Method for producing graphite fibers by catalytic graphitization

The invention provides a method for producing graphite fibers by catalytic graphitization, the method comprises the following steps: taking polyacrylonitrile-based precursor, and pre-oxidizing in air atmosphere; performing low-temperature carbonization; performing high-temperature carbonization; pre...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHAO HUI, LI YONG, QIAN YANGPING
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHAO HUI
LI YONG
QIAN YANGPING
description The invention provides a method for producing graphite fibers by catalytic graphitization, the method comprises the following steps: taking polyacrylonitrile-based precursor, and pre-oxidizing in air atmosphere; performing low-temperature carbonization; performing high-temperature carbonization; preparing a boron-containing catalyst; soaking the carbonized carbon fibers in a boron-containing catalyst and drying at the temperature of 180-200 DEG C, wherein the drying time is 60-90 s; and graphitizing: graphitizing for 20-40 seconds in an argon atmosphere at the temperature of 2200-2400 DEG C to obtain the graphite fibers. According to the invention, hydrogen chloride gas with a certain concentration is introduced into the carbonization section atmosphere, so that the carbonization time and temperature can be reduced, and the purity of fibers can be improved; meanwhile, the carbonized fiber is impregnated with a boron compound and then graphitized, the graphitization temperature can be reduced, the graphitizati
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113981569A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113981569A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113981569A3</originalsourceid><addsrcrecordid>eNrjZHDwTS3JyE9RSMsvUigoyk8pTc7MS1dIL0osyMgsSVVIy0xKLSpWSKpUSE4sScypLMlMhklmViWWZObn8TCwpiXmFKfyQmluBkU31xBnD93Ugvz41OKCxOTUvNSSeGc_Q0NjSwtDUzNLR2Ni1AAA_n8x5Q</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for producing graphite fibers by catalytic graphitization</title><source>esp@cenet</source><creator>ZHAO HUI ; LI YONG ; QIAN YANGPING</creator><creatorcontrib>ZHAO HUI ; LI YONG ; QIAN YANGPING</creatorcontrib><description>The invention provides a method for producing graphite fibers by catalytic graphitization, the method comprises the following steps: taking polyacrylonitrile-based precursor, and pre-oxidizing in air atmosphere; performing low-temperature carbonization; performing high-temperature carbonization; preparing a boron-containing catalyst; soaking the carbonized carbon fibers in a boron-containing catalyst and drying at the temperature of 180-200 DEG C, wherein the drying time is 60-90 s; and graphitizing: graphitizing for 20-40 seconds in an argon atmosphere at the temperature of 2200-2400 DEG C to obtain the graphite fibers. According to the invention, hydrogen chloride gas with a certain concentration is introduced into the carbonization section atmosphere, so that the carbonization time and temperature can be reduced, and the purity of fibers can be improved; meanwhile, the carbonized fiber is impregnated with a boron compound and then graphitized, the graphitization temperature can be reduced, the graphitizati</description><language>chi ; eng</language><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS ; CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS ; NATURAL OR ARTIFICIAL THREADS OR FIBRES ; SPINNING ; TEXTILES</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220128&amp;DB=EPODOC&amp;CC=CN&amp;NR=113981569A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220128&amp;DB=EPODOC&amp;CC=CN&amp;NR=113981569A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHAO HUI</creatorcontrib><creatorcontrib>LI YONG</creatorcontrib><creatorcontrib>QIAN YANGPING</creatorcontrib><title>Method for producing graphite fibers by catalytic graphitization</title><description>The invention provides a method for producing graphite fibers by catalytic graphitization, the method comprises the following steps: taking polyacrylonitrile-based precursor, and pre-oxidizing in air atmosphere; performing low-temperature carbonization; performing high-temperature carbonization; preparing a boron-containing catalyst; soaking the carbonized carbon fibers in a boron-containing catalyst and drying at the temperature of 180-200 DEG C, wherein the drying time is 60-90 s; and graphitizing: graphitizing for 20-40 seconds in an argon atmosphere at the temperature of 2200-2400 DEG C to obtain the graphite fibers. According to the invention, hydrogen chloride gas with a certain concentration is introduced into the carbonization section atmosphere, so that the carbonization time and temperature can be reduced, and the purity of fibers can be improved; meanwhile, the carbonized fiber is impregnated with a boron compound and then graphitized, the graphitization temperature can be reduced, the graphitizati</description><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</subject><subject>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</subject><subject>NATURAL OR ARTIFICIAL THREADS OR FIBRES</subject><subject>SPINNING</subject><subject>TEXTILES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHDwTS3JyE9RSMsvUigoyk8pTc7MS1dIL0osyMgsSVVIy0xKLSpWSKpUSE4sScypLMlMhklmViWWZObn8TCwpiXmFKfyQmluBkU31xBnD93Ugvz41OKCxOTUvNSSeGc_Q0NjSwtDUzNLR2Ni1AAA_n8x5Q</recordid><startdate>20220128</startdate><enddate>20220128</enddate><creator>ZHAO HUI</creator><creator>LI YONG</creator><creator>QIAN YANGPING</creator><scope>EVB</scope></search><sort><creationdate>20220128</creationdate><title>Method for producing graphite fibers by catalytic graphitization</title><author>ZHAO HUI ; LI YONG ; QIAN YANGPING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113981569A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2022</creationdate><topic>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</topic><topic>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</topic><topic>NATURAL OR ARTIFICIAL THREADS OR FIBRES</topic><topic>SPINNING</topic><topic>TEXTILES</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHAO HUI</creatorcontrib><creatorcontrib>LI YONG</creatorcontrib><creatorcontrib>QIAN YANGPING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHAO HUI</au><au>LI YONG</au><au>QIAN YANGPING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for producing graphite fibers by catalytic graphitization</title><date>2022-01-28</date><risdate>2022</risdate><abstract>The invention provides a method for producing graphite fibers by catalytic graphitization, the method comprises the following steps: taking polyacrylonitrile-based precursor, and pre-oxidizing in air atmosphere; performing low-temperature carbonization; performing high-temperature carbonization; preparing a boron-containing catalyst; soaking the carbonized carbon fibers in a boron-containing catalyst and drying at the temperature of 180-200 DEG C, wherein the drying time is 60-90 s; and graphitizing: graphitizing for 20-40 seconds in an argon atmosphere at the temperature of 2200-2400 DEG C to obtain the graphite fibers. According to the invention, hydrogen chloride gas with a certain concentration is introduced into the carbonization section atmosphere, so that the carbonization time and temperature can be reduced, and the purity of fibers can be improved; meanwhile, the carbonized fiber is impregnated with a boron compound and then graphitized, the graphitization temperature can be reduced, the graphitizati</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN113981569A
source esp@cenet
subjects APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS
CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS
NATURAL OR ARTIFICIAL THREADS OR FIBRES
SPINNING
TEXTILES
title Method for producing graphite fibers by catalytic graphitization
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-14T00%3A50%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHAO%20HUI&rft.date=2022-01-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113981569A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true