Synthesis method of hollow calcium hydroxide microspheres

The invention provides a method for synthesizing hollow calcium hydroxide microspheres, which comprises the following steps of: firstly, weighing corresponding anhydrous calcium chloride, anhydrous sodium carbonate and folic acid, mixing the weighed substances, uniformly mixing in a beaker by using...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MO FUWANG, LYU LIN, FEI XINYI, WEN QIUXIANG, PAN XIANHONG, MENG XIANGHUI, TAN HUAGENG, LAN BAOJIE, SUN FENGLU, ZHANG QIANGCHANG, TANG QUAN, LIN CAIGUANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MO FUWANG
LYU LIN
FEI XINYI
WEN QIUXIANG
PAN XIANHONG
MENG XIANGHUI
TAN HUAGENG
LAN BAOJIE
SUN FENGLU
ZHANG QIANGCHANG
TANG QUAN
LIN CAIGUANG
description The invention provides a method for synthesizing hollow calcium hydroxide microspheres, which comprises the following steps of: firstly, weighing corresponding anhydrous calcium chloride, anhydrous sodium carbonate and folic acid, mixing the weighed substances, uniformly mixing in a beaker by using water, putting into a polytetrafluoroethylene reaction kettle, putting into a drying oven, heating and reacting for 12 hours at 200 DEG C under the air condition, and cooling to room temperature to obtain the hollow calcium hydroxide microspheres. And cooling to room temperature, taking out, filtering, washing, drying, putting into a corundum crucible, roasting for 2 hours in an air atmosphere at 800 DEG C, naturally cooling to room temperature, taking out, and uniformly grinding to obtain white powder. According to the hollow calcium hydroxide microspheres prepared by the method, the synthesized product overcomes the defect that a traditional calcium hydroxide product is single in structure, the calcium hydroxide
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN114671449A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN114671449A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN114671449A3</originalsourceid><addsrcrecordid>eNrjZLAMrswryUgtzixWyE0tychPUchPU8jIz8nJL1dITsxJzizNVcioTCnKr8hMSVXIzUwuyi8uyEgtSi3mYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GhiZm5oYmJpaOxsSoAQCKqy9h</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Synthesis method of hollow calcium hydroxide microspheres</title><source>esp@cenet</source><creator>MO FUWANG ; LYU LIN ; FEI XINYI ; WEN QIUXIANG ; PAN XIANHONG ; MENG XIANGHUI ; TAN HUAGENG ; LAN BAOJIE ; SUN FENGLU ; ZHANG QIANGCHANG ; TANG QUAN ; LIN CAIGUANG</creator><creatorcontrib>MO FUWANG ; LYU LIN ; FEI XINYI ; WEN QIUXIANG ; PAN XIANHONG ; MENG XIANGHUI ; TAN HUAGENG ; LAN BAOJIE ; SUN FENGLU ; ZHANG QIANGCHANG ; TANG QUAN ; LIN CAIGUANG</creatorcontrib><description>The invention provides a method for synthesizing hollow calcium hydroxide microspheres, which comprises the following steps of: firstly, weighing corresponding anhydrous calcium chloride, anhydrous sodium carbonate and folic acid, mixing the weighed substances, uniformly mixing in a beaker by using water, putting into a polytetrafluoroethylene reaction kettle, putting into a drying oven, heating and reacting for 12 hours at 200 DEG C under the air condition, and cooling to room temperature to obtain the hollow calcium hydroxide microspheres. And cooling to room temperature, taking out, filtering, washing, drying, putting into a corundum crucible, roasting for 2 hours in an air atmosphere at 800 DEG C, naturally cooling to room temperature, taking out, and uniformly grinding to obtain white powder. According to the hollow calcium hydroxide microspheres prepared by the method, the synthesized product overcomes the defect that a traditional calcium hydroxide product is single in structure, the calcium hydroxide</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS ; INORGANIC CHEMISTRY ; METALLURGY</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220628&amp;DB=EPODOC&amp;CC=CN&amp;NR=114671449A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220628&amp;DB=EPODOC&amp;CC=CN&amp;NR=114671449A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MO FUWANG</creatorcontrib><creatorcontrib>LYU LIN</creatorcontrib><creatorcontrib>FEI XINYI</creatorcontrib><creatorcontrib>WEN QIUXIANG</creatorcontrib><creatorcontrib>PAN XIANHONG</creatorcontrib><creatorcontrib>MENG XIANGHUI</creatorcontrib><creatorcontrib>TAN HUAGENG</creatorcontrib><creatorcontrib>LAN BAOJIE</creatorcontrib><creatorcontrib>SUN FENGLU</creatorcontrib><creatorcontrib>ZHANG QIANGCHANG</creatorcontrib><creatorcontrib>TANG QUAN</creatorcontrib><creatorcontrib>LIN CAIGUANG</creatorcontrib><title>Synthesis method of hollow calcium hydroxide microspheres</title><description>The invention provides a method for synthesizing hollow calcium hydroxide microspheres, which comprises the following steps of: firstly, weighing corresponding anhydrous calcium chloride, anhydrous sodium carbonate and folic acid, mixing the weighed substances, uniformly mixing in a beaker by using water, putting into a polytetrafluoroethylene reaction kettle, putting into a drying oven, heating and reacting for 12 hours at 200 DEG C under the air condition, and cooling to room temperature to obtain the hollow calcium hydroxide microspheres. And cooling to room temperature, taking out, filtering, washing, drying, putting into a corundum crucible, roasting for 2 hours in an air atmosphere at 800 DEG C, naturally cooling to room temperature, taking out, and uniformly grinding to obtain white powder. According to the hollow calcium hydroxide microspheres prepared by the method, the synthesized product overcomes the defect that a traditional calcium hydroxide product is single in structure, the calcium hydroxide</description><subject>CHEMISTRY</subject><subject>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAMrswryUgtzixWyE0tychPUchPU8jIz8nJL1dITsxJzizNVcioTCnKr8hMSVXIzUwuyi8uyEgtSi3mYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GhiZm5oYmJpaOxsSoAQCKqy9h</recordid><startdate>20220628</startdate><enddate>20220628</enddate><creator>MO FUWANG</creator><creator>LYU LIN</creator><creator>FEI XINYI</creator><creator>WEN QIUXIANG</creator><creator>PAN XIANHONG</creator><creator>MENG XIANGHUI</creator><creator>TAN HUAGENG</creator><creator>LAN BAOJIE</creator><creator>SUN FENGLU</creator><creator>ZHANG QIANGCHANG</creator><creator>TANG QUAN</creator><creator>LIN CAIGUANG</creator><scope>EVB</scope></search><sort><creationdate>20220628</creationdate><title>Synthesis method of hollow calcium hydroxide microspheres</title><author>MO FUWANG ; LYU LIN ; FEI XINYI ; WEN QIUXIANG ; PAN XIANHONG ; MENG XIANGHUI ; TAN HUAGENG ; LAN BAOJIE ; SUN FENGLU ; ZHANG QIANGCHANG ; TANG QUAN ; LIN CAIGUANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN114671449A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><toplevel>online_resources</toplevel><creatorcontrib>MO FUWANG</creatorcontrib><creatorcontrib>LYU LIN</creatorcontrib><creatorcontrib>FEI XINYI</creatorcontrib><creatorcontrib>WEN QIUXIANG</creatorcontrib><creatorcontrib>PAN XIANHONG</creatorcontrib><creatorcontrib>MENG XIANGHUI</creatorcontrib><creatorcontrib>TAN HUAGENG</creatorcontrib><creatorcontrib>LAN BAOJIE</creatorcontrib><creatorcontrib>SUN FENGLU</creatorcontrib><creatorcontrib>ZHANG QIANGCHANG</creatorcontrib><creatorcontrib>TANG QUAN</creatorcontrib><creatorcontrib>LIN CAIGUANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MO FUWANG</au><au>LYU LIN</au><au>FEI XINYI</au><au>WEN QIUXIANG</au><au>PAN XIANHONG</au><au>MENG XIANGHUI</au><au>TAN HUAGENG</au><au>LAN BAOJIE</au><au>SUN FENGLU</au><au>ZHANG QIANGCHANG</au><au>TANG QUAN</au><au>LIN CAIGUANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Synthesis method of hollow calcium hydroxide microspheres</title><date>2022-06-28</date><risdate>2022</risdate><abstract>The invention provides a method for synthesizing hollow calcium hydroxide microspheres, which comprises the following steps of: firstly, weighing corresponding anhydrous calcium chloride, anhydrous sodium carbonate and folic acid, mixing the weighed substances, uniformly mixing in a beaker by using water, putting into a polytetrafluoroethylene reaction kettle, putting into a drying oven, heating and reacting for 12 hours at 200 DEG C under the air condition, and cooling to room temperature to obtain the hollow calcium hydroxide microspheres. And cooling to room temperature, taking out, filtering, washing, drying, putting into a corundum crucible, roasting for 2 hours in an air atmosphere at 800 DEG C, naturally cooling to room temperature, taking out, and uniformly grinding to obtain white powder. According to the hollow calcium hydroxide microspheres prepared by the method, the synthesized product overcomes the defect that a traditional calcium hydroxide product is single in structure, the calcium hydroxide</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN114671449A
source esp@cenet
subjects CHEMISTRY
COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS
INORGANIC CHEMISTRY
METALLURGY
title Synthesis method of hollow calcium hydroxide microspheres
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-04T16%3A55%3A34IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MO%20FUWANG&rft.date=2022-06-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN114671449A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true