Micro-deformation stress relief annealing process for precise cold-drawn seamless tube

The invention discloses a micro-deformation stress relief annealing process for a precise cold-drawn seamless tube, which comprises the following steps: carrying out rough shaping on a cold-drawn seamless tube, carrying out annealing treatment on the seamless tube subjected to rough shaping, and car...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WEI JINYU, LIU XIANCUI, LIU YANG, WANG JIACONG, LIU QINGJIAO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WEI JINYU
LIU XIANCUI
LIU YANG
WANG JIACONG
LIU QINGJIAO
description The invention discloses a micro-deformation stress relief annealing process for a precise cold-drawn seamless tube, which comprises the following steps: carrying out rough shaping on a cold-drawn seamless tube, carrying out annealing treatment on the seamless tube subjected to rough shaping, and carrying out fine shaping and annealing treatment on the seamless tube subjected to annealing post-treatment: orderly placing the seamless tube in an annealing furnace, the suspension length of the two ends is smaller than or equal to 0.5 m, the annealing temperature ranges from 400 DEG C to 450 DEG C, the heat preservation time ranges from 2 h to 2.5 h, controlled cooling is conducted to 300 +/-10 DEG C, and discharging and air cooling are conducted; the method can improve the production efficiency, improve the product quality and reduce the energy consumption. 本发明公开一种精密冷拔无缝管微变形去应力退火工艺,包括如下步骤:对冷拔后的无缝管进行粗整形、对粗整形后的无缝管进行退火处理、对退火后处理后的无缝管进行精整形,退火处理:将无缝管整齐摆放在退火炉中,两端悬空长度长度≤0.5m,退火温度为400-450℃,保温时间2-2.5h,控冷至300±10℃,出炉空冷;使用该方法
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115354122A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115354122A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115354122A3</originalsourceid><addsrcrecordid>eNqNizEOAiEUBWksjHoHPAAFu-4BzEZjo5Wx3XzhYUhYIB-M15dNPIDVm2TmrcXj6g0nZeESz1R9irJURimSETycpBhBwceXzJzMIlrZGMYXSJOCVZbp026gOSy-vp_YipWjULD77Ubsz6f7eFHIaULJZBBRp_Gm9dAPB911x_6f5gtkfTn9</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Micro-deformation stress relief annealing process for precise cold-drawn seamless tube</title><source>esp@cenet</source><creator>WEI JINYU ; LIU XIANCUI ; LIU YANG ; WANG JIACONG ; LIU QINGJIAO</creator><creatorcontrib>WEI JINYU ; LIU XIANCUI ; LIU YANG ; WANG JIACONG ; LIU QINGJIAO</creatorcontrib><description>The invention discloses a micro-deformation stress relief annealing process for a precise cold-drawn seamless tube, which comprises the following steps: carrying out rough shaping on a cold-drawn seamless tube, carrying out annealing treatment on the seamless tube subjected to rough shaping, and carrying out fine shaping and annealing treatment on the seamless tube subjected to annealing post-treatment: orderly placing the seamless tube in an annealing furnace, the suspension length of the two ends is smaller than or equal to 0.5 m, the annealing temperature ranges from 400 DEG C to 450 DEG C, the heat preservation time ranges from 2 h to 2.5 h, controlled cooling is conducted to 300 +/-10 DEG C, and discharging and air cooling are conducted; the method can improve the production efficiency, improve the product quality and reduce the energy consumption. 本发明公开一种精密冷拔无缝管微变形去应力退火工艺,包括如下步骤:对冷拔后的无缝管进行粗整形、对粗整形后的无缝管进行退火处理、对退火后处理后的无缝管进行精整形,退火处理:将无缝管整齐摆放在退火炉中,两端悬空长度长度≤0.5m,退火温度为400-450℃,保温时间2-2.5h,控冷至300±10℃,出炉空冷;使用该方法</description><language>chi ; eng</language><subject>CHEMISTRY ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; PERFORMING OPERATIONS ; PUNCHING METAL ; TRANSPORTING ; WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20221118&amp;DB=EPODOC&amp;CC=CN&amp;NR=115354122A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20221118&amp;DB=EPODOC&amp;CC=CN&amp;NR=115354122A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WEI JINYU</creatorcontrib><creatorcontrib>LIU XIANCUI</creatorcontrib><creatorcontrib>LIU YANG</creatorcontrib><creatorcontrib>WANG JIACONG</creatorcontrib><creatorcontrib>LIU QINGJIAO</creatorcontrib><title>Micro-deformation stress relief annealing process for precise cold-drawn seamless tube</title><description>The invention discloses a micro-deformation stress relief annealing process for a precise cold-drawn seamless tube, which comprises the following steps: carrying out rough shaping on a cold-drawn seamless tube, carrying out annealing treatment on the seamless tube subjected to rough shaping, and carrying out fine shaping and annealing treatment on the seamless tube subjected to annealing post-treatment: orderly placing the seamless tube in an annealing furnace, the suspension length of the two ends is smaller than or equal to 0.5 m, the annealing temperature ranges from 400 DEG C to 450 DEG C, the heat preservation time ranges from 2 h to 2.5 h, controlled cooling is conducted to 300 +/-10 DEG C, and discharging and air cooling are conducted; the method can improve the production efficiency, improve the product quality and reduce the energy consumption. 本发明公开一种精密冷拔无缝管微变形去应力退火工艺,包括如下步骤:对冷拔后的无缝管进行粗整形、对粗整形后的无缝管进行退火处理、对退火后处理后的无缝管进行精整形,退火处理:将无缝管整齐摆放在退火炉中,两端悬空长度长度≤0.5m,退火温度为400-450℃,保温时间2-2.5h,控冷至300±10℃,出炉空冷;使用该方法</description><subject>CHEMISTRY</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>TRANSPORTING</subject><subject>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNizEOAiEUBWksjHoHPAAFu-4BzEZjo5Wx3XzhYUhYIB-M15dNPIDVm2TmrcXj6g0nZeESz1R9irJURimSETycpBhBwceXzJzMIlrZGMYXSJOCVZbp026gOSy-vp_YipWjULD77Ubsz6f7eFHIaULJZBBRp_Gm9dAPB911x_6f5gtkfTn9</recordid><startdate>20221118</startdate><enddate>20221118</enddate><creator>WEI JINYU</creator><creator>LIU XIANCUI</creator><creator>LIU YANG</creator><creator>WANG JIACONG</creator><creator>LIU QINGJIAO</creator><scope>EVB</scope></search><sort><creationdate>20221118</creationdate><title>Micro-deformation stress relief annealing process for precise cold-drawn seamless tube</title><author>WEI JINYU ; LIU XIANCUI ; LIU YANG ; WANG JIACONG ; LIU QINGJIAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115354122A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>CHEMISTRY</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>TRANSPORTING</topic><topic>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</topic><toplevel>online_resources</toplevel><creatorcontrib>WEI JINYU</creatorcontrib><creatorcontrib>LIU XIANCUI</creatorcontrib><creatorcontrib>LIU YANG</creatorcontrib><creatorcontrib>WANG JIACONG</creatorcontrib><creatorcontrib>LIU QINGJIAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WEI JINYU</au><au>LIU XIANCUI</au><au>LIU YANG</au><au>WANG JIACONG</au><au>LIU QINGJIAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Micro-deformation stress relief annealing process for precise cold-drawn seamless tube</title><date>2022-11-18</date><risdate>2022</risdate><abstract>The invention discloses a micro-deformation stress relief annealing process for a precise cold-drawn seamless tube, which comprises the following steps: carrying out rough shaping on a cold-drawn seamless tube, carrying out annealing treatment on the seamless tube subjected to rough shaping, and carrying out fine shaping and annealing treatment on the seamless tube subjected to annealing post-treatment: orderly placing the seamless tube in an annealing furnace, the suspension length of the two ends is smaller than or equal to 0.5 m, the annealing temperature ranges from 400 DEG C to 450 DEG C, the heat preservation time ranges from 2 h to 2.5 h, controlled cooling is conducted to 300 +/-10 DEG C, and discharging and air cooling are conducted; the method can improve the production efficiency, improve the product quality and reduce the energy consumption. 本发明公开一种精密冷拔无缝管微变形去应力退火工艺,包括如下步骤:对冷拔后的无缝管进行粗整形、对粗整形后的无缝管进行退火处理、对退火后处理后的无缝管进行精整形,退火处理:将无缝管整齐摆放在退火炉中,两端悬空长度长度≤0.5m,退火温度为400-450℃,保温时间2-2.5h,控冷至300±10℃,出炉空冷;使用该方法</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN115354122A
source esp@cenet
subjects CHEMISTRY
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
PERFORMING OPERATIONS
PUNCHING METAL
TRANSPORTING
WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL
title Micro-deformation stress relief annealing process for precise cold-drawn seamless tube
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-28T11%3A22%3A01IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WEI%20JINYU&rft.date=2022-11-18&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115354122A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true