Preparation method of glass fiber reinforced plastic
The invention relates to a method for manufacturing glass fiber reinforced plastics by using an epoxy resin coupling agent based on carbon nanotube reinforcement. The preparation method comprises the following steps: mixing oxidized carbon nanotubes accounting for 0.1-2.5% of the mass of epoxy resin...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | WANG DONGXING DING ANG LI TIANJUN MARTYNOVICH, GOROSINSKI, SERGEY TIMOFEVICH, KATELL NIKOLAI SAMENTSOV, YURY IVANOVICH CHERNIUK OKSANA ANATOLYEVNA ZURAWSKI SERGEY VIKTOROVICH NIKOLAEVICH, MAHNO, STANISLAV ALEKSEVNA, IVANENKO EKATERINA WANG BO |
description | The invention relates to a method for manufacturing glass fiber reinforced plastics by using an epoxy resin coupling agent based on carbon nanotube reinforcement. The preparation method comprises the following steps: mixing oxidized carbon nanotubes accounting for 0.1-2.5% of the mass of epoxy resin with epoxy resin, homogenizing by using a three-roller grinder, ultrasonically dispersing unoxidized hydrophobic carbon nanotubes accounting for 0.3-1.5% of the mass of a curing agent in the curing agent, mixing modified epoxy resin with the modified curing agent, coating a glass fiber cloth with the mixture, and drying to obtain a finished product. The total content of the carbon nano tubes accounts for 0.15-2.2% of the mass of the solid resin, and then the glass fiber laminated body with the required layer number is formed and is subjected to pouring (vacuum) pressing, and the total content of the carbon nano tubes accounts for 0.15-2.2% of the mass of the solid resin. Compared with a traditional composite mater |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115302922A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115302922A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115302922A3</originalsourceid><addsrcrecordid>eNrjZDAJKEotSCxKLMnMz1PITS3JyE9RyE9TSM9JLC5WSMtMSi1SKErNzEvLL0pOTVEoAAqXZCbzMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DQ1NjAyNLIyNHY2LUAAA_CCzb</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of glass fiber reinforced plastic</title><source>esp@cenet</source><creator>WANG DONGXING ; DING ANG ; LI TIANJUN ; MARTYNOVICH, GOROSINSKI, SERGEY ; TIMOFEVICH, KATELL NIKOLAI ; SAMENTSOV, YURY IVANOVICH ; CHERNIUK OKSANA ANATOLYEVNA ; ZURAWSKI SERGEY VIKTOROVICH ; NIKOLAEVICH, MAHNO, STANISLAV ; ALEKSEVNA, IVANENKO EKATERINA ; WANG BO</creator><creatorcontrib>WANG DONGXING ; DING ANG ; LI TIANJUN ; MARTYNOVICH, GOROSINSKI, SERGEY ; TIMOFEVICH, KATELL NIKOLAI ; SAMENTSOV, YURY IVANOVICH ; CHERNIUK OKSANA ANATOLYEVNA ; ZURAWSKI SERGEY VIKTOROVICH ; NIKOLAEVICH, MAHNO, STANISLAV ; ALEKSEVNA, IVANENKO EKATERINA ; WANG BO</creatorcontrib><description>The invention relates to a method for manufacturing glass fiber reinforced plastics by using an epoxy resin coupling agent based on carbon nanotube reinforcement. The preparation method comprises the following steps: mixing oxidized carbon nanotubes accounting for 0.1-2.5% of the mass of epoxy resin with epoxy resin, homogenizing by using a three-roller grinder, ultrasonically dispersing unoxidized hydrophobic carbon nanotubes accounting for 0.3-1.5% of the mass of a curing agent in the curing agent, mixing modified epoxy resin with the modified curing agent, coating a glass fiber cloth with the mixture, and drying to obtain a finished product. The total content of the carbon nano tubes accounts for 0.15-2.2% of the mass of the solid resin, and then the glass fiber laminated body with the required layer number is formed and is subjected to pouring (vacuum) pressing, and the total content of the carbon nano tubes accounts for 0.15-2.2% of the mass of the solid resin. Compared with a traditional composite mater</description><language>chi ; eng</language><subject>LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; MAKING GRANULES OR PREFORMS ; PERFORMING OPERATIONS ; PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED ; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221108&DB=EPODOC&CC=CN&NR=115302922A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76419</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221108&DB=EPODOC&CC=CN&NR=115302922A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG DONGXING</creatorcontrib><creatorcontrib>DING ANG</creatorcontrib><creatorcontrib>LI TIANJUN</creatorcontrib><creatorcontrib>MARTYNOVICH, GOROSINSKI, SERGEY</creatorcontrib><creatorcontrib>TIMOFEVICH, KATELL NIKOLAI</creatorcontrib><creatorcontrib>SAMENTSOV, YURY IVANOVICH</creatorcontrib><creatorcontrib>CHERNIUK OKSANA ANATOLYEVNA</creatorcontrib><creatorcontrib>ZURAWSKI SERGEY VIKTOROVICH</creatorcontrib><creatorcontrib>NIKOLAEVICH, MAHNO, STANISLAV</creatorcontrib><creatorcontrib>ALEKSEVNA, IVANENKO EKATERINA</creatorcontrib><creatorcontrib>WANG BO</creatorcontrib><title>Preparation method of glass fiber reinforced plastic</title><description>The invention relates to a method for manufacturing glass fiber reinforced plastics by using an epoxy resin coupling agent based on carbon nanotube reinforcement. The preparation method comprises the following steps: mixing oxidized carbon nanotubes accounting for 0.1-2.5% of the mass of epoxy resin with epoxy resin, homogenizing by using a three-roller grinder, ultrasonically dispersing unoxidized hydrophobic carbon nanotubes accounting for 0.3-1.5% of the mass of a curing agent in the curing agent, mixing modified epoxy resin with the modified curing agent, coating a glass fiber cloth with the mixture, and drying to obtain a finished product. The total content of the carbon nano tubes accounts for 0.15-2.2% of the mass of the solid resin, and then the glass fiber laminated body with the required layer number is formed and is subjected to pouring (vacuum) pressing, and the total content of the carbon nano tubes accounts for 0.15-2.2% of the mass of the solid resin. Compared with a traditional composite mater</description><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>MAKING GRANULES OR PREFORMS</subject><subject>PERFORMING OPERATIONS</subject><subject>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</subject><subject>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAJKEotSCxKLMnMz1PITS3JyE9RyE9TSM9JLC5WSMtMSi1SKErNzEvLL0pOTVEoAAqXZCbzMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DQ1NjAyNLIyNHY2LUAAA_CCzb</recordid><startdate>20221108</startdate><enddate>20221108</enddate><creator>WANG DONGXING</creator><creator>DING ANG</creator><creator>LI TIANJUN</creator><creator>MARTYNOVICH, GOROSINSKI, SERGEY</creator><creator>TIMOFEVICH, KATELL NIKOLAI</creator><creator>SAMENTSOV, YURY IVANOVICH</creator><creator>CHERNIUK OKSANA ANATOLYEVNA</creator><creator>ZURAWSKI SERGEY VIKTOROVICH</creator><creator>NIKOLAEVICH, MAHNO, STANISLAV</creator><creator>ALEKSEVNA, IVANENKO EKATERINA</creator><creator>WANG BO</creator><scope>EVB</scope></search><sort><creationdate>20221108</creationdate><title>Preparation method of glass fiber reinforced plastic</title><author>WANG DONGXING ; DING ANG ; LI TIANJUN ; MARTYNOVICH, GOROSINSKI, SERGEY ; TIMOFEVICH, KATELL NIKOLAI ; SAMENTSOV, YURY IVANOVICH ; CHERNIUK OKSANA ANATOLYEVNA ; ZURAWSKI SERGEY VIKTOROVICH ; NIKOLAEVICH, MAHNO, STANISLAV ; ALEKSEVNA, IVANENKO EKATERINA ; WANG BO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115302922A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>MAKING GRANULES OR PREFORMS</topic><topic>PERFORMING OPERATIONS</topic><topic>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</topic><topic>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG DONGXING</creatorcontrib><creatorcontrib>DING ANG</creatorcontrib><creatorcontrib>LI TIANJUN</creatorcontrib><creatorcontrib>MARTYNOVICH, GOROSINSKI, SERGEY</creatorcontrib><creatorcontrib>TIMOFEVICH, KATELL NIKOLAI</creatorcontrib><creatorcontrib>SAMENTSOV, YURY IVANOVICH</creatorcontrib><creatorcontrib>CHERNIUK OKSANA ANATOLYEVNA</creatorcontrib><creatorcontrib>ZURAWSKI SERGEY VIKTOROVICH</creatorcontrib><creatorcontrib>NIKOLAEVICH, MAHNO, STANISLAV</creatorcontrib><creatorcontrib>ALEKSEVNA, IVANENKO EKATERINA</creatorcontrib><creatorcontrib>WANG BO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG DONGXING</au><au>DING ANG</au><au>LI TIANJUN</au><au>MARTYNOVICH, GOROSINSKI, SERGEY</au><au>TIMOFEVICH, KATELL NIKOLAI</au><au>SAMENTSOV, YURY IVANOVICH</au><au>CHERNIUK OKSANA ANATOLYEVNA</au><au>ZURAWSKI SERGEY VIKTOROVICH</au><au>NIKOLAEVICH, MAHNO, STANISLAV</au><au>ALEKSEVNA, IVANENKO EKATERINA</au><au>WANG BO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of glass fiber reinforced plastic</title><date>2022-11-08</date><risdate>2022</risdate><abstract>The invention relates to a method for manufacturing glass fiber reinforced plastics by using an epoxy resin coupling agent based on carbon nanotube reinforcement. The preparation method comprises the following steps: mixing oxidized carbon nanotubes accounting for 0.1-2.5% of the mass of epoxy resin with epoxy resin, homogenizing by using a three-roller grinder, ultrasonically dispersing unoxidized hydrophobic carbon nanotubes accounting for 0.3-1.5% of the mass of a curing agent in the curing agent, mixing modified epoxy resin with the modified curing agent, coating a glass fiber cloth with the mixture, and drying to obtain a finished product. The total content of the carbon nano tubes accounts for 0.15-2.2% of the mass of the solid resin, and then the glass fiber laminated body with the required layer number is formed and is subjected to pouring (vacuum) pressing, and the total content of the carbon nano tubes accounts for 0.15-2.2% of the mass of the solid resin. Compared with a traditional composite mater</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN115302922A |
source | esp@cenet |
subjects | LAYERED PRODUCTS LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM MAKING GRANULES OR PREFORMS PERFORMING OPERATIONS PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS TRANSPORTING WORKING OF PLASTICS WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL |
title | Preparation method of glass fiber reinforced plastic |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T16%3A35%3A01IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20DONGXING&rft.date=2022-11-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115302922A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |