Starting method for zinc hydrometallurgy of high-copper-content electrolyte
The invention discloses a starting method for zinc hydrometallurgy of a high-copper-content electrolyte, and belongs to the technical field of zinc hydrometallurgy electrodeposition. The method mainly comprises the following steps: fully circulating electrolyte before starting up; a cathode plate is...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | MA WEIQIANG HUANG HAINING ZHONG LEI ZHANG YAFEI ZHANG GUANGGUANG ZHONG YU SUN TENGLI GONG YANFEI LI HUQI YANG LIPING |
description | The invention discloses a starting method for zinc hydrometallurgy of a high-copper-content electrolyte, and belongs to the technical field of zinc hydrometallurgy electrodeposition. The method mainly comprises the following steps: fully circulating electrolyte before starting up; a cathode plate is arranged in the electrolytic bath, so that the electrolytic bath forms a circuit loop; supplying direct current; the direct-current power supply amount is gradually increased to meet normal production requirements; after the capacitor is turned on, the temperature of the electrolyte is kept below 32 DEG C within 4 hours; the acid content of the electrolyte is kept below 195 g/l; the precipitation condition is observed, and if the plate burning phenomenon does not exist, normal electrodeposition production can be carried out; observing a plate burning phenomenon in precipitation; adding a large amount of new solution to replace the circulating electrolyte; and after it is observed that cathode zinc is normally sepa |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115747881A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115747881A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115747881A3</originalsourceid><addsrcrecordid>eNrjZPAOLkksKsnMS1fITS3JyE9RSMsvUqjKzEtWyKhMKcoHCibm5JQWpVcq5KcpZGSmZ-gm5xcUpBYBqbyS1LwShdSc1OSSovycypJUHgbWtMSc4lReKM3NoOjmGuLsoZtakB-fWlyQmJyal1oS7-xnaGhqbmJuYWHoaEyMGgDATzZZ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Starting method for zinc hydrometallurgy of high-copper-content electrolyte</title><source>esp@cenet</source><creator>MA WEIQIANG ; HUANG HAINING ; ZHONG LEI ; ZHANG YAFEI ; ZHANG GUANGGUANG ; ZHONG YU ; SUN TENGLI ; GONG YANFEI ; LI HUQI ; YANG LIPING</creator><creatorcontrib>MA WEIQIANG ; HUANG HAINING ; ZHONG LEI ; ZHANG YAFEI ; ZHANG GUANGGUANG ; ZHONG YU ; SUN TENGLI ; GONG YANFEI ; LI HUQI ; YANG LIPING</creatorcontrib><description>The invention discloses a starting method for zinc hydrometallurgy of a high-copper-content electrolyte, and belongs to the technical field of zinc hydrometallurgy electrodeposition. The method mainly comprises the following steps: fully circulating electrolyte before starting up; a cathode plate is arranged in the electrolytic bath, so that the electrolytic bath forms a circuit loop; supplying direct current; the direct-current power supply amount is gradually increased to meet normal production requirements; after the capacitor is turned on, the temperature of the electrolyte is kept below 32 DEG C within 4 hours; the acid content of the electrolyte is kept below 195 g/l; the precipitation condition is observed, and if the plate burning phenomenon does not exist, normal electrodeposition production can be carried out; observing a plate burning phenomenon in precipitation; adding a large amount of new solution to replace the circulating electrolyte; and after it is observed that cathode zinc is normally sepa</description><language>chi ; eng</language><subject>APPARATUS THEREFOR ; CHEMISTRY ; ELECTROLYTIC OR ELECTROPHORETIC PROCESSES ; METALLURGY ; PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230307&DB=EPODOC&CC=CN&NR=115747881A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230307&DB=EPODOC&CC=CN&NR=115747881A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MA WEIQIANG</creatorcontrib><creatorcontrib>HUANG HAINING</creatorcontrib><creatorcontrib>ZHONG LEI</creatorcontrib><creatorcontrib>ZHANG YAFEI</creatorcontrib><creatorcontrib>ZHANG GUANGGUANG</creatorcontrib><creatorcontrib>ZHONG YU</creatorcontrib><creatorcontrib>SUN TENGLI</creatorcontrib><creatorcontrib>GONG YANFEI</creatorcontrib><creatorcontrib>LI HUQI</creatorcontrib><creatorcontrib>YANG LIPING</creatorcontrib><title>Starting method for zinc hydrometallurgy of high-copper-content electrolyte</title><description>The invention discloses a starting method for zinc hydrometallurgy of a high-copper-content electrolyte, and belongs to the technical field of zinc hydrometallurgy electrodeposition. The method mainly comprises the following steps: fully circulating electrolyte before starting up; a cathode plate is arranged in the electrolytic bath, so that the electrolytic bath forms a circuit loop; supplying direct current; the direct-current power supply amount is gradually increased to meet normal production requirements; after the capacitor is turned on, the temperature of the electrolyte is kept below 32 DEG C within 4 hours; the acid content of the electrolyte is kept below 195 g/l; the precipitation condition is observed, and if the plate burning phenomenon does not exist, normal electrodeposition production can be carried out; observing a plate burning phenomenon in precipitation; adding a large amount of new solution to replace the circulating electrolyte; and after it is observed that cathode zinc is normally sepa</description><subject>APPARATUS THEREFOR</subject><subject>CHEMISTRY</subject><subject>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</subject><subject>METALLURGY</subject><subject>PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPAOLkksKsnMS1fITS3JyE9RSMsvUqjKzEtWyKhMKcoHCibm5JQWpVcq5KcpZGSmZ-gm5xcUpBYBqbyS1LwShdSc1OSSovycypJUHgbWtMSc4lReKM3NoOjmGuLsoZtakB-fWlyQmJyal1oS7-xnaGhqbmJuYWHoaEyMGgDATzZZ</recordid><startdate>20230307</startdate><enddate>20230307</enddate><creator>MA WEIQIANG</creator><creator>HUANG HAINING</creator><creator>ZHONG LEI</creator><creator>ZHANG YAFEI</creator><creator>ZHANG GUANGGUANG</creator><creator>ZHONG YU</creator><creator>SUN TENGLI</creator><creator>GONG YANFEI</creator><creator>LI HUQI</creator><creator>YANG LIPING</creator><scope>EVB</scope></search><sort><creationdate>20230307</creationdate><title>Starting method for zinc hydrometallurgy of high-copper-content electrolyte</title><author>MA WEIQIANG ; HUANG HAINING ; ZHONG LEI ; ZHANG YAFEI ; ZHANG GUANGGUANG ; ZHONG YU ; SUN TENGLI ; GONG YANFEI ; LI HUQI ; YANG LIPING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115747881A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>APPARATUS THEREFOR</topic><topic>CHEMISTRY</topic><topic>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</topic><topic>METALLURGY</topic><topic>PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>MA WEIQIANG</creatorcontrib><creatorcontrib>HUANG HAINING</creatorcontrib><creatorcontrib>ZHONG LEI</creatorcontrib><creatorcontrib>ZHANG YAFEI</creatorcontrib><creatorcontrib>ZHANG GUANGGUANG</creatorcontrib><creatorcontrib>ZHONG YU</creatorcontrib><creatorcontrib>SUN TENGLI</creatorcontrib><creatorcontrib>GONG YANFEI</creatorcontrib><creatorcontrib>LI HUQI</creatorcontrib><creatorcontrib>YANG LIPING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MA WEIQIANG</au><au>HUANG HAINING</au><au>ZHONG LEI</au><au>ZHANG YAFEI</au><au>ZHANG GUANGGUANG</au><au>ZHONG YU</au><au>SUN TENGLI</au><au>GONG YANFEI</au><au>LI HUQI</au><au>YANG LIPING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Starting method for zinc hydrometallurgy of high-copper-content electrolyte</title><date>2023-03-07</date><risdate>2023</risdate><abstract>The invention discloses a starting method for zinc hydrometallurgy of a high-copper-content electrolyte, and belongs to the technical field of zinc hydrometallurgy electrodeposition. The method mainly comprises the following steps: fully circulating electrolyte before starting up; a cathode plate is arranged in the electrolytic bath, so that the electrolytic bath forms a circuit loop; supplying direct current; the direct-current power supply amount is gradually increased to meet normal production requirements; after the capacitor is turned on, the temperature of the electrolyte is kept below 32 DEG C within 4 hours; the acid content of the electrolyte is kept below 195 g/l; the precipitation condition is observed, and if the plate burning phenomenon does not exist, normal electrodeposition production can be carried out; observing a plate burning phenomenon in precipitation; adding a large amount of new solution to replace the circulating electrolyte; and after it is observed that cathode zinc is normally sepa</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN115747881A |
source | esp@cenet |
subjects | APPARATUS THEREFOR CHEMISTRY ELECTROLYTIC OR ELECTROPHORETIC PROCESSES METALLURGY PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS |
title | Starting method for zinc hydrometallurgy of high-copper-content electrolyte |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-06T11%3A16%3A12IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MA%20WEIQIANG&rft.date=2023-03-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115747881A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |