Preparation method of three-dimensional fluorinated carbon fiber flexible electrode

The invention discloses a preparation method of a three-dimensional fluorinated carbon fiber flexible electrode in the technical field of battery electrode preparation, and the preparation method comprises the following steps: 1, adding a metal salt into absolute ethyl alcohol, and stirring for 30 m...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG CHANG, LI XINLU, TENG JIUKANG, WEI JUNHUA, SHI BIN, CHEN XIAOTAO, YUAN DONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG CHANG
LI XINLU
TENG JIUKANG
WEI JUNHUA
SHI BIN
CHEN XIAOTAO
YUAN DONG
description The invention discloses a preparation method of a three-dimensional fluorinated carbon fiber flexible electrode in the technical field of battery electrode preparation, and the preparation method comprises the following steps: 1, adding a metal salt into absolute ethyl alcohol, and stirring for 30 minutes to obtain an ethanol solution in which metal ions are dissolved; 2, soaking carbon fiber cloth in the prepared ethanol solution for 10 minutes, transferring the soaked carbon fiber cloth into a sealed plastic box filled with argon, and applying pulse voltage to obtain three-dimensional carbon fiber cloth on which carbon nanotubes grow on carbon fibers in a high-density manner; and 3, placing the three-dimensional carbon fiber prepared in the step 2 in a reaction container, introducing nitrogen into the reactor to enable the internal pressure to reach 0.3 MPa, maintaining the pressure for 12 hours, controlling the temperature of the reactor at 600 DEG C, continuously introducing reaction gas into the reactor
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115538147A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115538147A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115538147A3</originalsourceid><addsrcrecordid>eNqNyrEKwjAURuEsDqK-Q3yADqEWXaUoTiLoXm6SPzSQJuEmgo9vBh_A6QzfWYvng5GJqfoU5YI6JyuTk3VmoLN-QSxNKEgX3ol9pAorDbFuu_Ma3AAfrwMkAkzlZLEVK0ehYPfrRuyvl9d465DThJLJIKJO412pYehP6nA89_88X6oxOQ8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of three-dimensional fluorinated carbon fiber flexible electrode</title><source>esp@cenet</source><creator>WANG CHANG ; LI XINLU ; TENG JIUKANG ; WEI JUNHUA ; SHI BIN ; CHEN XIAOTAO ; YUAN DONG</creator><creatorcontrib>WANG CHANG ; LI XINLU ; TENG JIUKANG ; WEI JUNHUA ; SHI BIN ; CHEN XIAOTAO ; YUAN DONG</creatorcontrib><description>The invention discloses a preparation method of a three-dimensional fluorinated carbon fiber flexible electrode in the technical field of battery electrode preparation, and the preparation method comprises the following steps: 1, adding a metal salt into absolute ethyl alcohol, and stirring for 30 minutes to obtain an ethanol solution in which metal ions are dissolved; 2, soaking carbon fiber cloth in the prepared ethanol solution for 10 minutes, transferring the soaked carbon fiber cloth into a sealed plastic box filled with argon, and applying pulse voltage to obtain three-dimensional carbon fiber cloth on which carbon nanotubes grow on carbon fibers in a high-density manner; and 3, placing the three-dimensional carbon fiber prepared in the step 2 in a reaction container, introducing nitrogen into the reactor to enable the internal pressure to reach 0.3 MPa, maintaining the pressure for 12 hours, controlling the temperature of the reactor at 600 DEG C, continuously introducing reaction gas into the reactor</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR ; LAUNDERING ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY ; TEXTILES ; TREATMENT OF TEXTILES OR THE LIKE ; TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20221230&amp;DB=EPODOC&amp;CC=CN&amp;NR=115538147A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20221230&amp;DB=EPODOC&amp;CC=CN&amp;NR=115538147A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG CHANG</creatorcontrib><creatorcontrib>LI XINLU</creatorcontrib><creatorcontrib>TENG JIUKANG</creatorcontrib><creatorcontrib>WEI JUNHUA</creatorcontrib><creatorcontrib>SHI BIN</creatorcontrib><creatorcontrib>CHEN XIAOTAO</creatorcontrib><creatorcontrib>YUAN DONG</creatorcontrib><title>Preparation method of three-dimensional fluorinated carbon fiber flexible electrode</title><description>The invention discloses a preparation method of a three-dimensional fluorinated carbon fiber flexible electrode in the technical field of battery electrode preparation, and the preparation method comprises the following steps: 1, adding a metal salt into absolute ethyl alcohol, and stirring for 30 minutes to obtain an ethanol solution in which metal ions are dissolved; 2, soaking carbon fiber cloth in the prepared ethanol solution for 10 minutes, transferring the soaked carbon fiber cloth into a sealed plastic box filled with argon, and applying pulse voltage to obtain three-dimensional carbon fiber cloth on which carbon nanotubes grow on carbon fibers in a high-density manner; and 3, placing the three-dimensional carbon fiber prepared in the step 2 in a reaction container, introducing nitrogen into the reactor to enable the internal pressure to reach 0.3 MPa, maintaining the pressure for 12 hours, controlling the temperature of the reactor at 600 DEG C, continuously introducing reaction gas into the reactor</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</subject><subject>LAUNDERING</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><subject>TEXTILES</subject><subject>TREATMENT OF TEXTILES OR THE LIKE</subject><subject>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEKwjAURuEsDqK-Q3yADqEWXaUoTiLoXm6SPzSQJuEmgo9vBh_A6QzfWYvng5GJqfoU5YI6JyuTk3VmoLN-QSxNKEgX3ol9pAorDbFuu_Ma3AAfrwMkAkzlZLEVK0ehYPfrRuyvl9d465DThJLJIKJO412pYehP6nA89_88X6oxOQ8</recordid><startdate>20221230</startdate><enddate>20221230</enddate><creator>WANG CHANG</creator><creator>LI XINLU</creator><creator>TENG JIUKANG</creator><creator>WEI JUNHUA</creator><creator>SHI BIN</creator><creator>CHEN XIAOTAO</creator><creator>YUAN DONG</creator><scope>EVB</scope></search><sort><creationdate>20221230</creationdate><title>Preparation method of three-dimensional fluorinated carbon fiber flexible electrode</title><author>WANG CHANG ; LI XINLU ; TENG JIUKANG ; WEI JUNHUA ; SHI BIN ; CHEN XIAOTAO ; YUAN DONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115538147A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</topic><topic>LAUNDERING</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><topic>TEXTILES</topic><topic>TREATMENT OF TEXTILES OR THE LIKE</topic><topic>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG CHANG</creatorcontrib><creatorcontrib>LI XINLU</creatorcontrib><creatorcontrib>TENG JIUKANG</creatorcontrib><creatorcontrib>WEI JUNHUA</creatorcontrib><creatorcontrib>SHI BIN</creatorcontrib><creatorcontrib>CHEN XIAOTAO</creatorcontrib><creatorcontrib>YUAN DONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG CHANG</au><au>LI XINLU</au><au>TENG JIUKANG</au><au>WEI JUNHUA</au><au>SHI BIN</au><au>CHEN XIAOTAO</au><au>YUAN DONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of three-dimensional fluorinated carbon fiber flexible electrode</title><date>2022-12-30</date><risdate>2022</risdate><abstract>The invention discloses a preparation method of a three-dimensional fluorinated carbon fiber flexible electrode in the technical field of battery electrode preparation, and the preparation method comprises the following steps: 1, adding a metal salt into absolute ethyl alcohol, and stirring for 30 minutes to obtain an ethanol solution in which metal ions are dissolved; 2, soaking carbon fiber cloth in the prepared ethanol solution for 10 minutes, transferring the soaked carbon fiber cloth into a sealed plastic box filled with argon, and applying pulse voltage to obtain three-dimensional carbon fiber cloth on which carbon nanotubes grow on carbon fibers in a high-density manner; and 3, placing the three-dimensional carbon fiber prepared in the step 2 in a reaction container, introducing nitrogen into the reactor to enable the internal pressure to reach 0.3 MPa, maintaining the pressure for 12 hours, controlling the temperature of the reactor at 600 DEG C, continuously introducing reaction gas into the reactor</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN115538147A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRICITY
FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR
LAUNDERING
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
TEXTILES
TREATMENT OF TEXTILES OR THE LIKE
TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS
title Preparation method of three-dimensional fluorinated carbon fiber flexible electrode
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T08%3A36%3A15IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20CHANG&rft.date=2022-12-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115538147A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true