Lead and silver leaching combined reagent for zinc leaching residues and application method
The invention relates to a zinc leaching residue lead and silver leaching combined reagent. The leaching combined reagent is composed of sodium chloride, 1-butyl-3-methylimidazolium hydrogen sulfate and sodium hypochlorite. Meanwhile, the invention further discloses an application method of the leac...
Gespeichert in:
Hauptverfasser: | , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | WANG ZHIFENG GUO HAINING CHEN DUJUAN WANG TINGXIA PENG GUIXIONG MIAO PEI LI GUODONG YANG JUNLONG |
description | The invention relates to a zinc leaching residue lead and silver leaching combined reagent. The leaching combined reagent is composed of sodium chloride, 1-butyl-3-methylimidazolium hydrogen sulfate and sodium hypochlorite. Meanwhile, the invention further discloses an application method of the leaching combined reagent, and the application method comprises the following steps: when the zinc leaching residues are leached, firstly adding 1-butyl-3-methylimidazolium hydrogen sulfate, and stirring to react for 5-10 minutes; adding sodium hypochlorite, and stirring to react for 20-30 minutes; and finally adding sodium chloride and stirring for reaction. The method does not need high-temperature high-acid pretreatment, and has the advantages of being high in lead and silver leaching rate, good in selectivity, high in process applicability and small in environmental influence.
本发明涉及一种锌浸出渣铅、银浸出组合药剂,该浸出组合药剂由氯化钠、1-丁基-3-甲基咪唑硫酸氢盐和次氯酸钠组成。同时,本发明还公开了该浸出组合药剂的应用方法,其在锌浸出渣浸出时,先添加1-丁基-3-甲基咪唑硫酸氢盐,搅拌反应5~10min;再添加次氯酸钠,搅拌反应20~30min |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115537560A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115537560A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115537560A3</originalsourceid><addsrcrecordid>eNqNy7EKwjAURuEuDqK-w_UBBEupzqUoDuLk5lCuyd_2QnoTkujg0wsiuDqd5Tvz4nYGW2K1lMQ9EcmBzSg6kPHTXRSWIniAZup9pJeo-ZGIJPaB9Pk5BCeGs3ilCXn0dlnMenYJq28Xxfp4uLanDYLvkAIbKHLXXsqyrqt9vds21T_mDUItO0Y</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Lead and silver leaching combined reagent for zinc leaching residues and application method</title><source>esp@cenet</source><creator>WANG ZHIFENG ; GUO HAINING ; CHEN DUJUAN ; WANG TINGXIA ; PENG GUIXIONG ; MIAO PEI ; LI GUODONG ; YANG JUNLONG</creator><creatorcontrib>WANG ZHIFENG ; GUO HAINING ; CHEN DUJUAN ; WANG TINGXIA ; PENG GUIXIONG ; MIAO PEI ; LI GUODONG ; YANG JUNLONG</creatorcontrib><description>The invention relates to a zinc leaching residue lead and silver leaching combined reagent. The leaching combined reagent is composed of sodium chloride, 1-butyl-3-methylimidazolium hydrogen sulfate and sodium hypochlorite. Meanwhile, the invention further discloses an application method of the leaching combined reagent, and the application method comprises the following steps: when the zinc leaching residues are leached, firstly adding 1-butyl-3-methylimidazolium hydrogen sulfate, and stirring to react for 5-10 minutes; adding sodium hypochlorite, and stirring to react for 20-30 minutes; and finally adding sodium chloride and stirring for reaction. The method does not need high-temperature high-acid pretreatment, and has the advantages of being high in lead and silver leaching rate, good in selectivity, high in process applicability and small in environmental influence.
本发明涉及一种锌浸出渣铅、银浸出组合药剂,该浸出组合药剂由氯化钠、1-丁基-3-甲基咪唑硫酸氢盐和次氯酸钠组成。同时,本发明还公开了该浸出组合药剂的应用方法,其在锌浸出渣浸出时,先添加1-丁基-3-甲基咪唑硫酸氢盐,搅拌反应5~10min;再添加次氯酸钠,搅拌反应20~30min</description><language>chi ; eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221230&DB=EPODOC&CC=CN&NR=115537560A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221230&DB=EPODOC&CC=CN&NR=115537560A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG ZHIFENG</creatorcontrib><creatorcontrib>GUO HAINING</creatorcontrib><creatorcontrib>CHEN DUJUAN</creatorcontrib><creatorcontrib>WANG TINGXIA</creatorcontrib><creatorcontrib>PENG GUIXIONG</creatorcontrib><creatorcontrib>MIAO PEI</creatorcontrib><creatorcontrib>LI GUODONG</creatorcontrib><creatorcontrib>YANG JUNLONG</creatorcontrib><title>Lead and silver leaching combined reagent for zinc leaching residues and application method</title><description>The invention relates to a zinc leaching residue lead and silver leaching combined reagent. The leaching combined reagent is composed of sodium chloride, 1-butyl-3-methylimidazolium hydrogen sulfate and sodium hypochlorite. Meanwhile, the invention further discloses an application method of the leaching combined reagent, and the application method comprises the following steps: when the zinc leaching residues are leached, firstly adding 1-butyl-3-methylimidazolium hydrogen sulfate, and stirring to react for 5-10 minutes; adding sodium hypochlorite, and stirring to react for 20-30 minutes; and finally adding sodium chloride and stirring for reaction. The method does not need high-temperature high-acid pretreatment, and has the advantages of being high in lead and silver leaching rate, good in selectivity, high in process applicability and small in environmental influence.
本发明涉及一种锌浸出渣铅、银浸出组合药剂,该浸出组合药剂由氯化钠、1-丁基-3-甲基咪唑硫酸氢盐和次氯酸钠组成。同时,本发明还公开了该浸出组合药剂的应用方法,其在锌浸出渣浸出时,先添加1-丁基-3-甲基咪唑硫酸氢盐,搅拌反应5~10min;再添加次氯酸钠,搅拌反应20~30min</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNy7EKwjAURuEuDqK-w_UBBEupzqUoDuLk5lCuyd_2QnoTkujg0wsiuDqd5Tvz4nYGW2K1lMQ9EcmBzSg6kPHTXRSWIniAZup9pJeo-ZGIJPaB9Pk5BCeGs3ilCXn0dlnMenYJq28Xxfp4uLanDYLvkAIbKHLXXsqyrqt9vds21T_mDUItO0Y</recordid><startdate>20221230</startdate><enddate>20221230</enddate><creator>WANG ZHIFENG</creator><creator>GUO HAINING</creator><creator>CHEN DUJUAN</creator><creator>WANG TINGXIA</creator><creator>PENG GUIXIONG</creator><creator>MIAO PEI</creator><creator>LI GUODONG</creator><creator>YANG JUNLONG</creator><scope>EVB</scope></search><sort><creationdate>20221230</creationdate><title>Lead and silver leaching combined reagent for zinc leaching residues and application method</title><author>WANG ZHIFENG ; GUO HAINING ; CHEN DUJUAN ; WANG TINGXIA ; PENG GUIXIONG ; MIAO PEI ; LI GUODONG ; YANG JUNLONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115537560A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG ZHIFENG</creatorcontrib><creatorcontrib>GUO HAINING</creatorcontrib><creatorcontrib>CHEN DUJUAN</creatorcontrib><creatorcontrib>WANG TINGXIA</creatorcontrib><creatorcontrib>PENG GUIXIONG</creatorcontrib><creatorcontrib>MIAO PEI</creatorcontrib><creatorcontrib>LI GUODONG</creatorcontrib><creatorcontrib>YANG JUNLONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG ZHIFENG</au><au>GUO HAINING</au><au>CHEN DUJUAN</au><au>WANG TINGXIA</au><au>PENG GUIXIONG</au><au>MIAO PEI</au><au>LI GUODONG</au><au>YANG JUNLONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Lead and silver leaching combined reagent for zinc leaching residues and application method</title><date>2022-12-30</date><risdate>2022</risdate><abstract>The invention relates to a zinc leaching residue lead and silver leaching combined reagent. The leaching combined reagent is composed of sodium chloride, 1-butyl-3-methylimidazolium hydrogen sulfate and sodium hypochlorite. Meanwhile, the invention further discloses an application method of the leaching combined reagent, and the application method comprises the following steps: when the zinc leaching residues are leached, firstly adding 1-butyl-3-methylimidazolium hydrogen sulfate, and stirring to react for 5-10 minutes; adding sodium hypochlorite, and stirring to react for 20-30 minutes; and finally adding sodium chloride and stirring for reaction. The method does not need high-temperature high-acid pretreatment, and has the advantages of being high in lead and silver leaching rate, good in selectivity, high in process applicability and small in environmental influence.
本发明涉及一种锌浸出渣铅、银浸出组合药剂,该浸出组合药剂由氯化钠、1-丁基-3-甲基咪唑硫酸氢盐和次氯酸钠组成。同时,本发明还公开了该浸出组合药剂的应用方法,其在锌浸出渣浸出时,先添加1-丁基-3-甲基咪唑硫酸氢盐,搅拌反应5~10min;再添加次氯酸钠,搅拌反应20~30min</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN115537560A |
source | esp@cenet |
subjects | CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY PRETREATMENT OF RAW MATERIALS PRODUCTION AND REFINING OF METALS TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Lead and silver leaching combined reagent for zinc leaching residues and application method |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-19T12%3A16%3A41IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20ZHIFENG&rft.date=2022-12-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115537560A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |