Preparation method and application of surface iron oxide graphene co-loaded zero-valent iron particle material

The invention provides a preparation method and application of a surface iron oxide and graphene co-loaded zero-valent iron particle material, and belongs to the technical field of environmental restoration and material preparation. The preparation method of the material comprises the following step...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG HONGYAN, XU SHENGTAI, GONG MING, HAN LUCHAO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG HONGYAN
XU SHENGTAI
GONG MING
HAN LUCHAO
description The invention provides a preparation method and application of a surface iron oxide and graphene co-loaded zero-valent iron particle material, and belongs to the technical field of environmental restoration and material preparation. The preparation method of the material comprises the following steps: firstly preparing a zero-valent iron particle material with a clean surface, then preparing graphene oxide with a large number of oxygen-containing functional groups by using a chemical oxidation method, and finally co-loading iron oxide and graphene on the surface of zero-valent iron through a reduction reaction to obtain the surface iron oxide and graphene co-loaded zero-valent iron particle material. According to the reduction loading method, graphene and iron oxide are firmly combined on the surface of zero-valent iron through covalent interaction, the electrochemical activity and stability of the surface of the material are greatly improved, the iron oxide with high conductivity and magnetism can be specifi
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115340167A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115340167A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115340167A3</originalsourceid><addsrcrecordid>eNqNjTEKwkAURNNYiHqH7wEChqipJShWYmEfPrsTs7DZv_ysIp7eSDyAxTDM8JiZZ-GqiKycnATqkTqxxGFUjN6ZqZaWhoe2bEBOv_nlLOiuHDsEkJHcC1tYekMlf7JHSBM5LidnPKjnBHXsl9msZT9g9fNFtj4db_U5R5QGQxw_AlJTX4piV243xb46lP8wH-MRQs0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method and application of surface iron oxide graphene co-loaded zero-valent iron particle material</title><source>esp@cenet</source><creator>WANG HONGYAN ; XU SHENGTAI ; GONG MING ; HAN LUCHAO</creator><creatorcontrib>WANG HONGYAN ; XU SHENGTAI ; GONG MING ; HAN LUCHAO</creatorcontrib><description>The invention provides a preparation method and application of a surface iron oxide and graphene co-loaded zero-valent iron particle material, and belongs to the technical field of environmental restoration and material preparation. The preparation method of the material comprises the following steps: firstly preparing a zero-valent iron particle material with a clean surface, then preparing graphene oxide with a large number of oxygen-containing functional groups by using a chemical oxidation method, and finally co-loading iron oxide and graphene on the surface of zero-valent iron through a reduction reaction to obtain the surface iron oxide and graphene co-loaded zero-valent iron particle material. According to the reduction loading method, graphene and iron oxide are firmly combined on the surface of zero-valent iron through covalent interaction, the electrochemical activity and stability of the surface of the material are greatly improved, the iron oxide with high conductivity and magnetism can be specifi</description><language>chi ; eng</language><subject>CHEMISTRY ; METALLURGY ; TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20221115&amp;DB=EPODOC&amp;CC=CN&amp;NR=115340167A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20221115&amp;DB=EPODOC&amp;CC=CN&amp;NR=115340167A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG HONGYAN</creatorcontrib><creatorcontrib>XU SHENGTAI</creatorcontrib><creatorcontrib>GONG MING</creatorcontrib><creatorcontrib>HAN LUCHAO</creatorcontrib><title>Preparation method and application of surface iron oxide graphene co-loaded zero-valent iron particle material</title><description>The invention provides a preparation method and application of a surface iron oxide and graphene co-loaded zero-valent iron particle material, and belongs to the technical field of environmental restoration and material preparation. The preparation method of the material comprises the following steps: firstly preparing a zero-valent iron particle material with a clean surface, then preparing graphene oxide with a large number of oxygen-containing functional groups by using a chemical oxidation method, and finally co-loading iron oxide and graphene on the surface of zero-valent iron through a reduction reaction to obtain the surface iron oxide and graphene co-loaded zero-valent iron particle material. According to the reduction loading method, graphene and iron oxide are firmly combined on the surface of zero-valent iron through covalent interaction, the electrochemical activity and stability of the surface of the material are greatly improved, the iron oxide with high conductivity and magnetism can be specifi</description><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjTEKwkAURNNYiHqH7wEChqipJShWYmEfPrsTs7DZv_ysIp7eSDyAxTDM8JiZZ-GqiKycnATqkTqxxGFUjN6ZqZaWhoe2bEBOv_nlLOiuHDsEkJHcC1tYekMlf7JHSBM5LidnPKjnBHXsl9msZT9g9fNFtj4db_U5R5QGQxw_AlJTX4piV243xb46lP8wH-MRQs0</recordid><startdate>20221115</startdate><enddate>20221115</enddate><creator>WANG HONGYAN</creator><creator>XU SHENGTAI</creator><creator>GONG MING</creator><creator>HAN LUCHAO</creator><scope>EVB</scope></search><sort><creationdate>20221115</creationdate><title>Preparation method and application of surface iron oxide graphene co-loaded zero-valent iron particle material</title><author>WANG HONGYAN ; XU SHENGTAI ; GONG MING ; HAN LUCHAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115340167A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG HONGYAN</creatorcontrib><creatorcontrib>XU SHENGTAI</creatorcontrib><creatorcontrib>GONG MING</creatorcontrib><creatorcontrib>HAN LUCHAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG HONGYAN</au><au>XU SHENGTAI</au><au>GONG MING</au><au>HAN LUCHAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method and application of surface iron oxide graphene co-loaded zero-valent iron particle material</title><date>2022-11-15</date><risdate>2022</risdate><abstract>The invention provides a preparation method and application of a surface iron oxide and graphene co-loaded zero-valent iron particle material, and belongs to the technical field of environmental restoration and material preparation. The preparation method of the material comprises the following steps: firstly preparing a zero-valent iron particle material with a clean surface, then preparing graphene oxide with a large number of oxygen-containing functional groups by using a chemical oxidation method, and finally co-loading iron oxide and graphene on the surface of zero-valent iron through a reduction reaction to obtain the surface iron oxide and graphene co-loaded zero-valent iron particle material. According to the reduction loading method, graphene and iron oxide are firmly combined on the surface of zero-valent iron through covalent interaction, the electrochemical activity and stability of the surface of the material are greatly improved, the iron oxide with high conductivity and magnetism can be specifi</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN115340167A
source esp@cenet
subjects CHEMISTRY
METALLURGY
TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE
title Preparation method and application of surface iron oxide graphene co-loaded zero-valent iron particle material
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-13T08%3A53%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20HONGYAN&rft.date=2022-11-15&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115340167A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true