Welding process of nodular cast iron traction motor for rail transit
The invention discloses a welding process of a nodular cast iron traction motor for rail transit. The welding process comprises the following steps of: 1) cleaning stainless steel at a position where a junction box is welded on a traction enclosure by using alcohol before welding; (2) temperature co...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | CUI HOULU MA CHONGYIN LI LIANJIANG LIU CHENGJIN SHI GUOQING CHEN HONGQING |
description | The invention discloses a welding process of a nodular cast iron traction motor for rail transit. The welding process comprises the following steps of: 1) cleaning stainless steel at a position where a junction box is welded on a traction enclosure by using alcohol before welding; (2) temperature control is conducted on the welding room through an air conditioner and a heating device; (3) the ferronickel welding rod is put into a heating furnace to be preheated to 180 DEG C; measuring by using a contact type thermodetector; (4) flame preheating is conducted on the position, where the junction box is welded, of the traction machine shell to 180 Measuring by using a contact type thermodetector; (5) fixing the junction box on the traction machine shell by using screws and then welding, and after repeated experiments, welding by using a ferronickel welding rod OK92.58 imported from Issa; better matching performance with two kinds of base metal is achieved; the length of a rivet welding spot is 3 centimeters; acco |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115401428A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115401428A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115401428A3</originalsourceid><addsrcrecordid>eNrjZHAJT81JycxLVygoyk9OLS5WyE9TyMtPKc1JLFJITiwuUcgsys9TKClKTC7JBDJy80vyixTSgLgoMTMHJJ5XnFnCw8CalphTnMoLpbkZFN1cQ5w9dFML8uNTiwsSk1PzUkvinf0MDU1NDAxNjCwcjYlRAwC_hTLe</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Welding process of nodular cast iron traction motor for rail transit</title><source>esp@cenet</source><creator>CUI HOULU ; MA CHONGYIN ; LI LIANJIANG ; LIU CHENGJIN ; SHI GUOQING ; CHEN HONGQING</creator><creatorcontrib>CUI HOULU ; MA CHONGYIN ; LI LIANJIANG ; LIU CHENGJIN ; SHI GUOQING ; CHEN HONGQING</creatorcontrib><description>The invention discloses a welding process of a nodular cast iron traction motor for rail transit. The welding process comprises the following steps of: 1) cleaning stainless steel at a position where a junction box is welded on a traction enclosure by using alcohol before welding; (2) temperature control is conducted on the welding room through an air conditioner and a heating device; (3) the ferronickel welding rod is put into a heating furnace to be preheated to 180 DEG C; measuring by using a contact type thermodetector; (4) flame preheating is conducted on the position, where the junction box is welded, of the traction machine shell to 180 Measuring by using a contact type thermodetector; (5) fixing the junction box on the traction machine shell by using screws and then welding, and after repeated experiments, welding by using a ferronickel welding rod OK92.58 imported from Issa; better matching performance with two kinds of base metal is achieved; the length of a rivet welding spot is 3 centimeters; acco</description><language>chi ; eng</language><subject>COMBINED OPERATIONS ; CONVERSION OR DISTRIBUTION OF ELECTRIC POWER ; DYNAMO-ELECTRIC MACHINES ; ELECTRICITY ; GENERATION ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; OTHER WORKING OF METAL ; PERFORMING OPERATIONS ; TRANSPORTING ; UNIVERSAL MACHINE TOOLS</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221129&DB=EPODOC&CC=CN&NR=115401428A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221129&DB=EPODOC&CC=CN&NR=115401428A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CUI HOULU</creatorcontrib><creatorcontrib>MA CHONGYIN</creatorcontrib><creatorcontrib>LI LIANJIANG</creatorcontrib><creatorcontrib>LIU CHENGJIN</creatorcontrib><creatorcontrib>SHI GUOQING</creatorcontrib><creatorcontrib>CHEN HONGQING</creatorcontrib><title>Welding process of nodular cast iron traction motor for rail transit</title><description>The invention discloses a welding process of a nodular cast iron traction motor for rail transit. The welding process comprises the following steps of: 1) cleaning stainless steel at a position where a junction box is welded on a traction enclosure by using alcohol before welding; (2) temperature control is conducted on the welding room through an air conditioner and a heating device; (3) the ferronickel welding rod is put into a heating furnace to be preheated to 180 DEG C; measuring by using a contact type thermodetector; (4) flame preheating is conducted on the position, where the junction box is welded, of the traction machine shell to 180 Measuring by using a contact type thermodetector; (5) fixing the junction box on the traction machine shell by using screws and then welding, and after repeated experiments, welding by using a ferronickel welding rod OK92.58 imported from Issa; better matching performance with two kinds of base metal is achieved; the length of a rivet welding spot is 3 centimeters; acco</description><subject>COMBINED OPERATIONS</subject><subject>CONVERSION OR DISTRIBUTION OF ELECTRIC POWER</subject><subject>DYNAMO-ELECTRIC MACHINES</subject><subject>ELECTRICITY</subject><subject>GENERATION</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>OTHER WORKING OF METAL</subject><subject>PERFORMING OPERATIONS</subject><subject>TRANSPORTING</subject><subject>UNIVERSAL MACHINE TOOLS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHAJT81JycxLVygoyk9OLS5WyE9TyMtPKc1JLFJITiwuUcgsys9TKClKTC7JBDJy80vyixTSgLgoMTMHJJ5XnFnCw8CalphTnMoLpbkZFN1cQ5w9dFML8uNTiwsSk1PzUkvinf0MDU1NDAxNjCwcjYlRAwC_hTLe</recordid><startdate>20221129</startdate><enddate>20221129</enddate><creator>CUI HOULU</creator><creator>MA CHONGYIN</creator><creator>LI LIANJIANG</creator><creator>LIU CHENGJIN</creator><creator>SHI GUOQING</creator><creator>CHEN HONGQING</creator><scope>EVB</scope></search><sort><creationdate>20221129</creationdate><title>Welding process of nodular cast iron traction motor for rail transit</title><author>CUI HOULU ; MA CHONGYIN ; LI LIANJIANG ; LIU CHENGJIN ; SHI GUOQING ; CHEN HONGQING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115401428A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>COMBINED OPERATIONS</topic><topic>CONVERSION OR DISTRIBUTION OF ELECTRIC POWER</topic><topic>DYNAMO-ELECTRIC MACHINES</topic><topic>ELECTRICITY</topic><topic>GENERATION</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>OTHER WORKING OF METAL</topic><topic>PERFORMING OPERATIONS</topic><topic>TRANSPORTING</topic><topic>UNIVERSAL MACHINE TOOLS</topic><toplevel>online_resources</toplevel><creatorcontrib>CUI HOULU</creatorcontrib><creatorcontrib>MA CHONGYIN</creatorcontrib><creatorcontrib>LI LIANJIANG</creatorcontrib><creatorcontrib>LIU CHENGJIN</creatorcontrib><creatorcontrib>SHI GUOQING</creatorcontrib><creatorcontrib>CHEN HONGQING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CUI HOULU</au><au>MA CHONGYIN</au><au>LI LIANJIANG</au><au>LIU CHENGJIN</au><au>SHI GUOQING</au><au>CHEN HONGQING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Welding process of nodular cast iron traction motor for rail transit</title><date>2022-11-29</date><risdate>2022</risdate><abstract>The invention discloses a welding process of a nodular cast iron traction motor for rail transit. The welding process comprises the following steps of: 1) cleaning stainless steel at a position where a junction box is welded on a traction enclosure by using alcohol before welding; (2) temperature control is conducted on the welding room through an air conditioner and a heating device; (3) the ferronickel welding rod is put into a heating furnace to be preheated to 180 DEG C; measuring by using a contact type thermodetector; (4) flame preheating is conducted on the position, where the junction box is welded, of the traction machine shell to 180 Measuring by using a contact type thermodetector; (5) fixing the junction box on the traction machine shell by using screws and then welding, and after repeated experiments, welding by using a ferronickel welding rod OK92.58 imported from Issa; better matching performance with two kinds of base metal is achieved; the length of a rivet welding spot is 3 centimeters; acco</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN115401428A |
source | esp@cenet |
subjects | COMBINED OPERATIONS CONVERSION OR DISTRIBUTION OF ELECTRIC POWER DYNAMO-ELECTRIC MACHINES ELECTRICITY GENERATION MACHINE TOOLS METAL-WORKING NOT OTHERWISE PROVIDED FOR OTHER WORKING OF METAL PERFORMING OPERATIONS TRANSPORTING UNIVERSAL MACHINE TOOLS |
title | Welding process of nodular cast iron traction motor for rail transit |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T23%3A55%3A54IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CUI%20HOULU&rft.date=2022-11-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115401428A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |