Preparation method of sustainable aviation fuel hydrogenation catalyst
The invention discloses a preparation method of a sustainable aviation fuel hydrogenation catalyst. The preparation method of the catalyst comprises the following steps: (1) stirring and mixing nickel salt, deionized water and an alcohol solvent for 1-5 hours under the conditions of normal temperatu...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | MA SHENGYONG WANG CHENGUANG WANG HAIYONG |
description | The invention discloses a preparation method of a sustainable aviation fuel hydrogenation catalyst. The preparation method of the catalyst comprises the following steps: (1) stirring and mixing nickel salt, deionized water and an alcohol solvent for 1-5 hours under the conditions of normal temperature and normal pressure, then adding Al2O3 into the solution, continuously stirring and mixing for 1-10 hours, and finally adding niobium salt, and stirring and mixing for 1-10 hours; and (2) drying the obtained mixed solution for 12-48 hours at the temperature of 80-150 DEG C and normal pressure in an air atmosphere. And (3) roasting the dried catalyst in a muffle furnace in an air atmosphere at normal pressure at 380-450 DEG C for 8-24 hours to obtain the Ni-Nb loaded bimetallic catalyst. The hydrogenation catalyst disclosed by the invention is simple to prepare, low in price, relatively mild and simple in use condition, long in service life and high in activity, and oxygen in bio-based hydrogenated crude oil can |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN114682263A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN114682263A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN114682263A3</originalsourceid><addsrcrecordid>eNrjZHALKEotSCxKLMnMz1PITS3JyE9RyE9TKC4tLknMzEtMyklVSCzLhEinlabmKGRUphTlp6fmQYSSE0sScyqLS3gYWNMSc4pTeaE0N4Oim2uIs4duakF-fGpxQWJyal5qSbyzn6GhiZmFkZGZsaMxMWoAkew0bA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of sustainable aviation fuel hydrogenation catalyst</title><source>esp@cenet</source><creator>MA SHENGYONG ; WANG CHENGUANG ; WANG HAIYONG</creator><creatorcontrib>MA SHENGYONG ; WANG CHENGUANG ; WANG HAIYONG</creatorcontrib><description>The invention discloses a preparation method of a sustainable aviation fuel hydrogenation catalyst. The preparation method of the catalyst comprises the following steps: (1) stirring and mixing nickel salt, deionized water and an alcohol solvent for 1-5 hours under the conditions of normal temperature and normal pressure, then adding Al2O3 into the solution, continuously stirring and mixing for 1-10 hours, and finally adding niobium salt, and stirring and mixing for 1-10 hours; and (2) drying the obtained mixed solution for 12-48 hours at the temperature of 80-150 DEG C and normal pressure in an air atmosphere. And (3) roasting the dried catalyst in a muffle furnace in an air atmosphere at normal pressure at 380-450 DEG C for 8-24 hours to obtain the Ni-Nb loaded bimetallic catalyst. The hydrogenation catalyst disclosed by the invention is simple to prepare, low in price, relatively mild and simple in use condition, long in service life and high in activity, and oxygen in bio-based hydrogenated crude oil can</description><language>chi ; eng</language><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY ; CHEMISTRY ; CRACKING HYDROCARBON OILS ; FUELS ; LUBRICANTS ; METALLURGY ; MINERAL WAXES ; PEAT ; PERFORMING OPERATIONS ; PETROLEUM, GAS OR COKE INDUSTRIES ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVEHYDROGENATION, OLIGOMERISATION, POLYMERISATION ; RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, ORGASES ; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS ; REFORMING OF NAPHTHA ; TECHNICAL GASES CONTAINING CARBON MONOXIDE ; THEIR RELEVANT APPARATUS ; TRANSPORTING</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220701&DB=EPODOC&CC=CN&NR=114682263A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25551,76304</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220701&DB=EPODOC&CC=CN&NR=114682263A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MA SHENGYONG</creatorcontrib><creatorcontrib>WANG CHENGUANG</creatorcontrib><creatorcontrib>WANG HAIYONG</creatorcontrib><title>Preparation method of sustainable aviation fuel hydrogenation catalyst</title><description>The invention discloses a preparation method of a sustainable aviation fuel hydrogenation catalyst. The preparation method of the catalyst comprises the following steps: (1) stirring and mixing nickel salt, deionized water and an alcohol solvent for 1-5 hours under the conditions of normal temperature and normal pressure, then adding Al2O3 into the solution, continuously stirring and mixing for 1-10 hours, and finally adding niobium salt, and stirring and mixing for 1-10 hours; and (2) drying the obtained mixed solution for 12-48 hours at the temperature of 80-150 DEG C and normal pressure in an air atmosphere. And (3) roasting the dried catalyst in a muffle furnace in an air atmosphere at normal pressure at 380-450 DEG C for 8-24 hours to obtain the Ni-Nb loaded bimetallic catalyst. The hydrogenation catalyst disclosed by the invention is simple to prepare, low in price, relatively mild and simple in use condition, long in service life and high in activity, and oxygen in bio-based hydrogenated crude oil can</description><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</subject><subject>CHEMISTRY</subject><subject>CRACKING HYDROCARBON OILS</subject><subject>FUELS</subject><subject>LUBRICANTS</subject><subject>METALLURGY</subject><subject>MINERAL WAXES</subject><subject>PEAT</subject><subject>PERFORMING OPERATIONS</subject><subject>PETROLEUM, GAS OR COKE INDUSTRIES</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVEHYDROGENATION, OLIGOMERISATION, POLYMERISATION</subject><subject>RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, ORGASES</subject><subject>REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS</subject><subject>REFORMING OF NAPHTHA</subject><subject>TECHNICAL GASES CONTAINING CARBON MONOXIDE</subject><subject>THEIR RELEVANT APPARATUS</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHALKEotSCxKLMnMz1PITS3JyE9RyE9TKC4tLknMzEtMyklVSCzLhEinlabmKGRUphTlp6fmQYSSE0sScyqLS3gYWNMSc4pTeaE0N4Oim2uIs4duakF-fGpxQWJyal5qSbyzn6GhiZmFkZGZsaMxMWoAkew0bA</recordid><startdate>20220701</startdate><enddate>20220701</enddate><creator>MA SHENGYONG</creator><creator>WANG CHENGUANG</creator><creator>WANG HAIYONG</creator><scope>EVB</scope></search><sort><creationdate>20220701</creationdate><title>Preparation method of sustainable aviation fuel hydrogenation catalyst</title><author>MA SHENGYONG ; WANG CHENGUANG ; WANG HAIYONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN114682263A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</topic><topic>CHEMISTRY</topic><topic>CRACKING HYDROCARBON OILS</topic><topic>FUELS</topic><topic>LUBRICANTS</topic><topic>METALLURGY</topic><topic>MINERAL WAXES</topic><topic>PEAT</topic><topic>PERFORMING OPERATIONS</topic><topic>PETROLEUM, GAS OR COKE INDUSTRIES</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVEHYDROGENATION, OLIGOMERISATION, POLYMERISATION</topic><topic>RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, ORGASES</topic><topic>REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS</topic><topic>REFORMING OF NAPHTHA</topic><topic>TECHNICAL GASES CONTAINING CARBON MONOXIDE</topic><topic>THEIR RELEVANT APPARATUS</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>MA SHENGYONG</creatorcontrib><creatorcontrib>WANG CHENGUANG</creatorcontrib><creatorcontrib>WANG HAIYONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MA SHENGYONG</au><au>WANG CHENGUANG</au><au>WANG HAIYONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of sustainable aviation fuel hydrogenation catalyst</title><date>2022-07-01</date><risdate>2022</risdate><abstract>The invention discloses a preparation method of a sustainable aviation fuel hydrogenation catalyst. The preparation method of the catalyst comprises the following steps: (1) stirring and mixing nickel salt, deionized water and an alcohol solvent for 1-5 hours under the conditions of normal temperature and normal pressure, then adding Al2O3 into the solution, continuously stirring and mixing for 1-10 hours, and finally adding niobium salt, and stirring and mixing for 1-10 hours; and (2) drying the obtained mixed solution for 12-48 hours at the temperature of 80-150 DEG C and normal pressure in an air atmosphere. And (3) roasting the dried catalyst in a muffle furnace in an air atmosphere at normal pressure at 380-450 DEG C for 8-24 hours to obtain the Ni-Nb loaded bimetallic catalyst. The hydrogenation catalyst disclosed by the invention is simple to prepare, low in price, relatively mild and simple in use condition, long in service life and high in activity, and oxygen in bio-based hydrogenated crude oil can</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN114682263A |
source | esp@cenet |
subjects | CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY CHEMISTRY CRACKING HYDROCARBON OILS FUELS LUBRICANTS METALLURGY MINERAL WAXES PEAT PERFORMING OPERATIONS PETROLEUM, GAS OR COKE INDUSTRIES PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVEHYDROGENATION, OLIGOMERISATION, POLYMERISATION RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, ORGASES REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS REFORMING OF NAPHTHA TECHNICAL GASES CONTAINING CARBON MONOXIDE THEIR RELEVANT APPARATUS TRANSPORTING |
title | Preparation method of sustainable aviation fuel hydrogenation catalyst |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-15T10%3A39%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MA%20SHENGYONG&rft.date=2022-07-01&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN114682263A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |