Micron-sized 316L stainless steel formed by selective laser melting and preparation method of micron-sized 316L stainless steel
The invention discloses 316L stainless steel formed through micron-sized selective laser melting and a preparation method, and belongs to the technical field of intelligent manufacturing, the 316L stainless steel is manufactured through the micron-sized selective laser melting technology, the strate...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | ZHANG PING WANG MIAOHUI FAN BIN XIAO NING DU BAOPENG GE XUEYUAN LIU HAILONG |
description | The invention discloses 316L stainless steel formed through micron-sized selective laser melting and a preparation method, and belongs to the technical field of intelligent manufacturing, the 316L stainless steel is manufactured through the micron-sized selective laser melting technology, the strategy of strip scanning and rotating is adopted in the preparation process, the width of a strip ranges from 0 mm to 10 mm, and the layer-by-layer rotating angle ranges from 10 degrees to 90 degrees. The process conditions adopted by the micron-sized selective laser melting technology are as follows: the laser power is 10 to 100W, the laser spot diameter is 10 to 35 microns, and the laser scanning speed is 100 to 2000mm/s; the distance between laser spots is 10-100 microns; and the thickness of the powder spreading layer is 5-20 microns. The superfine metal powder and the ultra-small light spot diameter are adopted for micron-sized selective laser melting, micron-sized ultrahigh-precision 3D printing of different meta |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115383130A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115383130A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115383130A3</originalsourceid><addsrcrecordid>eNqNjLsKwkAURNNYiPoP1w8IuCyKrQTFQq3swzWZxIV9sXcRtPHX3cJeqxnOHGZavc-mS8HXYl7oSavNiSSz8RYipQGWhpBc2W5PElh02TxAlgWJHGw2fiT2PcWEyImzCb7wfA89hYHcr_d5NRnYChbfnFXLw_7aHGvE0EIid_DIbXNRaq23WunVTv_jfABPU0fj</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Micron-sized 316L stainless steel formed by selective laser melting and preparation method of micron-sized 316L stainless steel</title><source>esp@cenet</source><creator>ZHANG PING ; WANG MIAOHUI ; FAN BIN ; XIAO NING ; DU BAOPENG ; GE XUEYUAN ; LIU HAILONG</creator><creatorcontrib>ZHANG PING ; WANG MIAOHUI ; FAN BIN ; XIAO NING ; DU BAOPENG ; GE XUEYUAN ; LIU HAILONG</creatorcontrib><description>The invention discloses 316L stainless steel formed through micron-sized selective laser melting and a preparation method, and belongs to the technical field of intelligent manufacturing, the 316L stainless steel is manufactured through the micron-sized selective laser melting technology, the strategy of strip scanning and rotating is adopted in the preparation process, the width of a strip ranges from 0 mm to 10 mm, and the layer-by-layer rotating angle ranges from 10 degrees to 90 degrees. The process conditions adopted by the micron-sized selective laser melting technology are as follows: the laser power is 10 to 100W, the laser spot diameter is 10 to 35 microns, and the laser scanning speed is 100 to 2000mm/s; the distance between laser spots is 10-100 microns; and the thickness of the powder spreading layer is 5-20 microns. The superfine metal powder and the ultra-small light spot diameter are adopted for micron-sized selective laser melting, micron-sized ultrahigh-precision 3D printing of different meta</description><language>chi ; eng</language><subject>ADDITIVE MANUFACTURING TECHNOLOGY ; ADDITIVE MANUFACTURING, i.e. MANUFACTURING OFTHREE-DIMENSIONAL [3-D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVEAGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3-D PRINTING,STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING ; CASTING ; MAKING METALLIC POWDER ; MANUFACTURE OF ARTICLES FROM METALLIC POWDER ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING ; WORKING METALLIC POWDER</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221125&DB=EPODOC&CC=CN&NR=115383130A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221125&DB=EPODOC&CC=CN&NR=115383130A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHANG PING</creatorcontrib><creatorcontrib>WANG MIAOHUI</creatorcontrib><creatorcontrib>FAN BIN</creatorcontrib><creatorcontrib>XIAO NING</creatorcontrib><creatorcontrib>DU BAOPENG</creatorcontrib><creatorcontrib>GE XUEYUAN</creatorcontrib><creatorcontrib>LIU HAILONG</creatorcontrib><title>Micron-sized 316L stainless steel formed by selective laser melting and preparation method of micron-sized 316L stainless steel</title><description>The invention discloses 316L stainless steel formed through micron-sized selective laser melting and a preparation method, and belongs to the technical field of intelligent manufacturing, the 316L stainless steel is manufactured through the micron-sized selective laser melting technology, the strategy of strip scanning and rotating is adopted in the preparation process, the width of a strip ranges from 0 mm to 10 mm, and the layer-by-layer rotating angle ranges from 10 degrees to 90 degrees. The process conditions adopted by the micron-sized selective laser melting technology are as follows: the laser power is 10 to 100W, the laser spot diameter is 10 to 35 microns, and the laser scanning speed is 100 to 2000mm/s; the distance between laser spots is 10-100 microns; and the thickness of the powder spreading layer is 5-20 microns. The superfine metal powder and the ultra-small light spot diameter are adopted for micron-sized selective laser melting, micron-sized ultrahigh-precision 3D printing of different meta</description><subject>ADDITIVE MANUFACTURING TECHNOLOGY</subject><subject>ADDITIVE MANUFACTURING, i.e. MANUFACTURING OFTHREE-DIMENSIONAL [3-D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVEAGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3-D PRINTING,STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING</subject><subject>CASTING</subject><subject>MAKING METALLIC POWDER</subject><subject>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><subject>WORKING METALLIC POWDER</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjLsKwkAURNNYiPoP1w8IuCyKrQTFQq3swzWZxIV9sXcRtPHX3cJeqxnOHGZavc-mS8HXYl7oSavNiSSz8RYipQGWhpBc2W5PElh02TxAlgWJHGw2fiT2PcWEyImzCb7wfA89hYHcr_d5NRnYChbfnFXLw_7aHGvE0EIid_DIbXNRaq23WunVTv_jfABPU0fj</recordid><startdate>20221125</startdate><enddate>20221125</enddate><creator>ZHANG PING</creator><creator>WANG MIAOHUI</creator><creator>FAN BIN</creator><creator>XIAO NING</creator><creator>DU BAOPENG</creator><creator>GE XUEYUAN</creator><creator>LIU HAILONG</creator><scope>EVB</scope></search><sort><creationdate>20221125</creationdate><title>Micron-sized 316L stainless steel formed by selective laser melting and preparation method of micron-sized 316L stainless steel</title><author>ZHANG PING ; WANG MIAOHUI ; FAN BIN ; XIAO NING ; DU BAOPENG ; GE XUEYUAN ; LIU HAILONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115383130A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>ADDITIVE MANUFACTURING TECHNOLOGY</topic><topic>ADDITIVE MANUFACTURING, i.e. MANUFACTURING OFTHREE-DIMENSIONAL [3-D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVEAGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3-D PRINTING,STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING</topic><topic>CASTING</topic><topic>MAKING METALLIC POWDER</topic><topic>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><topic>WORKING METALLIC POWDER</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHANG PING</creatorcontrib><creatorcontrib>WANG MIAOHUI</creatorcontrib><creatorcontrib>FAN BIN</creatorcontrib><creatorcontrib>XIAO NING</creatorcontrib><creatorcontrib>DU BAOPENG</creatorcontrib><creatorcontrib>GE XUEYUAN</creatorcontrib><creatorcontrib>LIU HAILONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHANG PING</au><au>WANG MIAOHUI</au><au>FAN BIN</au><au>XIAO NING</au><au>DU BAOPENG</au><au>GE XUEYUAN</au><au>LIU HAILONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Micron-sized 316L stainless steel formed by selective laser melting and preparation method of micron-sized 316L stainless steel</title><date>2022-11-25</date><risdate>2022</risdate><abstract>The invention discloses 316L stainless steel formed through micron-sized selective laser melting and a preparation method, and belongs to the technical field of intelligent manufacturing, the 316L stainless steel is manufactured through the micron-sized selective laser melting technology, the strategy of strip scanning and rotating is adopted in the preparation process, the width of a strip ranges from 0 mm to 10 mm, and the layer-by-layer rotating angle ranges from 10 degrees to 90 degrees. The process conditions adopted by the micron-sized selective laser melting technology are as follows: the laser power is 10 to 100W, the laser spot diameter is 10 to 35 microns, and the laser scanning speed is 100 to 2000mm/s; the distance between laser spots is 10-100 microns; and the thickness of the powder spreading layer is 5-20 microns. The superfine metal powder and the ultra-small light spot diameter are adopted for micron-sized selective laser melting, micron-sized ultrahigh-precision 3D printing of different meta</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN115383130A |
source | esp@cenet |
subjects | ADDITIVE MANUFACTURING TECHNOLOGY ADDITIVE MANUFACTURING, i.e. MANUFACTURING OFTHREE-DIMENSIONAL [3-D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVEAGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3-D PRINTING,STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING CASTING MAKING METALLIC POWDER MANUFACTURE OF ARTICLES FROM METALLIC POWDER PERFORMING OPERATIONS POWDER METALLURGY TRANSPORTING WORKING METALLIC POWDER |
title | Micron-sized 316L stainless steel formed by selective laser melting and preparation method of micron-sized 316L stainless steel |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T20%3A06%3A27IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHANG%20PING&rft.date=2022-11-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115383130A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |