Anti-whitening efficient binder for vamp cloth and foxing strip rubber as well as preparation method and application of anti-whitening efficient binder

The invention discloses an anti-whitening efficient binder for vamp cloth and foxing strip rubber as well as preparation method and application of anti-whitening efficient binder. The anti-whitening efficient binder is characterized in that a binding system consists of three parts; a binding agent F...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANG XIAOFEI, ZHANG SHILIN, WANG CHUNQIAO, TIAN JI, MAO CHANGHU, JIN QIHUAI, LIAO PUJIANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YANG XIAOFEI
ZHANG SHILIN
WANG CHUNQIAO
TIAN JI
MAO CHANGHU
JIN QIHUAI
LIAO PUJIANG
description The invention discloses an anti-whitening efficient binder for vamp cloth and foxing strip rubber as well as preparation method and application of anti-whitening efficient binder. The anti-whitening efficient binder is characterized in that a binding system consists of three parts; a binding agent FB050 (100 parts) containing 5 parts of a curing agent and 3 parts of a 5% sodium carboxymethyl cellulose water swelling body is brushed on a binding part on the surface of the vamp cloth, and then drying is conducted for 45 minutes under the condition of hot circulating air at a temperature of 40-50 DEG C; meanwhile, high-viscosity gasoline adhesive cement made of SCR5 natural rubber is brushed on the bonding surface of the foxing strip rubber and dried for 25-30 minutes; a swabbed and dried foxing strip is bonded on the surface of a shoe upper which is well dried after swabbing, and pressing is conducted for 1-1.5 seconds; and hot air vulcanization is performed under the conditions of 115 DEG C and 0.38 MPa for 40
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113789139A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113789139A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113789139A3</originalsourceid><addsrcrecordid>eNqNjTEOgkAQRWksjHqH8QAUhEIpCdFYWdmTAWZlkmV2szuKN_G6globq5e8vJ-_TJ6lKKdjz0rCcgUyhlsmUWhYOgpgXIA7Dh5a67QHlG5SjzmNGthDuDXNlGGEkayd6QN5DKjsBAbS3nXvFXpvuf1oZyb183edLAzaSJsvV8n2eLhUp5S8qyl6bElI6-qcZfluX2R5Ueb_NC8MbFIl</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Anti-whitening efficient binder for vamp cloth and foxing strip rubber as well as preparation method and application of anti-whitening efficient binder</title><source>esp@cenet</source><creator>YANG XIAOFEI ; ZHANG SHILIN ; WANG CHUNQIAO ; TIAN JI ; MAO CHANGHU ; JIN QIHUAI ; LIAO PUJIANG</creator><creatorcontrib>YANG XIAOFEI ; ZHANG SHILIN ; WANG CHUNQIAO ; TIAN JI ; MAO CHANGHU ; JIN QIHUAI ; LIAO PUJIANG</creatorcontrib><description>The invention discloses an anti-whitening efficient binder for vamp cloth and foxing strip rubber as well as preparation method and application of anti-whitening efficient binder. The anti-whitening efficient binder is characterized in that a binding system consists of three parts; a binding agent FB050 (100 parts) containing 5 parts of a curing agent and 3 parts of a 5% sodium carboxymethyl cellulose water swelling body is brushed on a binding part on the surface of the vamp cloth, and then drying is conducted for 45 minutes under the condition of hot circulating air at a temperature of 40-50 DEG C; meanwhile, high-viscosity gasoline adhesive cement made of SCR5 natural rubber is brushed on the bonding surface of the foxing strip rubber and dried for 25-30 minutes; a swabbed and dried foxing strip is bonded on the surface of a shoe upper which is well dried after swabbing, and pressing is conducted for 1-1.5 seconds; and hot air vulcanization is performed under the conditions of 115 DEG C and 0.38 MPa for 40</description><language>chi ; eng</language><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ; ADHESIVES ; CHARACTERISTIC FEATURES OF FOOTWEAR ; CHEMISTRY ; DYES ; FOOTWEAR ; HUMAN NECESSITIES ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ; PAINTS ; PARTS OF FOOTWEAR ; POLISHES ; USE OF MATERIALS AS ADHESIVES</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211214&amp;DB=EPODOC&amp;CC=CN&amp;NR=113789139A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211214&amp;DB=EPODOC&amp;CC=CN&amp;NR=113789139A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YANG XIAOFEI</creatorcontrib><creatorcontrib>ZHANG SHILIN</creatorcontrib><creatorcontrib>WANG CHUNQIAO</creatorcontrib><creatorcontrib>TIAN JI</creatorcontrib><creatorcontrib>MAO CHANGHU</creatorcontrib><creatorcontrib>JIN QIHUAI</creatorcontrib><creatorcontrib>LIAO PUJIANG</creatorcontrib><title>Anti-whitening efficient binder for vamp cloth and foxing strip rubber as well as preparation method and application of anti-whitening efficient binder</title><description>The invention discloses an anti-whitening efficient binder for vamp cloth and foxing strip rubber as well as preparation method and application of anti-whitening efficient binder. The anti-whitening efficient binder is characterized in that a binding system consists of three parts; a binding agent FB050 (100 parts) containing 5 parts of a curing agent and 3 parts of a 5% sodium carboxymethyl cellulose water swelling body is brushed on a binding part on the surface of the vamp cloth, and then drying is conducted for 45 minutes under the condition of hot circulating air at a temperature of 40-50 DEG C; meanwhile, high-viscosity gasoline adhesive cement made of SCR5 natural rubber is brushed on the bonding surface of the foxing strip rubber and dried for 25-30 minutes; a swabbed and dried foxing strip is bonded on the surface of a shoe upper which is well dried after swabbing, and pressing is conducted for 1-1.5 seconds; and hot air vulcanization is performed under the conditions of 115 DEG C and 0.38 MPa for 40</description><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</subject><subject>ADHESIVES</subject><subject>CHARACTERISTIC FEATURES OF FOOTWEAR</subject><subject>CHEMISTRY</subject><subject>DYES</subject><subject>FOOTWEAR</subject><subject>HUMAN NECESSITIES</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</subject><subject>PAINTS</subject><subject>PARTS OF FOOTWEAR</subject><subject>POLISHES</subject><subject>USE OF MATERIALS AS ADHESIVES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjTEOgkAQRWksjHqH8QAUhEIpCdFYWdmTAWZlkmV2szuKN_G6globq5e8vJ-_TJ6lKKdjz0rCcgUyhlsmUWhYOgpgXIA7Dh5a67QHlG5SjzmNGthDuDXNlGGEkayd6QN5DKjsBAbS3nXvFXpvuf1oZyb183edLAzaSJsvV8n2eLhUp5S8qyl6bElI6-qcZfluX2R5Ueb_NC8MbFIl</recordid><startdate>20211214</startdate><enddate>20211214</enddate><creator>YANG XIAOFEI</creator><creator>ZHANG SHILIN</creator><creator>WANG CHUNQIAO</creator><creator>TIAN JI</creator><creator>MAO CHANGHU</creator><creator>JIN QIHUAI</creator><creator>LIAO PUJIANG</creator><scope>EVB</scope></search><sort><creationdate>20211214</creationdate><title>Anti-whitening efficient binder for vamp cloth and foxing strip rubber as well as preparation method and application of anti-whitening efficient binder</title><author>YANG XIAOFEI ; ZHANG SHILIN ; WANG CHUNQIAO ; TIAN JI ; MAO CHANGHU ; JIN QIHUAI ; LIAO PUJIANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113789139A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</topic><topic>ADHESIVES</topic><topic>CHARACTERISTIC FEATURES OF FOOTWEAR</topic><topic>CHEMISTRY</topic><topic>DYES</topic><topic>FOOTWEAR</topic><topic>HUMAN NECESSITIES</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</topic><topic>PAINTS</topic><topic>PARTS OF FOOTWEAR</topic><topic>POLISHES</topic><topic>USE OF MATERIALS AS ADHESIVES</topic><toplevel>online_resources</toplevel><creatorcontrib>YANG XIAOFEI</creatorcontrib><creatorcontrib>ZHANG SHILIN</creatorcontrib><creatorcontrib>WANG CHUNQIAO</creatorcontrib><creatorcontrib>TIAN JI</creatorcontrib><creatorcontrib>MAO CHANGHU</creatorcontrib><creatorcontrib>JIN QIHUAI</creatorcontrib><creatorcontrib>LIAO PUJIANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YANG XIAOFEI</au><au>ZHANG SHILIN</au><au>WANG CHUNQIAO</au><au>TIAN JI</au><au>MAO CHANGHU</au><au>JIN QIHUAI</au><au>LIAO PUJIANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Anti-whitening efficient binder for vamp cloth and foxing strip rubber as well as preparation method and application of anti-whitening efficient binder</title><date>2021-12-14</date><risdate>2021</risdate><abstract>The invention discloses an anti-whitening efficient binder for vamp cloth and foxing strip rubber as well as preparation method and application of anti-whitening efficient binder. The anti-whitening efficient binder is characterized in that a binding system consists of three parts; a binding agent FB050 (100 parts) containing 5 parts of a curing agent and 3 parts of a 5% sodium carboxymethyl cellulose water swelling body is brushed on a binding part on the surface of the vamp cloth, and then drying is conducted for 45 minutes under the condition of hot circulating air at a temperature of 40-50 DEG C; meanwhile, high-viscosity gasoline adhesive cement made of SCR5 natural rubber is brushed on the bonding surface of the foxing strip rubber and dried for 25-30 minutes; a swabbed and dried foxing strip is bonded on the surface of a shoe upper which is well dried after swabbing, and pressing is conducted for 1-1.5 seconds; and hot air vulcanization is performed under the conditions of 115 DEG C and 0.38 MPa for 40</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN113789139A
source esp@cenet
subjects ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE
ADHESIVES
CHARACTERISTIC FEATURES OF FOOTWEAR
CHEMISTRY
DYES
FOOTWEAR
HUMAN NECESSITIES
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL
PAINTS
PARTS OF FOOTWEAR
POLISHES
USE OF MATERIALS AS ADHESIVES
title Anti-whitening efficient binder for vamp cloth and foxing strip rubber as well as preparation method and application of anti-whitening efficient binder
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T22%3A09%3A07IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YANG%20XIAOFEI&rft.date=2021-12-14&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113789139A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true