High-heat-resistance PA plastic and preparation method thereof

The invention discloses a high-heat-resistance PA (Polyamide) plastic and a preparation method of the high-heat-resistance PA plastic. The invention discloses a plastic master batch, which is prepared from the following ingredients in parts by weight: 100 to 120 parts of PA resin, 20 to 40 parts of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: LU SENWEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LU SENWEI
description The invention discloses a high-heat-resistance PA (Polyamide) plastic and a preparation method of the high-heat-resistance PA plastic. The invention discloses a plastic master batch, which is prepared from the following ingredients in parts by weight: 100 to 120 parts of PA resin, 20 to 40 parts of polyamide, 20 to 30 parts of glass fibers, 10 to 15 parts of triisocyanurate, 1 to 10 parts of hydroxyl silicone oil, 5 to 10 parts of polypropylene ester, 10 to 30 parts of auxiliaries, 40 to 60 parts of ethyl alcohol and 40 to 50 parts of softened water. According to the present invention, by adding the flame retardant, the material has characteristics of good wear resistance, good pressure resistance, excellent heat resistance and excellent flame resistance, and the production cost is reduced by improving the preparation method. 本发明公开了一种高耐热性PA塑料及其制备方法,其中,一种高耐热性PA塑料,按重量份数计包括如下组分:100-120份的PA树脂、20-40份的聚酰胺、20-30份的玻璃纤维、10-15份的三异三聚氰酸酯、1-10份的羟基硅油、5-10份的聚丙烯酯、10-30份的助剂、40-60份的乙醇、40-50份的软化水,本发明通过改进塑料母粒的配方,有效提高了塑料成品的力学性能,使
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN114507437A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN114507437A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN114507437A3</originalsourceid><addsrcrecordid>eNrjZLDzyEzP0M1ITSzRLUotziwuScxLTlUIcFQoyEksLslMVkjMS1EoKEotSCxKLMnMz1PITS3JyE9RKMlILUrNT-NhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfHOfoaGJqYG5ibG5o7GxKgBADcxMFk</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>High-heat-resistance PA plastic and preparation method thereof</title><source>esp@cenet</source><creator>LU SENWEI</creator><creatorcontrib>LU SENWEI</creatorcontrib><description>The invention discloses a high-heat-resistance PA (Polyamide) plastic and a preparation method of the high-heat-resistance PA plastic. The invention discloses a plastic master batch, which is prepared from the following ingredients in parts by weight: 100 to 120 parts of PA resin, 20 to 40 parts of polyamide, 20 to 30 parts of glass fibers, 10 to 15 parts of triisocyanurate, 1 to 10 parts of hydroxyl silicone oil, 5 to 10 parts of polypropylene ester, 10 to 30 parts of auxiliaries, 40 to 60 parts of ethyl alcohol and 40 to 50 parts of softened water. According to the present invention, by adding the flame retardant, the material has characteristics of good wear resistance, good pressure resistance, excellent heat resistance and excellent flame resistance, and the production cost is reduced by improving the preparation method. 本发明公开了一种高耐热性PA塑料及其制备方法,其中,一种高耐热性PA塑料,按重量份数计包括如下组分:100-120份的PA树脂、20-40份的聚酰胺、20-30份的玻璃纤维、10-15份的三异三聚氰酸酯、1-10份的羟基硅油、5-10份的聚丙烯酯、10-30份的助剂、40-60份的乙醇、40-50份的软化水,本发明通过改进塑料母粒的配方,有效提高了塑料成品的力学性能,使</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220517&amp;DB=EPODOC&amp;CC=CN&amp;NR=114507437A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220517&amp;DB=EPODOC&amp;CC=CN&amp;NR=114507437A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LU SENWEI</creatorcontrib><title>High-heat-resistance PA plastic and preparation method thereof</title><description>The invention discloses a high-heat-resistance PA (Polyamide) plastic and a preparation method of the high-heat-resistance PA plastic. The invention discloses a plastic master batch, which is prepared from the following ingredients in parts by weight: 100 to 120 parts of PA resin, 20 to 40 parts of polyamide, 20 to 30 parts of glass fibers, 10 to 15 parts of triisocyanurate, 1 to 10 parts of hydroxyl silicone oil, 5 to 10 parts of polypropylene ester, 10 to 30 parts of auxiliaries, 40 to 60 parts of ethyl alcohol and 40 to 50 parts of softened water. According to the present invention, by adding the flame retardant, the material has characteristics of good wear resistance, good pressure resistance, excellent heat resistance and excellent flame resistance, and the production cost is reduced by improving the preparation method. 本发明公开了一种高耐热性PA塑料及其制备方法,其中,一种高耐热性PA塑料,按重量份数计包括如下组分:100-120份的PA树脂、20-40份的聚酰胺、20-30份的玻璃纤维、10-15份的三异三聚氰酸酯、1-10份的羟基硅油、5-10份的聚丙烯酯、10-30份的助剂、40-60份的乙醇、40-50份的软化水,本发明通过改进塑料母粒的配方,有效提高了塑料成品的力学性能,使</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDzyEzP0M1ITSzRLUotziwuScxLTlUIcFQoyEksLslMVkjMS1EoKEotSCxKLMnMz1PITS3JyE9RKMlILUrNT-NhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfHOfoaGJqYG5ibG5o7GxKgBADcxMFk</recordid><startdate>20220517</startdate><enddate>20220517</enddate><creator>LU SENWEI</creator><scope>EVB</scope></search><sort><creationdate>20220517</creationdate><title>High-heat-resistance PA plastic and preparation method thereof</title><author>LU SENWEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN114507437A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>LU SENWEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LU SENWEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>High-heat-resistance PA plastic and preparation method thereof</title><date>2022-05-17</date><risdate>2022</risdate><abstract>The invention discloses a high-heat-resistance PA (Polyamide) plastic and a preparation method of the high-heat-resistance PA plastic. The invention discloses a plastic master batch, which is prepared from the following ingredients in parts by weight: 100 to 120 parts of PA resin, 20 to 40 parts of polyamide, 20 to 30 parts of glass fibers, 10 to 15 parts of triisocyanurate, 1 to 10 parts of hydroxyl silicone oil, 5 to 10 parts of polypropylene ester, 10 to 30 parts of auxiliaries, 40 to 60 parts of ethyl alcohol and 40 to 50 parts of softened water. According to the present invention, by adding the flame retardant, the material has characteristics of good wear resistance, good pressure resistance, excellent heat resistance and excellent flame resistance, and the production cost is reduced by improving the preparation method. 本发明公开了一种高耐热性PA塑料及其制备方法,其中,一种高耐热性PA塑料,按重量份数计包括如下组分:100-120份的PA树脂、20-40份的聚酰胺、20-30份的玻璃纤维、10-15份的三异三聚氰酸酯、1-10份的羟基硅油、5-10份的聚丙烯酯、10-30份的助剂、40-60份的乙醇、40-50份的软化水,本发明通过改进塑料母粒的配方,有效提高了塑料成品的力学性能,使</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN114507437A
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS
title High-heat-resistance PA plastic and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-15T13%3A29%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LU%20SENWEI&rft.date=2022-05-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN114507437A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true