Leaching method of high-silicon-zinc roasted ore

The invention relates to a leaching method of high-silicon zinc roasted ore, and belongs to the technical field of zinc roasted ore leaching. The method comprises the three leaching steps of neutral leaching, weak acid leaching and sub-hot acid leaching, dissolution of acid-soluble silicon dioxide i...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHANG MEI, JIN JIAQIANG, LUO HENG, CHEN CHUNLIN, DONG TIEGUANG, XU CHENGDONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHANG MEI
JIN JIAQIANG
LUO HENG
CHEN CHUNLIN
DONG TIEGUANG
XU CHENGDONG
description The invention relates to a leaching method of high-silicon zinc roasted ore, and belongs to the technical field of zinc roasted ore leaching. The method comprises the three leaching steps of neutral leaching, weak acid leaching and sub-hot acid leaching, dissolution of acid-soluble silicon dioxide in the zinc roasted ore and precipitation of silicon protein are synchronously carried out by controlling the acidity of ore pulp in the neutral leaching process, and therefore silicic acid is prevented from forming the maximum concentration in the neutral leaching process; and large-size difficult-to-settle slag cannot be formed at the last stage of intermediate leaching, ore pulp easy to settle is produced, the supernatant rate of the leached ore pulp is increased, the influence of silicon on the leaching process of the zinc roasted ore is greatly reduced, and smooth production is guaranteed. 本发明涉及一种高硅锌焙烧矿的浸出方法,属于锌焙烧矿浸出技术领域;本发明包括中性浸出、弱酸浸出和亚热酸浸出三个浸出步骤,通过控制中性浸出过程中矿浆的酸度使锌焙烧矿中的酸可溶二氧化硅溶出和硅蛋白的沉淀析出同步进行,从而阻止硅酸在中浸过程中形成最大浓度
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115612860A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115612860A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115612860A3</originalsourceid><addsrcrecordid>eNrjZDDwSU1MzsjMS1fITS3JyE9RyE9TyMhMz9AtzszJTM7P063KzEtWKMpPLC5JBUoWpfIwsKYl5hSn8kJpbgZFN9cQZw_d1IL8-NTigsTk1LzUknhnP0NDUzNDIwszA0djYtQAAD1LKvs</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Leaching method of high-silicon-zinc roasted ore</title><source>esp@cenet</source><creator>ZHANG MEI ; JIN JIAQIANG ; LUO HENG ; CHEN CHUNLIN ; DONG TIEGUANG ; XU CHENGDONG</creator><creatorcontrib>ZHANG MEI ; JIN JIAQIANG ; LUO HENG ; CHEN CHUNLIN ; DONG TIEGUANG ; XU CHENGDONG</creatorcontrib><description>The invention relates to a leaching method of high-silicon zinc roasted ore, and belongs to the technical field of zinc roasted ore leaching. The method comprises the three leaching steps of neutral leaching, weak acid leaching and sub-hot acid leaching, dissolution of acid-soluble silicon dioxide in the zinc roasted ore and precipitation of silicon protein are synchronously carried out by controlling the acidity of ore pulp in the neutral leaching process, and therefore silicic acid is prevented from forming the maximum concentration in the neutral leaching process; and large-size difficult-to-settle slag cannot be formed at the last stage of intermediate leaching, ore pulp easy to settle is produced, the supernatant rate of the leached ore pulp is increased, the influence of silicon on the leaching process of the zinc roasted ore is greatly reduced, and smooth production is guaranteed. 本发明涉及一种高硅锌焙烧矿的浸出方法,属于锌焙烧矿浸出技术领域;本发明包括中性浸出、弱酸浸出和亚热酸浸出三个浸出步骤,通过控制中性浸出过程中矿浆的酸度使锌焙烧矿中的酸可溶二氧化硅溶出和硅蛋白的沉淀析出同步进行,从而阻止硅酸在中浸过程中形成最大浓度</description><language>chi ; eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230117&amp;DB=EPODOC&amp;CC=CN&amp;NR=115612860A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230117&amp;DB=EPODOC&amp;CC=CN&amp;NR=115612860A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHANG MEI</creatorcontrib><creatorcontrib>JIN JIAQIANG</creatorcontrib><creatorcontrib>LUO HENG</creatorcontrib><creatorcontrib>CHEN CHUNLIN</creatorcontrib><creatorcontrib>DONG TIEGUANG</creatorcontrib><creatorcontrib>XU CHENGDONG</creatorcontrib><title>Leaching method of high-silicon-zinc roasted ore</title><description>The invention relates to a leaching method of high-silicon zinc roasted ore, and belongs to the technical field of zinc roasted ore leaching. The method comprises the three leaching steps of neutral leaching, weak acid leaching and sub-hot acid leaching, dissolution of acid-soluble silicon dioxide in the zinc roasted ore and precipitation of silicon protein are synchronously carried out by controlling the acidity of ore pulp in the neutral leaching process, and therefore silicic acid is prevented from forming the maximum concentration in the neutral leaching process; and large-size difficult-to-settle slag cannot be formed at the last stage of intermediate leaching, ore pulp easy to settle is produced, the supernatant rate of the leached ore pulp is increased, the influence of silicon on the leaching process of the zinc roasted ore is greatly reduced, and smooth production is guaranteed. 本发明涉及一种高硅锌焙烧矿的浸出方法,属于锌焙烧矿浸出技术领域;本发明包括中性浸出、弱酸浸出和亚热酸浸出三个浸出步骤,通过控制中性浸出过程中矿浆的酸度使锌焙烧矿中的酸可溶二氧化硅溶出和硅蛋白的沉淀析出同步进行,从而阻止硅酸在中浸过程中形成最大浓度</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDDwSU1MzsjMS1fITS3JyE9RyE9TyMhMz9AtzszJTM7P063KzEtWKMpPLC5JBUoWpfIwsKYl5hSn8kJpbgZFN9cQZw_d1IL8-NTigsTk1LzUknhnP0NDUzNDIwszA0djYtQAAD1LKvs</recordid><startdate>20230117</startdate><enddate>20230117</enddate><creator>ZHANG MEI</creator><creator>JIN JIAQIANG</creator><creator>LUO HENG</creator><creator>CHEN CHUNLIN</creator><creator>DONG TIEGUANG</creator><creator>XU CHENGDONG</creator><scope>EVB</scope></search><sort><creationdate>20230117</creationdate><title>Leaching method of high-silicon-zinc roasted ore</title><author>ZHANG MEI ; JIN JIAQIANG ; LUO HENG ; CHEN CHUNLIN ; DONG TIEGUANG ; XU CHENGDONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115612860A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHANG MEI</creatorcontrib><creatorcontrib>JIN JIAQIANG</creatorcontrib><creatorcontrib>LUO HENG</creatorcontrib><creatorcontrib>CHEN CHUNLIN</creatorcontrib><creatorcontrib>DONG TIEGUANG</creatorcontrib><creatorcontrib>XU CHENGDONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHANG MEI</au><au>JIN JIAQIANG</au><au>LUO HENG</au><au>CHEN CHUNLIN</au><au>DONG TIEGUANG</au><au>XU CHENGDONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Leaching method of high-silicon-zinc roasted ore</title><date>2023-01-17</date><risdate>2023</risdate><abstract>The invention relates to a leaching method of high-silicon zinc roasted ore, and belongs to the technical field of zinc roasted ore leaching. The method comprises the three leaching steps of neutral leaching, weak acid leaching and sub-hot acid leaching, dissolution of acid-soluble silicon dioxide in the zinc roasted ore and precipitation of silicon protein are synchronously carried out by controlling the acidity of ore pulp in the neutral leaching process, and therefore silicic acid is prevented from forming the maximum concentration in the neutral leaching process; and large-size difficult-to-settle slag cannot be formed at the last stage of intermediate leaching, ore pulp easy to settle is produced, the supernatant rate of the leached ore pulp is increased, the influence of silicon on the leaching process of the zinc roasted ore is greatly reduced, and smooth production is guaranteed. 本发明涉及一种高硅锌焙烧矿的浸出方法,属于锌焙烧矿浸出技术领域;本发明包括中性浸出、弱酸浸出和亚热酸浸出三个浸出步骤,通过控制中性浸出过程中矿浆的酸度使锌焙烧矿中的酸可溶二氧化硅溶出和硅蛋白的沉淀析出同步进行,从而阻止硅酸在中浸过程中形成最大浓度</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN115612860A
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Leaching method of high-silicon-zinc roasted ore
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-12T20%3A14%3A21IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHANG%20MEI&rft.date=2023-01-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115612860A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true