Method for efficiently oxidizing molybdenite in sulfuric acid and ferric sulfate solution under normal pressure condition
The invention discloses a method for efficiently oxidizing molybdenite in a sulfuric acid and ferric sulfate solution under a normal pressure condition, which comprises the following steps of: adding trace iodide ions into a sulfuric acid-ferric sulfate mixed solution under the normal pressure condi...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | WANG JUN'E ZHANG JIAHAO WU ZHENGHUI WANG MEIJUN XIE HONGZHEN WANG QIANKUN FAN DAOYAN |
description | The invention discloses a method for efficiently oxidizing molybdenite in a sulfuric acid and ferric sulfate solution under a normal pressure condition, which comprises the following steps of: adding trace iodide ions into a sulfuric acid-ferric sulfate mixed solution under the normal pressure condition by utilizing the chemical catalysis characteristic of iodide ions/iodine elementary substances; according to the method, the problem that a passive film is compact in the conventional acid leaching process of molybdenite and other molybdenum-containing sulfide minerals can be solved, SO2 flue gas emission pollution is reduced, copper and molybdenum are synchronously separated, meanwhile, efficient oxidation of molybdenum concentrate under the wet process condition is achieved, and efficient enrichment of molybdenum in acid leaching residues is promoted. By the adoption of the preparation method, efficient oxidation and copper-molybdenum separation of the molybdenum concentrate can be achieved in the catalytic |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115305363A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115305363A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115305363A3</originalsourceid><addsrcrecordid>eNqNi0EKwjAQRbtxIeodxgMIllD3UhQ3unJfYjLRgXSmTBKwnt4WPICrz-O9v6zGK-aXeAiigCGQI-QcR5A3efoQP6GXOD48MmUEYkglhqLkwDryYHm6os48Czs1SWLJJAyFPSqwaG8jDIopFUVwwp5mv64WwcaEm9-uqu35dG8vOxykwzRYh4y5a2913Zh9Yw7maP5pvp2AR7w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for efficiently oxidizing molybdenite in sulfuric acid and ferric sulfate solution under normal pressure condition</title><source>esp@cenet</source><creator>WANG JUN'E ; ZHANG JIAHAO ; WU ZHENGHUI ; WANG MEIJUN ; XIE HONGZHEN ; WANG QIANKUN ; FAN DAOYAN</creator><creatorcontrib>WANG JUN'E ; ZHANG JIAHAO ; WU ZHENGHUI ; WANG MEIJUN ; XIE HONGZHEN ; WANG QIANKUN ; FAN DAOYAN</creatorcontrib><description>The invention discloses a method for efficiently oxidizing molybdenite in a sulfuric acid and ferric sulfate solution under a normal pressure condition, which comprises the following steps of: adding trace iodide ions into a sulfuric acid-ferric sulfate mixed solution under the normal pressure condition by utilizing the chemical catalysis characteristic of iodide ions/iodine elementary substances; according to the method, the problem that a passive film is compact in the conventional acid leaching process of molybdenite and other molybdenum-containing sulfide minerals can be solved, SO2 flue gas emission pollution is reduced, copper and molybdenum are synchronously separated, meanwhile, efficient oxidation of molybdenum concentrate under the wet process condition is achieved, and efficient enrichment of molybdenum in acid leaching residues is promoted. By the adoption of the preparation method, efficient oxidation and copper-molybdenum separation of the molybdenum concentrate can be achieved in the catalytic</description><language>chi ; eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221108&DB=EPODOC&CC=CN&NR=115305363A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221108&DB=EPODOC&CC=CN&NR=115305363A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG JUN'E</creatorcontrib><creatorcontrib>ZHANG JIAHAO</creatorcontrib><creatorcontrib>WU ZHENGHUI</creatorcontrib><creatorcontrib>WANG MEIJUN</creatorcontrib><creatorcontrib>XIE HONGZHEN</creatorcontrib><creatorcontrib>WANG QIANKUN</creatorcontrib><creatorcontrib>FAN DAOYAN</creatorcontrib><title>Method for efficiently oxidizing molybdenite in sulfuric acid and ferric sulfate solution under normal pressure condition</title><description>The invention discloses a method for efficiently oxidizing molybdenite in a sulfuric acid and ferric sulfate solution under a normal pressure condition, which comprises the following steps of: adding trace iodide ions into a sulfuric acid-ferric sulfate mixed solution under the normal pressure condition by utilizing the chemical catalysis characteristic of iodide ions/iodine elementary substances; according to the method, the problem that a passive film is compact in the conventional acid leaching process of molybdenite and other molybdenum-containing sulfide minerals can be solved, SO2 flue gas emission pollution is reduced, copper and molybdenum are synchronously separated, meanwhile, efficient oxidation of molybdenum concentrate under the wet process condition is achieved, and efficient enrichment of molybdenum in acid leaching residues is promoted. By the adoption of the preparation method, efficient oxidation and copper-molybdenum separation of the molybdenum concentrate can be achieved in the catalytic</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNi0EKwjAQRbtxIeodxgMIllD3UhQ3unJfYjLRgXSmTBKwnt4WPICrz-O9v6zGK-aXeAiigCGQI-QcR5A3efoQP6GXOD48MmUEYkglhqLkwDryYHm6os48Czs1SWLJJAyFPSqwaG8jDIopFUVwwp5mv64WwcaEm9-uqu35dG8vOxykwzRYh4y5a2913Zh9Yw7maP5pvp2AR7w</recordid><startdate>20221108</startdate><enddate>20221108</enddate><creator>WANG JUN'E</creator><creator>ZHANG JIAHAO</creator><creator>WU ZHENGHUI</creator><creator>WANG MEIJUN</creator><creator>XIE HONGZHEN</creator><creator>WANG QIANKUN</creator><creator>FAN DAOYAN</creator><scope>EVB</scope></search><sort><creationdate>20221108</creationdate><title>Method for efficiently oxidizing molybdenite in sulfuric acid and ferric sulfate solution under normal pressure condition</title><author>WANG JUN'E ; ZHANG JIAHAO ; WU ZHENGHUI ; WANG MEIJUN ; XIE HONGZHEN ; WANG QIANKUN ; FAN DAOYAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115305363A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG JUN'E</creatorcontrib><creatorcontrib>ZHANG JIAHAO</creatorcontrib><creatorcontrib>WU ZHENGHUI</creatorcontrib><creatorcontrib>WANG MEIJUN</creatorcontrib><creatorcontrib>XIE HONGZHEN</creatorcontrib><creatorcontrib>WANG QIANKUN</creatorcontrib><creatorcontrib>FAN DAOYAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG JUN'E</au><au>ZHANG JIAHAO</au><au>WU ZHENGHUI</au><au>WANG MEIJUN</au><au>XIE HONGZHEN</au><au>WANG QIANKUN</au><au>FAN DAOYAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for efficiently oxidizing molybdenite in sulfuric acid and ferric sulfate solution under normal pressure condition</title><date>2022-11-08</date><risdate>2022</risdate><abstract>The invention discloses a method for efficiently oxidizing molybdenite in a sulfuric acid and ferric sulfate solution under a normal pressure condition, which comprises the following steps of: adding trace iodide ions into a sulfuric acid-ferric sulfate mixed solution under the normal pressure condition by utilizing the chemical catalysis characteristic of iodide ions/iodine elementary substances; according to the method, the problem that a passive film is compact in the conventional acid leaching process of molybdenite and other molybdenum-containing sulfide minerals can be solved, SO2 flue gas emission pollution is reduced, copper and molybdenum are synchronously separated, meanwhile, efficient oxidation of molybdenum concentrate under the wet process condition is achieved, and efficient enrichment of molybdenum in acid leaching residues is promoted. By the adoption of the preparation method, efficient oxidation and copper-molybdenum separation of the molybdenum concentrate can be achieved in the catalytic</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN115305363A |
source | esp@cenet |
subjects | CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY PRETREATMENT OF RAW MATERIALS PRODUCTION AND REFINING OF METALS TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Method for efficiently oxidizing molybdenite in sulfuric acid and ferric sulfate solution under normal pressure condition |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-31T23%3A22%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20JUN'E&rft.date=2022-11-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115305363A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |