LF rapid desulfurization method of HPB300 plain carbon deformed steel bar

The invention relates to the technical field of steelmaking, in particular to an LF rapid desulfurization method of HPB300 plain carbon deformed steel bar. According to the corresponding relation between the C content of the argon station sample and the LF refining arrival oxygen, a corresponding am...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YAN WENCAI, ZHANG JIANPING, XU YOUSHUN, LI JING, LI WENJIAN, LIU ZHILONG, CHEN WENGEN, DENG CHANGFU, LIU CONGXIAN, ZHAO JIANCHENG, HUANG HONGWEI, LUO HUANXIN, CHEN SHAOCHONG, WU JUNHUI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YAN WENCAI
ZHANG JIANPING
XU YOUSHUN
LI JING
LI WENJIAN
LIU ZHILONG
CHEN WENGEN
DENG CHANGFU
LIU CONGXIAN
ZHAO JIANCHENG
HUANG HONGWEI
LUO HUANXIN
CHEN SHAOCHONG
WU JUNHUI
description The invention relates to the technical field of steelmaking, in particular to an LF rapid desulfurization method of HPB300 plain carbon deformed steel bar. According to the corresponding relation between the C content of the argon station sample and the LF refining arrival oxygen, a corresponding amount of high-aluminum slag is added, so that good diffusion deoxidation efficiency can be obtained corresponding to different C contents, and desulfurization is promoted; and moreover, the high-aluminum slag is used for replacing a ferrosilicon powder deoxidizing agent on the silicon killed steel, so that the deoxidizing effect is obvious, the desulfurization speed is synchronously accelerated, and the labor intensity of workers is effectively reduced. Meanwhile, according to the rapid desulfurization method disclosed by the invention, the addition amount of lime and the corresponding strong stirring time are controlled according to the S content of the argon station sample, so that efficient desulfurization is ens
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN114854936A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN114854936A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN114854936A3</originalsourceid><addsrcrecordid>eNrjZPD0cVMoSizITFFISS0uzUkrLcqsSizJzM9TyE0tychPUchPU_AIcDI2MFAoyEnMzFNITixKAsqmpKblF-WmpigUl6Sm5igkJRbxMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DQxMLUxNLYzNHY2LUAABD7TNw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>LF rapid desulfurization method of HPB300 plain carbon deformed steel bar</title><source>esp@cenet</source><creator>YAN WENCAI ; ZHANG JIANPING ; XU YOUSHUN ; LI JING ; LI WENJIAN ; LIU ZHILONG ; CHEN WENGEN ; DENG CHANGFU ; LIU CONGXIAN ; ZHAO JIANCHENG ; HUANG HONGWEI ; LUO HUANXIN ; CHEN SHAOCHONG ; WU JUNHUI</creator><creatorcontrib>YAN WENCAI ; ZHANG JIANPING ; XU YOUSHUN ; LI JING ; LI WENJIAN ; LIU ZHILONG ; CHEN WENGEN ; DENG CHANGFU ; LIU CONGXIAN ; ZHAO JIANCHENG ; HUANG HONGWEI ; LUO HUANXIN ; CHEN SHAOCHONG ; WU JUNHUI</creatorcontrib><description>The invention relates to the technical field of steelmaking, in particular to an LF rapid desulfurization method of HPB300 plain carbon deformed steel bar. According to the corresponding relation between the C content of the argon station sample and the LF refining arrival oxygen, a corresponding amount of high-aluminum slag is added, so that good diffusion deoxidation efficiency can be obtained corresponding to different C contents, and desulfurization is promoted; and moreover, the high-aluminum slag is used for replacing a ferrosilicon powder deoxidizing agent on the silicon killed steel, so that the deoxidizing effect is obvious, the desulfurization speed is synchronously accelerated, and the labor intensity of workers is effectively reduced. Meanwhile, according to the rapid desulfurization method disclosed by the invention, the addition amount of lime and the corresponding strong stirring time are controlled according to the S content of the argon station sample, so that efficient desulfurization is ens</description><language>chi ; eng</language><subject>CHEMISTRY ; METALLURGY ; METALLURGY OF IRON ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220805&amp;DB=EPODOC&amp;CC=CN&amp;NR=114854936A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220805&amp;DB=EPODOC&amp;CC=CN&amp;NR=114854936A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YAN WENCAI</creatorcontrib><creatorcontrib>ZHANG JIANPING</creatorcontrib><creatorcontrib>XU YOUSHUN</creatorcontrib><creatorcontrib>LI JING</creatorcontrib><creatorcontrib>LI WENJIAN</creatorcontrib><creatorcontrib>LIU ZHILONG</creatorcontrib><creatorcontrib>CHEN WENGEN</creatorcontrib><creatorcontrib>DENG CHANGFU</creatorcontrib><creatorcontrib>LIU CONGXIAN</creatorcontrib><creatorcontrib>ZHAO JIANCHENG</creatorcontrib><creatorcontrib>HUANG HONGWEI</creatorcontrib><creatorcontrib>LUO HUANXIN</creatorcontrib><creatorcontrib>CHEN SHAOCHONG</creatorcontrib><creatorcontrib>WU JUNHUI</creatorcontrib><title>LF rapid desulfurization method of HPB300 plain carbon deformed steel bar</title><description>The invention relates to the technical field of steelmaking, in particular to an LF rapid desulfurization method of HPB300 plain carbon deformed steel bar. According to the corresponding relation between the C content of the argon station sample and the LF refining arrival oxygen, a corresponding amount of high-aluminum slag is added, so that good diffusion deoxidation efficiency can be obtained corresponding to different C contents, and desulfurization is promoted; and moreover, the high-aluminum slag is used for replacing a ferrosilicon powder deoxidizing agent on the silicon killed steel, so that the deoxidizing effect is obvious, the desulfurization speed is synchronously accelerated, and the labor intensity of workers is effectively reduced. Meanwhile, according to the rapid desulfurization method disclosed by the invention, the addition amount of lime and the corresponding strong stirring time are controlled according to the S content of the argon station sample, so that efficient desulfurization is ens</description><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPD0cVMoSizITFFISS0uzUkrLcqsSizJzM9TyE0tychPUchPU_AIcDI2MFAoyEnMzFNITixKAsqmpKblF-WmpigUl6Sm5igkJRbxMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DQxMLUxNLYzNHY2LUAABD7TNw</recordid><startdate>20220805</startdate><enddate>20220805</enddate><creator>YAN WENCAI</creator><creator>ZHANG JIANPING</creator><creator>XU YOUSHUN</creator><creator>LI JING</creator><creator>LI WENJIAN</creator><creator>LIU ZHILONG</creator><creator>CHEN WENGEN</creator><creator>DENG CHANGFU</creator><creator>LIU CONGXIAN</creator><creator>ZHAO JIANCHENG</creator><creator>HUANG HONGWEI</creator><creator>LUO HUANXIN</creator><creator>CHEN SHAOCHONG</creator><creator>WU JUNHUI</creator><scope>EVB</scope></search><sort><creationdate>20220805</creationdate><title>LF rapid desulfurization method of HPB300 plain carbon deformed steel bar</title><author>YAN WENCAI ; ZHANG JIANPING ; XU YOUSHUN ; LI JING ; LI WENJIAN ; LIU ZHILONG ; CHEN WENGEN ; DENG CHANGFU ; LIU CONGXIAN ; ZHAO JIANCHENG ; HUANG HONGWEI ; LUO HUANXIN ; CHEN SHAOCHONG ; WU JUNHUI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN114854936A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><toplevel>online_resources</toplevel><creatorcontrib>YAN WENCAI</creatorcontrib><creatorcontrib>ZHANG JIANPING</creatorcontrib><creatorcontrib>XU YOUSHUN</creatorcontrib><creatorcontrib>LI JING</creatorcontrib><creatorcontrib>LI WENJIAN</creatorcontrib><creatorcontrib>LIU ZHILONG</creatorcontrib><creatorcontrib>CHEN WENGEN</creatorcontrib><creatorcontrib>DENG CHANGFU</creatorcontrib><creatorcontrib>LIU CONGXIAN</creatorcontrib><creatorcontrib>ZHAO JIANCHENG</creatorcontrib><creatorcontrib>HUANG HONGWEI</creatorcontrib><creatorcontrib>LUO HUANXIN</creatorcontrib><creatorcontrib>CHEN SHAOCHONG</creatorcontrib><creatorcontrib>WU JUNHUI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YAN WENCAI</au><au>ZHANG JIANPING</au><au>XU YOUSHUN</au><au>LI JING</au><au>LI WENJIAN</au><au>LIU ZHILONG</au><au>CHEN WENGEN</au><au>DENG CHANGFU</au><au>LIU CONGXIAN</au><au>ZHAO JIANCHENG</au><au>HUANG HONGWEI</au><au>LUO HUANXIN</au><au>CHEN SHAOCHONG</au><au>WU JUNHUI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>LF rapid desulfurization method of HPB300 plain carbon deformed steel bar</title><date>2022-08-05</date><risdate>2022</risdate><abstract>The invention relates to the technical field of steelmaking, in particular to an LF rapid desulfurization method of HPB300 plain carbon deformed steel bar. According to the corresponding relation between the C content of the argon station sample and the LF refining arrival oxygen, a corresponding amount of high-aluminum slag is added, so that good diffusion deoxidation efficiency can be obtained corresponding to different C contents, and desulfurization is promoted; and moreover, the high-aluminum slag is used for replacing a ferrosilicon powder deoxidizing agent on the silicon killed steel, so that the deoxidizing effect is obvious, the desulfurization speed is synchronously accelerated, and the labor intensity of workers is effectively reduced. Meanwhile, according to the rapid desulfurization method disclosed by the invention, the addition amount of lime and the corresponding strong stirring time are controlled according to the S content of the argon station sample, so that efficient desulfurization is ens</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN114854936A
source esp@cenet
subjects CHEMISTRY
METALLURGY
METALLURGY OF IRON
PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL
TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
title LF rapid desulfurization method of HPB300 plain carbon deformed steel bar
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T18%3A45%3A17IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YAN%20WENCAI&rft.date=2022-08-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN114854936A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true