Surface treatment method for bearing cast iron blank

The invention discloses a surface treatment method of a bearing cast iron blank, which comprises the following steps: step 1, placing the bearing cast iron blank under the condition that the temperature is 700-800 DEG C, preserving heat for 2-5 hours, and carrying out decarburization treatment on th...