Polypropylene composite material with low linear expansion coefficient and high surface hardness and preparation method thereof
The invention relates to a polypropylene composite material with low linear expansion coefficient and high surface hardness, which comprises the following components by weight: 100 parts of PP resin, 5 to 15 parts of functional fused silica powder, 10 to 20 parts of functional wollastonite powder, 8...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | KONG WEI JI CHENG MENG CHENGMING CHEN GUANGWEI YUE TONGJIAN |
description | The invention relates to a polypropylene composite material with low linear expansion coefficient and high surface hardness, which comprises the following components by weight: 100 parts of PP resin, 5 to 15 parts of functional fused silica powder, 10 to 20 parts of functional wollastonite powder, 8 to 15 parts of POE, and 0.3 to 0.5 part of an antioxidant. The functional wollastonite powder is a product obtained after wollastonite is subjected to surface treatment by an ultra-dispersion coupling agent, and the weight part ratio of the wollastonite to the ultra-dispersion coupling agent is (20: 1)-(25: 1); the functional fused silica powder is a product obtained after surface treatment is carried out on fused silica through an ultra-dispersion coupling agent, and the weight part ratio of the fused silica to the ultra-dispersion coupling agent is 25: 1-30: 1; the linear expansion coefficient of the fused silica is 0.5 * 10 mm/mm/DEG C; the ultra-dispersion coupling agent is a coupling agent SP-1013 produce |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113831641A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113831641A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113831641A3</originalsourceid><addsrcrecordid>eNqNjDEKwkAQRdNYiHqH8QAWISK2EhQrsbAPQ_LXHdjsLLsrMZVXN4oHsHrFf__Ni9dV3RiihtHBg1rtgybJoJ4zorCjQbIlpwM58eBIeAb2SdRPMoyRVuAzse_Iyt1SekTDLchy7DxS-i4hInDk_Hn1yFY7yhYRapbFzLBLWP24KNan460-bxC0QQpTyiM39aUsq31V7rblofrHeQO-REoZ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Polypropylene composite material with low linear expansion coefficient and high surface hardness and preparation method thereof</title><source>esp@cenet</source><creator>KONG WEI ; JI CHENG ; MENG CHENGMING ; CHEN GUANGWEI ; YUE TONGJIAN</creator><creatorcontrib>KONG WEI ; JI CHENG ; MENG CHENGMING ; CHEN GUANGWEI ; YUE TONGJIAN</creatorcontrib><description>The invention relates to a polypropylene composite material with low linear expansion coefficient and high surface hardness, which comprises the following components by weight: 100 parts of PP resin, 5 to 15 parts of functional fused silica powder, 10 to 20 parts of functional wollastonite powder, 8 to 15 parts of POE, and 0.3 to 0.5 part of an antioxidant. The functional wollastonite powder is a product obtained after wollastonite is subjected to surface treatment by an ultra-dispersion coupling agent, and the weight part ratio of the wollastonite to the ultra-dispersion coupling agent is (20: 1)-(25: 1); the functional fused silica powder is a product obtained after surface treatment is carried out on fused silica through an ultra-dispersion coupling agent, and the weight part ratio of the fused silica to the ultra-dispersion coupling agent is 25: 1-30: 1; the linear expansion coefficient of the fused silica is 0.5 * 10<-6> mm/mm/DEG C; the ultra-dispersion coupling agent is a coupling agent SP-1013 produce</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20211224&DB=EPODOC&CC=CN&NR=113831641A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20211224&DB=EPODOC&CC=CN&NR=113831641A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KONG WEI</creatorcontrib><creatorcontrib>JI CHENG</creatorcontrib><creatorcontrib>MENG CHENGMING</creatorcontrib><creatorcontrib>CHEN GUANGWEI</creatorcontrib><creatorcontrib>YUE TONGJIAN</creatorcontrib><title>Polypropylene composite material with low linear expansion coefficient and high surface hardness and preparation method thereof</title><description>The invention relates to a polypropylene composite material with low linear expansion coefficient and high surface hardness, which comprises the following components by weight: 100 parts of PP resin, 5 to 15 parts of functional fused silica powder, 10 to 20 parts of functional wollastonite powder, 8 to 15 parts of POE, and 0.3 to 0.5 part of an antioxidant. The functional wollastonite powder is a product obtained after wollastonite is subjected to surface treatment by an ultra-dispersion coupling agent, and the weight part ratio of the wollastonite to the ultra-dispersion coupling agent is (20: 1)-(25: 1); the functional fused silica powder is a product obtained after surface treatment is carried out on fused silica through an ultra-dispersion coupling agent, and the weight part ratio of the fused silica to the ultra-dispersion coupling agent is 25: 1-30: 1; the linear expansion coefficient of the fused silica is 0.5 * 10<-6> mm/mm/DEG C; the ultra-dispersion coupling agent is a coupling agent SP-1013 produce</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjDEKwkAQRdNYiHqH8QAWISK2EhQrsbAPQ_LXHdjsLLsrMZVXN4oHsHrFf__Ni9dV3RiihtHBg1rtgybJoJ4zorCjQbIlpwM58eBIeAb2SdRPMoyRVuAzse_Iyt1SekTDLchy7DxS-i4hInDk_Hn1yFY7yhYRapbFzLBLWP24KNan460-bxC0QQpTyiM39aUsq31V7rblofrHeQO-REoZ</recordid><startdate>20211224</startdate><enddate>20211224</enddate><creator>KONG WEI</creator><creator>JI CHENG</creator><creator>MENG CHENGMING</creator><creator>CHEN GUANGWEI</creator><creator>YUE TONGJIAN</creator><scope>EVB</scope></search><sort><creationdate>20211224</creationdate><title>Polypropylene composite material with low linear expansion coefficient and high surface hardness and preparation method thereof</title><author>KONG WEI ; JI CHENG ; MENG CHENGMING ; CHEN GUANGWEI ; YUE TONGJIAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113831641A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>KONG WEI</creatorcontrib><creatorcontrib>JI CHENG</creatorcontrib><creatorcontrib>MENG CHENGMING</creatorcontrib><creatorcontrib>CHEN GUANGWEI</creatorcontrib><creatorcontrib>YUE TONGJIAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KONG WEI</au><au>JI CHENG</au><au>MENG CHENGMING</au><au>CHEN GUANGWEI</au><au>YUE TONGJIAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Polypropylene composite material with low linear expansion coefficient and high surface hardness and preparation method thereof</title><date>2021-12-24</date><risdate>2021</risdate><abstract>The invention relates to a polypropylene composite material with low linear expansion coefficient and high surface hardness, which comprises the following components by weight: 100 parts of PP resin, 5 to 15 parts of functional fused silica powder, 10 to 20 parts of functional wollastonite powder, 8 to 15 parts of POE, and 0.3 to 0.5 part of an antioxidant. The functional wollastonite powder is a product obtained after wollastonite is subjected to surface treatment by an ultra-dispersion coupling agent, and the weight part ratio of the wollastonite to the ultra-dispersion coupling agent is (20: 1)-(25: 1); the functional fused silica powder is a product obtained after surface treatment is carried out on fused silica through an ultra-dispersion coupling agent, and the weight part ratio of the fused silica to the ultra-dispersion coupling agent is 25: 1-30: 1; the linear expansion coefficient of the fused silica is 0.5 * 10<-6> mm/mm/DEG C; the ultra-dispersion coupling agent is a coupling agent SP-1013 produce</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN113831641A |
source | esp@cenet |
subjects | CHEMISTRY COMPOSITIONS BASED THEREON COMPOSITIONS OF MACROMOLECULAR COMPOUNDS METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS THEIR PREPARATION OR CHEMICAL WORKING-UP USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS |
title | Polypropylene composite material with low linear expansion coefficient and high surface hardness and preparation method thereof |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-09T10%3A57%3A43IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KONG%20WEI&rft.date=2021-12-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113831641A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |