Hot-rolled round steel process for preventing mixed crystal of refined grains of hub bearing steel
The invention discloses a round steel hot rolling process for preventing mixed crystal of refined grains of steel for hub bearings, and relates to the technical field of steel production. The preheating section is less than or equal to 800 DEG C, the first heating section is less than or equal to 95...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | QIU JUNHUA WANG RUIZHANG ZHAO HAIYANG XU WEI |
description | The invention discloses a round steel hot rolling process for preventing mixed crystal of refined grains of steel for hub bearings, and relates to the technical field of steel production. The preheating section is less than or equal to 800 DEG C, the first heating section is less than or equal to 950 DEG C, the second heating section is 1030 +/-20 DEG C, the first soaking section is 1030 +/-20 DEG C, and the second soaking section is 1030 +/-20 DEG C; through on-line rolling and 7 water tank water cooling, the final rolling in a rolling mill is controlled to be 790-810 DEG C, and the target rolling is 800 DEG C; and slowly cooling to 750-770 DEG C in a heat insulation cover on a cooling bed at the target temperature of 760 DEG C, and then air cooling. Large pearlite group structures and core martensite are eliminated through grain refining and mixed crystal preventing processes, the impact toughness of the material can be greatly improved, the service life of the material is prolonged, the safety of the mater |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115672974A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115672974A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115672974A3</originalsourceid><addsrcrecordid>eNqNjLsOgkAQRWksjPoP4wdQ4ItYGqKhsrInC9zFTdYdMrMY_XvB-AFW9-Tk5M6TuuSYCnuPloSH0JJGwFMv3ECVLMvIeCJEFzp6uNcYNvLWaDyxJYF1YVSdGBd0MvehphpGpvz7tUxm1njF6reLZH0534oyRc8VtDcNAmJVXLNsf8g3x3x32v7TfABbPD4c</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Hot-rolled round steel process for preventing mixed crystal of refined grains of hub bearing steel</title><source>esp@cenet</source><creator>QIU JUNHUA ; WANG RUIZHANG ; ZHAO HAIYANG ; XU WEI</creator><creatorcontrib>QIU JUNHUA ; WANG RUIZHANG ; ZHAO HAIYANG ; XU WEI</creatorcontrib><description>The invention discloses a round steel hot rolling process for preventing mixed crystal of refined grains of steel for hub bearings, and relates to the technical field of steel production. The preheating section is less than or equal to 800 DEG C, the first heating section is less than or equal to 950 DEG C, the second heating section is 1030 +/-20 DEG C, the first soaking section is 1030 +/-20 DEG C, and the second soaking section is 1030 +/-20 DEG C; through on-line rolling and 7 water tank water cooling, the final rolling in a rolling mill is controlled to be 790-810 DEG C, and the target rolling is 800 DEG C; and slowly cooling to 750-770 DEG C in a heat insulation cover on a cooling bed at the target temperature of 760 DEG C, and then air cooling. Large pearlite group structures and core martensite are eliminated through grain refining and mixed crystal preventing processes, the impact toughness of the material can be greatly improved, the service life of the material is prolonged, the safety of the mater</description><language>chi ; eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METALLURGY ; PERFORMING OPERATIONS ; PUNCHING METAL ; ROLLING OF METAL ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230203&DB=EPODOC&CC=CN&NR=115672974A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230203&DB=EPODOC&CC=CN&NR=115672974A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>QIU JUNHUA</creatorcontrib><creatorcontrib>WANG RUIZHANG</creatorcontrib><creatorcontrib>ZHAO HAIYANG</creatorcontrib><creatorcontrib>XU WEI</creatorcontrib><title>Hot-rolled round steel process for preventing mixed crystal of refined grains of hub bearing steel</title><description>The invention discloses a round steel hot rolling process for preventing mixed crystal of refined grains of steel for hub bearings, and relates to the technical field of steel production. The preheating section is less than or equal to 800 DEG C, the first heating section is less than or equal to 950 DEG C, the second heating section is 1030 +/-20 DEG C, the first soaking section is 1030 +/-20 DEG C, and the second soaking section is 1030 +/-20 DEG C; through on-line rolling and 7 water tank water cooling, the final rolling in a rolling mill is controlled to be 790-810 DEG C, and the target rolling is 800 DEG C; and slowly cooling to 750-770 DEG C in a heat insulation cover on a cooling bed at the target temperature of 760 DEG C, and then air cooling. Large pearlite group structures and core martensite are eliminated through grain refining and mixed crystal preventing processes, the impact toughness of the material can be greatly improved, the service life of the material is prolonged, the safety of the mater</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>ROLLING OF METAL</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjLsOgkAQRWksjPoP4wdQ4ItYGqKhsrInC9zFTdYdMrMY_XvB-AFW9-Tk5M6TuuSYCnuPloSH0JJGwFMv3ECVLMvIeCJEFzp6uNcYNvLWaDyxJYF1YVSdGBd0MvehphpGpvz7tUxm1njF6reLZH0534oyRc8VtDcNAmJVXLNsf8g3x3x32v7TfABbPD4c</recordid><startdate>20230203</startdate><enddate>20230203</enddate><creator>QIU JUNHUA</creator><creator>WANG RUIZHANG</creator><creator>ZHAO HAIYANG</creator><creator>XU WEI</creator><scope>EVB</scope></search><sort><creationdate>20230203</creationdate><title>Hot-rolled round steel process for preventing mixed crystal of refined grains of hub bearing steel</title><author>QIU JUNHUA ; WANG RUIZHANG ; ZHAO HAIYANG ; XU WEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115672974A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>ROLLING OF METAL</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>QIU JUNHUA</creatorcontrib><creatorcontrib>WANG RUIZHANG</creatorcontrib><creatorcontrib>ZHAO HAIYANG</creatorcontrib><creatorcontrib>XU WEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>QIU JUNHUA</au><au>WANG RUIZHANG</au><au>ZHAO HAIYANG</au><au>XU WEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Hot-rolled round steel process for preventing mixed crystal of refined grains of hub bearing steel</title><date>2023-02-03</date><risdate>2023</risdate><abstract>The invention discloses a round steel hot rolling process for preventing mixed crystal of refined grains of steel for hub bearings, and relates to the technical field of steel production. The preheating section is less than or equal to 800 DEG C, the first heating section is less than or equal to 950 DEG C, the second heating section is 1030 +/-20 DEG C, the first soaking section is 1030 +/-20 DEG C, and the second soaking section is 1030 +/-20 DEG C; through on-line rolling and 7 water tank water cooling, the final rolling in a rolling mill is controlled to be 790-810 DEG C, and the target rolling is 800 DEG C; and slowly cooling to 750-770 DEG C in a heat insulation cover on a cooling bed at the target temperature of 760 DEG C, and then air cooling. Large pearlite group structures and core martensite are eliminated through grain refining and mixed crystal preventing processes, the impact toughness of the material can be greatly improved, the service life of the material is prolonged, the safety of the mater</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN115672974A |
source | esp@cenet |
subjects | ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL METALLURGY PERFORMING OPERATIONS PUNCHING METAL ROLLING OF METAL TRANSPORTING TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Hot-rolled round steel process for preventing mixed crystal of refined grains of hub bearing steel |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-30T17%3A41%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=QIU%20JUNHUA&rft.date=2023-02-03&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115672974A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |