Method for preparing carbon nano tube by hydrothermal method

A method for preparing a carbon nanotube by a hydrothermal method belongs to the technical field of nano material preparation, and comprises the following steps: placing graphene oxide (GO) powder in deionized water, and carrying out ultrasonic treatment to obtain a GO solution; dropwise adding dilu...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LI BING, SUN WEI, HAN CUNXIN, GAO JIAWANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LI BING
SUN WEI
HAN CUNXIN
GAO JIAWANG
description A method for preparing a carbon nanotube by a hydrothermal method belongs to the technical field of nano material preparation, and comprises the following steps: placing graphene oxide (GO) powder in deionized water, and carrying out ultrasonic treatment to obtain a GO solution; dropwise adding diluted hydrochloric acid into the GO solution to obtain an acidified GO solution; and putting the acidified GO solution into a reaction kettle, and reacting at the temperature of 200 DEG C for 2 hours to obtain the carbon nanotube. According to the method, the graphene oxide is used as a source, and the self-curling effect of the graphene oxide under the weakly acidic hydrothermal condition is utilized, so that a catalyst and strong acid do not need to be introduced, the preparation process is simple, and the application of the graphene oxide in the fields of catalyst carriers and energy storage is facilitated. 一种水热法制备碳纳米管的方法,属于纳米材料制备技术领域,其制备方法是将氧化石墨烯(GO)粉末置于去离子水中,经过超声,获得GO溶液;向GO溶液滴入稀盐酸,得到酸化的GO溶液;再将酸化GO溶液置于反应釜中,反应温度20
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN114988394A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN114988394A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN114988394A3</originalsourceid><addsrcrecordid>eNrjZLDxTS3JyE9RSMsvUigoSi1ILMrMS1dITixKys9TyEvMy1coKU1KVUiqVMioTCnKL8lILcpNzFHIBeviYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GhiaWFhbGliaOxsSoAQDodS_x</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing carbon nano tube by hydrothermal method</title><source>esp@cenet</source><creator>LI BING ; SUN WEI ; HAN CUNXIN ; GAO JIAWANG</creator><creatorcontrib>LI BING ; SUN WEI ; HAN CUNXIN ; GAO JIAWANG</creatorcontrib><description>A method for preparing a carbon nanotube by a hydrothermal method belongs to the technical field of nano material preparation, and comprises the following steps: placing graphene oxide (GO) powder in deionized water, and carrying out ultrasonic treatment to obtain a GO solution; dropwise adding diluted hydrochloric acid into the GO solution to obtain an acidified GO solution; and putting the acidified GO solution into a reaction kettle, and reacting at the temperature of 200 DEG C for 2 hours to obtain the carbon nanotube. According to the method, the graphene oxide is used as a source, and the self-curling effect of the graphene oxide under the weakly acidic hydrothermal condition is utilized, so that a catalyst and strong acid do not need to be introduced, the preparation process is simple, and the application of the graphene oxide in the fields of catalyst carriers and energy storage is facilitated. 一种水热法制备碳纳米管的方法,属于纳米材料制备技术领域,其制备方法是将氧化石墨烯(GO)粉末置于去离子水中,经过超声,获得GO溶液;向GO溶液滴入稀盐酸,得到酸化的GO溶液;再将酸化GO溶液置于反应釜中,反应温度20</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS THEREOF ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220902&amp;DB=EPODOC&amp;CC=CN&amp;NR=114988394A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25566,76549</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220902&amp;DB=EPODOC&amp;CC=CN&amp;NR=114988394A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LI BING</creatorcontrib><creatorcontrib>SUN WEI</creatorcontrib><creatorcontrib>HAN CUNXIN</creatorcontrib><creatorcontrib>GAO JIAWANG</creatorcontrib><title>Method for preparing carbon nano tube by hydrothermal method</title><description>A method for preparing a carbon nanotube by a hydrothermal method belongs to the technical field of nano material preparation, and comprises the following steps: placing graphene oxide (GO) powder in deionized water, and carrying out ultrasonic treatment to obtain a GO solution; dropwise adding diluted hydrochloric acid into the GO solution to obtain an acidified GO solution; and putting the acidified GO solution into a reaction kettle, and reacting at the temperature of 200 DEG C for 2 hours to obtain the carbon nanotube. According to the method, the graphene oxide is used as a source, and the self-curling effect of the graphene oxide under the weakly acidic hydrothermal condition is utilized, so that a catalyst and strong acid do not need to be introduced, the preparation process is simple, and the application of the graphene oxide in the fields of catalyst carriers and energy storage is facilitated. 一种水热法制备碳纳米管的方法,属于纳米材料制备技术领域,其制备方法是将氧化石墨烯(GO)粉末置于去离子水中,经过超声,获得GO溶液;向GO溶液滴入稀盐酸,得到酸化的GO溶液;再将酸化GO溶液置于反应釜中,反应温度20</description><subject>CHEMISTRY</subject><subject>COMPOUNDS THEREOF</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDxTS3JyE9RSMsvUigoSi1ILMrMS1dITixKys9TyEvMy1coKU1KVUiqVMioTCnKL8lILcpNzFHIBeviYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GhiaWFhbGliaOxsSoAQDodS_x</recordid><startdate>20220902</startdate><enddate>20220902</enddate><creator>LI BING</creator><creator>SUN WEI</creator><creator>HAN CUNXIN</creator><creator>GAO JIAWANG</creator><scope>EVB</scope></search><sort><creationdate>20220902</creationdate><title>Method for preparing carbon nano tube by hydrothermal method</title><author>LI BING ; SUN WEI ; HAN CUNXIN ; GAO JIAWANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN114988394A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS THEREOF</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>LI BING</creatorcontrib><creatorcontrib>SUN WEI</creatorcontrib><creatorcontrib>HAN CUNXIN</creatorcontrib><creatorcontrib>GAO JIAWANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LI BING</au><au>SUN WEI</au><au>HAN CUNXIN</au><au>GAO JIAWANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing carbon nano tube by hydrothermal method</title><date>2022-09-02</date><risdate>2022</risdate><abstract>A method for preparing a carbon nanotube by a hydrothermal method belongs to the technical field of nano material preparation, and comprises the following steps: placing graphene oxide (GO) powder in deionized water, and carrying out ultrasonic treatment to obtain a GO solution; dropwise adding diluted hydrochloric acid into the GO solution to obtain an acidified GO solution; and putting the acidified GO solution into a reaction kettle, and reacting at the temperature of 200 DEG C for 2 hours to obtain the carbon nanotube. According to the method, the graphene oxide is used as a source, and the self-curling effect of the graphene oxide under the weakly acidic hydrothermal condition is utilized, so that a catalyst and strong acid do not need to be introduced, the preparation process is simple, and the application of the graphene oxide in the fields of catalyst carriers and energy storage is facilitated. 一种水热法制备碳纳米管的方法,属于纳米材料制备技术领域,其制备方法是将氧化石墨烯(GO)粉末置于去离子水中,经过超声,获得GO溶液;向GO溶液滴入稀盐酸,得到酸化的GO溶液;再将酸化GO溶液置于反应釜中,反应温度20</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN114988394A
source esp@cenet
subjects CHEMISTRY
COMPOUNDS THEREOF
INORGANIC CHEMISTRY
METALLURGY
NON-METALLIC ELEMENTS
title Method for preparing carbon nano tube by hydrothermal method
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-17T23%3A49%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LI%20BING&rft.date=2022-09-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN114988394A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true