Method for preparing 3N selenium from selenium slag
The invention discloses a method for preparing 3N selenium from selenium slag. The invention provides a method for preparing 3N selenium by purifying selenium slag, which comprises the following steps: crushing and grinding the selenium slag to 200-400 meshes, adding sulfuric acid for pickling to re...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | XU NA HE QIUGU XU QINGXIN YAN SEN HE XIAOCAI DIAO WEIZHI XU YAFEI REN TING SHI HUIXIAN YUAN YE REN JIUYANG |
description | The invention discloses a method for preparing 3N selenium from selenium slag. The invention provides a method for preparing 3N selenium by purifying selenium slag, which comprises the following steps: crushing and grinding the selenium slag to 200-400 meshes, adding sulfuric acid for pickling to remove copper, and carrying out solid-liquid separation to obtain copper liquid copper-removed slag; adding the copper removal slag into a sodium sulfite solution, carrying out pressure leaching, and carrying out solid-liquid separation to obtain leaching slag and a leaching solution; and after being repeatedly washed with water, the red selenium is converted into ash selenium under high-temperature baking of an infrared lamp, and the ash selenium can reach the standard of 3N selenium. The technology of pressure leaching, low-temperature selenium precipitation and high-temperature transformation is adopted, the technological process is short, the selenium recovery rate is high, the grade of obtained refined selenium |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN114715859A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN114715859A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN114715859A3</originalsourceid><addsrcrecordid>eNrjZDD2TS3JyE9RSMsvUigoSi1ILMrMS1cw9lMoTs1JzcsszVVIK8rPRfCKcxLTeRhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoaGJuaGphamlozExagDQsywc</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing 3N selenium from selenium slag</title><source>esp@cenet</source><creator>XU NA ; HE QIUGU ; XU QINGXIN ; YAN SEN ; HE XIAOCAI ; DIAO WEIZHI ; XU YAFEI ; REN TING ; SHI HUIXIAN ; YUAN YE ; REN JIUYANG</creator><creatorcontrib>XU NA ; HE QIUGU ; XU QINGXIN ; YAN SEN ; HE XIAOCAI ; DIAO WEIZHI ; XU YAFEI ; REN TING ; SHI HUIXIAN ; YUAN YE ; REN JIUYANG</creatorcontrib><description>The invention discloses a method for preparing 3N selenium from selenium slag. The invention provides a method for preparing 3N selenium by purifying selenium slag, which comprises the following steps: crushing and grinding the selenium slag to 200-400 meshes, adding sulfuric acid for pickling to remove copper, and carrying out solid-liquid separation to obtain copper liquid copper-removed slag; adding the copper removal slag into a sodium sulfite solution, carrying out pressure leaching, and carrying out solid-liquid separation to obtain leaching slag and a leaching solution; and after being repeatedly washed with water, the red selenium is converted into ash selenium under high-temperature baking of an infrared lamp, and the ash selenium can reach the standard of 3N selenium. The technology of pressure leaching, low-temperature selenium precipitation and high-temperature transformation is adopted, the technological process is short, the selenium recovery rate is high, the grade of obtained refined selenium</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS THEREOF ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220708&DB=EPODOC&CC=CN&NR=114715859A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25568,76551</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220708&DB=EPODOC&CC=CN&NR=114715859A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>XU NA</creatorcontrib><creatorcontrib>HE QIUGU</creatorcontrib><creatorcontrib>XU QINGXIN</creatorcontrib><creatorcontrib>YAN SEN</creatorcontrib><creatorcontrib>HE XIAOCAI</creatorcontrib><creatorcontrib>DIAO WEIZHI</creatorcontrib><creatorcontrib>XU YAFEI</creatorcontrib><creatorcontrib>REN TING</creatorcontrib><creatorcontrib>SHI HUIXIAN</creatorcontrib><creatorcontrib>YUAN YE</creatorcontrib><creatorcontrib>REN JIUYANG</creatorcontrib><title>Method for preparing 3N selenium from selenium slag</title><description>The invention discloses a method for preparing 3N selenium from selenium slag. The invention provides a method for preparing 3N selenium by purifying selenium slag, which comprises the following steps: crushing and grinding the selenium slag to 200-400 meshes, adding sulfuric acid for pickling to remove copper, and carrying out solid-liquid separation to obtain copper liquid copper-removed slag; adding the copper removal slag into a sodium sulfite solution, carrying out pressure leaching, and carrying out solid-liquid separation to obtain leaching slag and a leaching solution; and after being repeatedly washed with water, the red selenium is converted into ash selenium under high-temperature baking of an infrared lamp, and the ash selenium can reach the standard of 3N selenium. The technology of pressure leaching, low-temperature selenium precipitation and high-temperature transformation is adopted, the technological process is short, the selenium recovery rate is high, the grade of obtained refined selenium</description><subject>CHEMISTRY</subject><subject>COMPOUNDS THEREOF</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD2TS3JyE9RSMsvUigoSi1ILMrMS1cw9lMoTs1JzcsszVVIK8rPRfCKcxLTeRhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoaGJuaGphamlozExagDQsywc</recordid><startdate>20220708</startdate><enddate>20220708</enddate><creator>XU NA</creator><creator>HE QIUGU</creator><creator>XU QINGXIN</creator><creator>YAN SEN</creator><creator>HE XIAOCAI</creator><creator>DIAO WEIZHI</creator><creator>XU YAFEI</creator><creator>REN TING</creator><creator>SHI HUIXIAN</creator><creator>YUAN YE</creator><creator>REN JIUYANG</creator><scope>EVB</scope></search><sort><creationdate>20220708</creationdate><title>Method for preparing 3N selenium from selenium slag</title><author>XU NA ; HE QIUGU ; XU QINGXIN ; YAN SEN ; HE XIAOCAI ; DIAO WEIZHI ; XU YAFEI ; REN TING ; SHI HUIXIAN ; YUAN YE ; REN JIUYANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN114715859A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS THEREOF</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>XU NA</creatorcontrib><creatorcontrib>HE QIUGU</creatorcontrib><creatorcontrib>XU QINGXIN</creatorcontrib><creatorcontrib>YAN SEN</creatorcontrib><creatorcontrib>HE XIAOCAI</creatorcontrib><creatorcontrib>DIAO WEIZHI</creatorcontrib><creatorcontrib>XU YAFEI</creatorcontrib><creatorcontrib>REN TING</creatorcontrib><creatorcontrib>SHI HUIXIAN</creatorcontrib><creatorcontrib>YUAN YE</creatorcontrib><creatorcontrib>REN JIUYANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>XU NA</au><au>HE QIUGU</au><au>XU QINGXIN</au><au>YAN SEN</au><au>HE XIAOCAI</au><au>DIAO WEIZHI</au><au>XU YAFEI</au><au>REN TING</au><au>SHI HUIXIAN</au><au>YUAN YE</au><au>REN JIUYANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing 3N selenium from selenium slag</title><date>2022-07-08</date><risdate>2022</risdate><abstract>The invention discloses a method for preparing 3N selenium from selenium slag. The invention provides a method for preparing 3N selenium by purifying selenium slag, which comprises the following steps: crushing and grinding the selenium slag to 200-400 meshes, adding sulfuric acid for pickling to remove copper, and carrying out solid-liquid separation to obtain copper liquid copper-removed slag; adding the copper removal slag into a sodium sulfite solution, carrying out pressure leaching, and carrying out solid-liquid separation to obtain leaching slag and a leaching solution; and after being repeatedly washed with water, the red selenium is converted into ash selenium under high-temperature baking of an infrared lamp, and the ash selenium can reach the standard of 3N selenium. The technology of pressure leaching, low-temperature selenium precipitation and high-temperature transformation is adopted, the technological process is short, the selenium recovery rate is high, the grade of obtained refined selenium</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN114715859A |
source | esp@cenet |
subjects | CHEMISTRY COMPOUNDS THEREOF INORGANIC CHEMISTRY METALLURGY NON-METALLIC ELEMENTS |
title | Method for preparing 3N selenium from selenium slag |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-16T15%3A27%3A13IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=XU%20NA&rft.date=2022-07-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN114715859A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |