide and chromium oxysulfate; (3) copper and cadmium separation: adding a sulfuric acid solution and water into the solid phase for acid leaching reaction to respectively obtain a cadmium sulfate solution and copper slag with the copper content of more than 90%; and (4) preparing cadmium phosphide: pumping the cadmium sulfate solution in
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115896457A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115896457A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115896457A3</originalsourceid><addsrcrecordid>eNrjZLD3TS3JyE9RSMsvUigoSi1ILMrMS1dITkzJzSzNVSjIyC8uyMhMSVVIK8rPVUjOLyhILdKFyRbnJKbzMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DQ1MLSzMTU3NHY2LUAACi9jEn</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing cadmium phosphide from copper-cadmium slag</title><source>esp@cenet</source><creator>YAO YINGFENG ; FANG YANXIA ; WU KEFU ; WANG YUANRUI ; SUN SHUAINAN ; WANG YAPING ; MA JIANFEI ; ZHANG YANCUI ; ZHAN ZHIWANG ; WANG HONGYAN ; GUO YONGHONG ; PANG ZHENYE ; NIU YONGSHENG ; GONG YANFEI ; YANG YANG</creator><creatorcontrib>YAO YINGFENG ; FANG YANXIA ; WU KEFU ; WANG YUANRUI ; SUN SHUAINAN ; WANG YAPING ; MA JIANFEI ; ZHANG YANCUI ; ZHAN ZHIWANG ; WANG HONGYAN ; GUO YONGHONG ; PANG ZHENYE ; NIU YONGSHENG ; GONG YANFEI ; YANG YANG</creatorcontrib><description>The invention relates to a method for preparing cadmium phosphide by using copper-cadmium slag, which comprises the following steps: (1) oxidizing and acid leaching: mixing the copper-cadmium slag, ammonium dichromate and water, stirring to react, controlling the pH value at the end point to be 5-5.2, and performing solid-liquid separation to respectively obtain a mixed solution of zinc sulfate and chromium sulfate and a solid phase; (2) zinc and chromium separation: adding ammonia water into the mixed solution of zinc sulfate and chromium sulfate for chromium precipitation reaction to respectively obtain a [Zn (NH3) 4] (OH) 2 solution and a mixed precipitate of chromium hydroxide and chromium oxysulfate; (3) copper and cadmium separation: adding a sulfuric acid solution and water into the solid phase for acid leaching reaction to respectively obtain a cadmium sulfate solution and copper slag with the copper content of more than 90%; and (4) preparing cadmium phosphide: pumping the cadmium sulfate solution in</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; FERROUS OR NON-FERROUS ALLOYS ; INORGANIC CHEMISTRY ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230404&amp;DB=EPODOC&amp;CC=CN&amp;NR=115896457A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230404&amp;DB=EPODOC&amp;CC=CN&amp;NR=115896457A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YAO YINGFENG</creatorcontrib><creatorcontrib>FANG YANXIA</creatorcontrib><creatorcontrib>WU KEFU</creatorcontrib><creatorcontrib>WANG YUANRUI</creatorcontrib><creatorcontrib>SUN SHUAINAN</creatorcontrib><creatorcontrib>WANG YAPING</creatorcontrib><creatorcontrib>MA JIANFEI</creatorcontrib><creatorcontrib>ZHANG YANCUI</creatorcontrib><creatorcontrib>ZHAN ZHIWANG</creatorcontrib><creatorcontrib>WANG HONGYAN</creatorcontrib><creatorcontrib>GUO YONGHONG</creatorcontrib><creatorcontrib>PANG ZHENYE</creatorcontrib><creatorcontrib>NIU YONGSHENG</creatorcontrib><creatorcontrib>GONG YANFEI</creatorcontrib><creatorcontrib>YANG YANG</creatorcontrib><title>Method for preparing cadmium phosphide from copper-cadmium slag</title><description>The invention relates to a method for preparing cadmium phosphide by using copper-cadmium slag, which comprises the following steps: (1) oxidizing and acid leaching: mixing the copper-cadmium slag, ammonium dichromate and water, stirring to react, controlling the pH value at the end point to be 5-5.2, and performing solid-liquid separation to respectively obtain a mixed solution of zinc sulfate and chromium sulfate and a solid phase; (2) zinc and chromium separation: adding ammonia water into the mixed solution of zinc sulfate and chromium sulfate for chromium precipitation reaction to respectively obtain a [Zn (NH3) 4] (OH) 2 solution and a mixed precipitate of chromium hydroxide and chromium oxysulfate; (3) copper and cadmium separation: adding a sulfuric acid solution and water into the solid phase for acid leaching reaction to respectively obtain a cadmium sulfate solution and copper slag with the copper content of more than 90%; and (4) preparing cadmium phosphide: pumping the cadmium sulfate solution in</description><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLD3TS3JyE9RSMsvUigoSi1ILMrMS1dITkzJzSzNVSjIyC8uyMhMSVVIK8rPVUjOLyhILdKFyRbnJKbzMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DQ1MLSzMTU3NHY2LUAACi9jEn</recordid><startdate>20230404</startdate><enddate>20230404</enddate><creator>YAO YINGFENG</creator><creator>FANG YANXIA</creator><creator>WU KEFU</creator><creator>WANG YUANRUI</creator><creator>SUN SHUAINAN</creator><creator>WANG YAPING</creator><creator>MA JIANFEI</creator><creator>ZHANG YANCUI</creator><creator>ZHAN ZHIWANG</creator><creator>WANG HONGYAN</creator><creator>GUO YONGHONG</creator><creator>PANG ZHENYE</creator><creator>NIU YONGSHENG</creator><creator>GONG YANFEI</creator><creator>YANG YANG</creator><scope>EVB</scope></search><sort><creationdate>20230404</creationdate><title>Method for preparing cadmium phosphide from copper-cadmium slag</title><author>YAO YINGFENG ; FANG YANXIA ; WU KEFU ; WANG YUANRUI ; SUN SHUAINAN ; WANG YAPING ; MA JIANFEI ; ZHANG YANCUI ; ZHAN ZHIWANG ; WANG HONGYAN ; GUO YONGHONG ; PANG ZHENYE ; NIU YONGSHENG ; GONG YANFEI ; YANG YANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115896457A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>YAO YINGFENG</creatorcontrib><creatorcontrib>FANG YANXIA</creatorcontrib><creatorcontrib>WU KEFU</creatorcontrib><creatorcontrib>WANG YUANRUI</creatorcontrib><creatorcontrib>SUN SHUAINAN</creatorcontrib><creatorcontrib>WANG YAPING</creatorcontrib><creatorcontrib>MA JIANFEI</creatorcontrib><creatorcontrib>ZHANG YANCUI</creatorcontrib><creatorcontrib>ZHAN ZHIWANG</creatorcontrib><creatorcontrib>WANG HONGYAN</creatorcontrib><creatorcontrib>GUO YONGHONG</creatorcontrib><creatorcontrib>PANG ZHENYE</creatorcontrib><creatorcontrib>NIU YONGSHENG</creatorcontrib><creatorcontrib>GONG YANFEI</creatorcontrib><creatorcontrib>YANG YANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YAO YINGFENG</au><au>FANG YANXIA</au><au>WU KEFU</au><au>WANG YUANRUI</au><au>SUN SHUAINAN</au><au>WANG YAPING</au><au>MA JIANFEI</au><au>ZHANG YANCUI</au><au>ZHAN ZHIWANG</au><au>WANG HONGYAN</au><au>GUO YONGHONG</au><au>PANG ZHENYE</au><au>NIU YONGSHENG</au><au>GONG YANFEI</au><au>YANG YANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing cadmium phosphide from copper-cadmium slag</title><date>2023-04-04</date><risdate>2023</risdate><abstract>The invention relates to a method for preparing cadmium phosphide by using copper-cadmium slag, which comprises the following steps: (1) oxidizing and acid leaching: mixing the copper-cadmium slag, ammonium dichromate and water, stirring to react, controlling the pH value at the end point to be 5-5.2, and performing solid-liquid separation to respectively obtain a mixed solution of zinc sulfate and chromium sulfate and a solid phase; (2) zinc and chromium separation: adding ammonia water into the mixed solution of zinc sulfate and chromium sulfate for chromium precipitation reaction to respectively obtain a [Zn (NH3) 4] (OH) 2 solution and a mixed precipitate of chromium hydroxide and chromium oxysulfate; (3) copper and cadmium separation: adding a sulfuric acid solution and water into the solid phase for acid leaching reaction to respectively obtain a cadmium sulfate solution and copper slag with the copper content of more than 90%; and (4) preparing cadmium phosphide: pumping the cadmium sulfate solution in</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN115896457A
source esp@cenet
subjects CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
FERROUS OR NON-FERROUS ALLOYS
INORGANIC CHEMISTRY
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Method for preparing cadmium phosphide from copper-cadmium slag
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T17%3A15%3A52IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YAO%20YINGFENG&rft.date=2023-04-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115896457A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true