Modified magnesium phosphate cement mortar and preparation method thereof

The invention discloses a modified magnesium phosphate cement mortar, which is composed of the following components: magnesium oxide, potassium dihydrogen phosphate, a composite retarder, sand, silica fume and water, wherein the molar ratio of magnesium oxide to potassium dihydrogen phosphate in the...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MA SIMIN, YE YANXIA, XIE FULIN, FU CUIHONG, JING CONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MA SIMIN
YE YANXIA
XIE FULIN
FU CUIHONG
JING CONG
description The invention discloses a modified magnesium phosphate cement mortar, which is composed of the following components: magnesium oxide, potassium dihydrogen phosphate, a composite retarder, sand, silica fume and water, wherein the molar ratio of magnesium oxide to potassium dihydrogen phosphate in the modified magnesium phosphate cement mortar is 4: 1-6: 1, and the addition amount of the composite retarder is 3-10% of the total mass of magnesium oxide and potassium dihydrogen phosphate; the mass ratio of the silica fume to the total mass of the magnesium oxide, the potassium dihydrogen phosphate and the silica fume is 5%-20%, the mass ratio of the sand to the total mass of the magnesium oxide, the phosphate and the silica fume is 1: 1, the magnesium oxide, the potassium dihydrogen phosphate, the composite retarder and the silica fume jointly form a gelling component, and the mass ratio of the water to the gelling component is 0.2-0.25. The modified magnesium phosphate cement mortar disclosed by the invention is
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113773042A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113773042A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113773042A3</originalsourceid><addsrcrecordid>eNqNyjEKAjEQBdA0FqLeYTyA4Bpha1kULbSyX4bNXxMwmSEZ72_jAaxe85budpeQ5oRAmV8FLX0yaZSmkQ00IaMYZanGlbgE0grlypakUIZFCWQRFTKv3WLmd8Pm58ptL-fncN1BZURTnlBg4_DoOt_3fn88nPw_5wslHDUy</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Modified magnesium phosphate cement mortar and preparation method thereof</title><source>esp@cenet</source><creator>MA SIMIN ; YE YANXIA ; XIE FULIN ; FU CUIHONG ; JING CONG</creator><creatorcontrib>MA SIMIN ; YE YANXIA ; XIE FULIN ; FU CUIHONG ; JING CONG</creatorcontrib><description>The invention discloses a modified magnesium phosphate cement mortar, which is composed of the following components: magnesium oxide, potassium dihydrogen phosphate, a composite retarder, sand, silica fume and water, wherein the molar ratio of magnesium oxide to potassium dihydrogen phosphate in the modified magnesium phosphate cement mortar is 4: 1-6: 1, and the addition amount of the composite retarder is 3-10% of the total mass of magnesium oxide and potassium dihydrogen phosphate; the mass ratio of the silica fume to the total mass of the magnesium oxide, the potassium dihydrogen phosphate and the silica fume is 5%-20%, the mass ratio of the sand to the total mass of the magnesium oxide, the phosphate and the silica fume is 1: 1, the magnesium oxide, the potassium dihydrogen phosphate, the composite retarder and the silica fume jointly form a gelling component, and the mass ratio of the water to the gelling component is 0.2-0.25. The modified magnesium phosphate cement mortar disclosed by the invention is</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211210&amp;DB=EPODOC&amp;CC=CN&amp;NR=113773042A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25562,76317</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211210&amp;DB=EPODOC&amp;CC=CN&amp;NR=113773042A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MA SIMIN</creatorcontrib><creatorcontrib>YE YANXIA</creatorcontrib><creatorcontrib>XIE FULIN</creatorcontrib><creatorcontrib>FU CUIHONG</creatorcontrib><creatorcontrib>JING CONG</creatorcontrib><title>Modified magnesium phosphate cement mortar and preparation method thereof</title><description>The invention discloses a modified magnesium phosphate cement mortar, which is composed of the following components: magnesium oxide, potassium dihydrogen phosphate, a composite retarder, sand, silica fume and water, wherein the molar ratio of magnesium oxide to potassium dihydrogen phosphate in the modified magnesium phosphate cement mortar is 4: 1-6: 1, and the addition amount of the composite retarder is 3-10% of the total mass of magnesium oxide and potassium dihydrogen phosphate; the mass ratio of the silica fume to the total mass of the magnesium oxide, the potassium dihydrogen phosphate and the silica fume is 5%-20%, the mass ratio of the sand to the total mass of the magnesium oxide, the phosphate and the silica fume is 1: 1, the magnesium oxide, the potassium dihydrogen phosphate, the composite retarder and the silica fume jointly form a gelling component, and the mass ratio of the water to the gelling component is 0.2-0.25. The modified magnesium phosphate cement mortar disclosed by the invention is</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjEKAjEQBdA0FqLeYTyA4Bpha1kULbSyX4bNXxMwmSEZ72_jAaxe85budpeQ5oRAmV8FLX0yaZSmkQ00IaMYZanGlbgE0grlypakUIZFCWQRFTKv3WLmd8Pm58ptL-fncN1BZURTnlBg4_DoOt_3fn88nPw_5wslHDUy</recordid><startdate>20211210</startdate><enddate>20211210</enddate><creator>MA SIMIN</creator><creator>YE YANXIA</creator><creator>XIE FULIN</creator><creator>FU CUIHONG</creator><creator>JING CONG</creator><scope>EVB</scope></search><sort><creationdate>20211210</creationdate><title>Modified magnesium phosphate cement mortar and preparation method thereof</title><author>MA SIMIN ; YE YANXIA ; XIE FULIN ; FU CUIHONG ; JING CONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113773042A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>MA SIMIN</creatorcontrib><creatorcontrib>YE YANXIA</creatorcontrib><creatorcontrib>XIE FULIN</creatorcontrib><creatorcontrib>FU CUIHONG</creatorcontrib><creatorcontrib>JING CONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MA SIMIN</au><au>YE YANXIA</au><au>XIE FULIN</au><au>FU CUIHONG</au><au>JING CONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Modified magnesium phosphate cement mortar and preparation method thereof</title><date>2021-12-10</date><risdate>2021</risdate><abstract>The invention discloses a modified magnesium phosphate cement mortar, which is composed of the following components: magnesium oxide, potassium dihydrogen phosphate, a composite retarder, sand, silica fume and water, wherein the molar ratio of magnesium oxide to potassium dihydrogen phosphate in the modified magnesium phosphate cement mortar is 4: 1-6: 1, and the addition amount of the composite retarder is 3-10% of the total mass of magnesium oxide and potassium dihydrogen phosphate; the mass ratio of the silica fume to the total mass of the magnesium oxide, the potassium dihydrogen phosphate and the silica fume is 5%-20%, the mass ratio of the sand to the total mass of the magnesium oxide, the phosphate and the silica fume is 1: 1, the magnesium oxide, the potassium dihydrogen phosphate, the composite retarder and the silica fume jointly form a gelling component, and the mass ratio of the water to the gelling component is 0.2-0.25. The modified magnesium phosphate cement mortar disclosed by the invention is</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN113773042A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Modified magnesium phosphate cement mortar and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-09T17%3A13%3A17IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MA%20SIMIN&rft.date=2021-12-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113773042A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true