Preparation process of steel slag-based water permeable brick cured by hydration-carbonization coupling system and steel slag-based carbonized water permeable brick
The invention belongs to the technical field of steel slag building material resource utilization and carbon capture, and particularly relates to a steel slag-based water permeable brick cured by using CO2 through a hydration-carbonization coupling system and a preparation process of the steel slag-...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | WANG SONGNING ZHANG YUZHUO FANG YANFENG WANG QINGHE YAO SHUHONG WANG YANQIN |
description | The invention belongs to the technical field of steel slag building material resource utilization and carbon capture, and particularly relates to a steel slag-based water permeable brick cured by using CO2 through a hydration-carbonization coupling system and a preparation process of the steel slag-based water permeable brick. The preparation method comprises the following steps: uniformly mixing coarse aggregate and water according to a proper liquid-solid ratio, adding a gelling material, water and a carbon sequestration reinforcing agent, uniformly stirring, pouring into a mold for compression molding, curing for 4-10 hours under the conditions that the temperature is 20-25 DEG C and the relative humidity is about 95%, and demolding to obtain a semi-finished product of the steel slag water-permeable brick; and curing for 12-18 hours under the condition that the relative humidity is less than 75%, and carbonizing and curing for 2-8 hours in a carbonization reaction kettle to obtain the steel slag-based carb |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN114538849A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN114538849A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN114538849A3</originalsourceid><addsrcrecordid>eNqNzTEKwkAQBdA0FqLeYTxAipAIsZSgWImFfZjdTOLiZneZSZB4Hg9qIFqJYDXF___NPHqemQIydsY7COw1iYCvQToiC2KxiRUKVXDHjhgCcUuoLIFio2-gex4zNcB1qCYk1sjKO_OYSO37YI1rQIaRbAFd9W1_Jr_eLKNZjVZo9b6LaH3YX4pjTMGXJAE1OerK4pQk2SbN82y7S__pvABDvleq</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation process of steel slag-based water permeable brick cured by hydration-carbonization coupling system and steel slag-based carbonized water permeable brick</title><source>esp@cenet</source><creator>WANG SONGNING ; ZHANG YUZHUO ; FANG YANFENG ; WANG QINGHE ; YAO SHUHONG ; WANG YANQIN</creator><creatorcontrib>WANG SONGNING ; ZHANG YUZHUO ; FANG YANFENG ; WANG QINGHE ; YAO SHUHONG ; WANG YANQIN</creatorcontrib><description>The invention belongs to the technical field of steel slag building material resource utilization and carbon capture, and particularly relates to a steel slag-based water permeable brick cured by using CO2 through a hydration-carbonization coupling system and a preparation process of the steel slag-based water permeable brick. The preparation method comprises the following steps: uniformly mixing coarse aggregate and water according to a proper liquid-solid ratio, adding a gelling material, water and a carbon sequestration reinforcing agent, uniformly stirring, pouring into a mold for compression molding, curing for 4-10 hours under the conditions that the temperature is 20-25 DEG C and the relative humidity is about 95%, and demolding to obtain a semi-finished product of the steel slag water-permeable brick; and curing for 12-18 hours under the condition that the relative humidity is less than 75%, and carbonizing and curing for 2-8 hours in a carbonization reaction kettle to obtain the steel slag-based carb</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; PERFORMING OPERATIONS ; REFRACTORIES ; SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER ; SLAG ; TRANSPORTING ; TREATMENT OF NATURAL STONE ; WORKING CEMENT, CLAY, OR STONE</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220527&DB=EPODOC&CC=CN&NR=114538849A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25555,76308</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220527&DB=EPODOC&CC=CN&NR=114538849A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG SONGNING</creatorcontrib><creatorcontrib>ZHANG YUZHUO</creatorcontrib><creatorcontrib>FANG YANFENG</creatorcontrib><creatorcontrib>WANG QINGHE</creatorcontrib><creatorcontrib>YAO SHUHONG</creatorcontrib><creatorcontrib>WANG YANQIN</creatorcontrib><title>Preparation process of steel slag-based water permeable brick cured by hydration-carbonization coupling system and steel slag-based carbonized water permeable brick</title><description>The invention belongs to the technical field of steel slag building material resource utilization and carbon capture, and particularly relates to a steel slag-based water permeable brick cured by using CO2 through a hydration-carbonization coupling system and a preparation process of the steel slag-based water permeable brick. The preparation method comprises the following steps: uniformly mixing coarse aggregate and water according to a proper liquid-solid ratio, adding a gelling material, water and a carbon sequestration reinforcing agent, uniformly stirring, pouring into a mold for compression molding, curing for 4-10 hours under the conditions that the temperature is 20-25 DEG C and the relative humidity is about 95%, and demolding to obtain a semi-finished product of the steel slag water-permeable brick; and curing for 12-18 hours under the condition that the relative humidity is less than 75%, and carbonizing and curing for 2-8 hours in a carbonization reaction kettle to obtain the steel slag-based carb</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>REFRACTORIES</subject><subject>SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER</subject><subject>SLAG</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF NATURAL STONE</subject><subject>WORKING CEMENT, CLAY, OR STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNzTEKwkAQBdA0FqLeYTxAipAIsZSgWImFfZjdTOLiZneZSZB4Hg9qIFqJYDXF___NPHqemQIydsY7COw1iYCvQToiC2KxiRUKVXDHjhgCcUuoLIFio2-gex4zNcB1qCYk1sjKO_OYSO37YI1rQIaRbAFd9W1_Jr_eLKNZjVZo9b6LaH3YX4pjTMGXJAE1OerK4pQk2SbN82y7S__pvABDvleq</recordid><startdate>20220527</startdate><enddate>20220527</enddate><creator>WANG SONGNING</creator><creator>ZHANG YUZHUO</creator><creator>FANG YANFENG</creator><creator>WANG QINGHE</creator><creator>YAO SHUHONG</creator><creator>WANG YANQIN</creator><scope>EVB</scope></search><sort><creationdate>20220527</creationdate><title>Preparation process of steel slag-based water permeable brick cured by hydration-carbonization coupling system and steel slag-based carbonized water permeable brick</title><author>WANG SONGNING ; ZHANG YUZHUO ; FANG YANFENG ; WANG QINGHE ; YAO SHUHONG ; WANG YANQIN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN114538849A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>REFRACTORIES</topic><topic>SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER</topic><topic>SLAG</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF NATURAL STONE</topic><topic>WORKING CEMENT, CLAY, OR STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG SONGNING</creatorcontrib><creatorcontrib>ZHANG YUZHUO</creatorcontrib><creatorcontrib>FANG YANFENG</creatorcontrib><creatorcontrib>WANG QINGHE</creatorcontrib><creatorcontrib>YAO SHUHONG</creatorcontrib><creatorcontrib>WANG YANQIN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG SONGNING</au><au>ZHANG YUZHUO</au><au>FANG YANFENG</au><au>WANG QINGHE</au><au>YAO SHUHONG</au><au>WANG YANQIN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation process of steel slag-based water permeable brick cured by hydration-carbonization coupling system and steel slag-based carbonized water permeable brick</title><date>2022-05-27</date><risdate>2022</risdate><abstract>The invention belongs to the technical field of steel slag building material resource utilization and carbon capture, and particularly relates to a steel slag-based water permeable brick cured by using CO2 through a hydration-carbonization coupling system and a preparation process of the steel slag-based water permeable brick. The preparation method comprises the following steps: uniformly mixing coarse aggregate and water according to a proper liquid-solid ratio, adding a gelling material, water and a carbon sequestration reinforcing agent, uniformly stirring, pouring into a mold for compression molding, curing for 4-10 hours under the conditions that the temperature is 20-25 DEG C and the relative humidity is about 95%, and demolding to obtain a semi-finished product of the steel slag water-permeable brick; and curing for 12-18 hours under the condition that the relative humidity is less than 75%, and carbonizing and curing for 2-8 hours in a carbonization reaction kettle to obtain the steel slag-based carb</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN114538849A |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE LIME, MAGNESIA METALLURGY PERFORMING OPERATIONS REFRACTORIES SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER SLAG TRANSPORTING TREATMENT OF NATURAL STONE WORKING CEMENT, CLAY, OR STONE |
title | Preparation process of steel slag-based water permeable brick cured by hydration-carbonization coupling system and steel slag-based carbonized water permeable brick |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-15T02%3A02%3A18IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20SONGNING&rft.date=2022-05-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN114538849A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |