High-modulus asphalt mixture as well as preparation method and application thereof
The invention discloses a high-modulus asphalt mixture as well as a preparation method and application thereof, and belongs to the technical field of pavement construction. The high-modulus asphalt mixture is prepared by mixing high-modulus asphalt, aggregate, machine-made sand and mineral powder ac...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | HUANG YONGSHENG ZHANG QIYUE PAN MINGJIANG AILIKEMU AIZEZI WANG SISI WANG YONGXUE YANG BILIANG |
description | The invention discloses a high-modulus asphalt mixture as well as a preparation method and application thereof, and belongs to the technical field of pavement construction. The high-modulus asphalt mixture is prepared by mixing high-modulus asphalt, aggregate, machine-made sand and mineral powder according to a preset proportion, the high-modulus asphalt has the needle penetration of 15-40mm, the softening point of more than or equal to 60 DEG C, the ductility of more than or equal to 5cm, the flash point of more than or equal to 230 DEG C, the density of more than or equal to 1.1 g/cm < 3 >, the elastic recovery rate of more than or equal to 50%, the 48-hour softening point difference corresponding to storage stability segregation of less than or equal to 2.5 DEG C, the mass change of less than or equal to +/-0.5%, the residual needle penetration ratio of more than or equal to 70% and the residual ductility of more than or equal to 2cm. When the high-modulus asphalt, replacing SBS modified asphalt or asphalt |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113772998A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113772998A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113772998A3</originalsourceid><addsrcrecordid>eNrjZAjyyEzP0M3NTynNKS1WSCwuyEjMKVHIzawoKS1KBfIVylNzckB0QVFqQWJRYklmfp5CbmpJRn6KQmIeEBcU5GQmQ4RLMlKLUvPTeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoaGxubmRpaWFozExagA_XDh-</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>High-modulus asphalt mixture as well as preparation method and application thereof</title><source>esp@cenet</source><creator>HUANG YONGSHENG ; ZHANG QIYUE ; PAN MINGJIANG ; AILIKEMU AIZEZI ; WANG SISI ; WANG YONGXUE ; YANG BILIANG</creator><creatorcontrib>HUANG YONGSHENG ; ZHANG QIYUE ; PAN MINGJIANG ; AILIKEMU AIZEZI ; WANG SISI ; WANG YONGXUE ; YANG BILIANG</creatorcontrib><description>The invention discloses a high-modulus asphalt mixture as well as a preparation method and application thereof, and belongs to the technical field of pavement construction. The high-modulus asphalt mixture is prepared by mixing high-modulus asphalt, aggregate, machine-made sand and mineral powder according to a preset proportion, the high-modulus asphalt has the needle penetration of 15-40mm, the softening point of more than or equal to 60 DEG C, the ductility of more than or equal to 5cm, the flash point of more than or equal to 230 DEG C, the density of more than or equal to 1.1 g/cm < 3 >, the elastic recovery rate of more than or equal to 50%, the 48-hour softening point difference corresponding to storage stability segregation of less than or equal to 2.5 DEG C, the mass change of less than or equal to +/-0.5%, the residual needle penetration ratio of more than or equal to 70% and the residual ductility of more than or equal to 2cm. When the high-modulus asphalt, replacing SBS modified asphalt or asphalt</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES ; CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE ; FIXED CONSTRUCTIONS ; LIME, MAGNESIA ; MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20211210&DB=EPODOC&CC=CN&NR=113772998A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20211210&DB=EPODOC&CC=CN&NR=113772998A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HUANG YONGSHENG</creatorcontrib><creatorcontrib>ZHANG QIYUE</creatorcontrib><creatorcontrib>PAN MINGJIANG</creatorcontrib><creatorcontrib>AILIKEMU AIZEZI</creatorcontrib><creatorcontrib>WANG SISI</creatorcontrib><creatorcontrib>WANG YONGXUE</creatorcontrib><creatorcontrib>YANG BILIANG</creatorcontrib><title>High-modulus asphalt mixture as well as preparation method and application thereof</title><description>The invention discloses a high-modulus asphalt mixture as well as a preparation method and application thereof, and belongs to the technical field of pavement construction. The high-modulus asphalt mixture is prepared by mixing high-modulus asphalt, aggregate, machine-made sand and mineral powder according to a preset proportion, the high-modulus asphalt has the needle penetration of 15-40mm, the softening point of more than or equal to 60 DEG C, the ductility of more than or equal to 5cm, the flash point of more than or equal to 230 DEG C, the density of more than or equal to 1.1 g/cm < 3 >, the elastic recovery rate of more than or equal to 50%, the 48-hour softening point difference corresponding to storage stability segregation of less than or equal to 2.5 DEG C, the mass change of less than or equal to +/-0.5%, the residual needle penetration ratio of more than or equal to 70% and the residual ductility of more than or equal to 2cm. When the high-modulus asphalt, replacing SBS modified asphalt or asphalt</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES</subject><subject>CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE</subject><subject>FIXED CONSTRUCTIONS</subject><subject>LIME, MAGNESIA</subject><subject>MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZAjyyEzP0M3NTynNKS1WSCwuyEjMKVHIzawoKS1KBfIVylNzckB0QVFqQWJRYklmfp5CbmpJRn6KQmIeEBcU5GQmQ4RLMlKLUvPTeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoaGxubmRpaWFozExagA_XDh-</recordid><startdate>20211210</startdate><enddate>20211210</enddate><creator>HUANG YONGSHENG</creator><creator>ZHANG QIYUE</creator><creator>PAN MINGJIANG</creator><creator>AILIKEMU AIZEZI</creator><creator>WANG SISI</creator><creator>WANG YONGXUE</creator><creator>YANG BILIANG</creator><scope>EVB</scope></search><sort><creationdate>20211210</creationdate><title>High-modulus asphalt mixture as well as preparation method and application thereof</title><author>HUANG YONGSHENG ; ZHANG QIYUE ; PAN MINGJIANG ; AILIKEMU AIZEZI ; WANG SISI ; WANG YONGXUE ; YANG BILIANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113772998A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES</topic><topic>CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE</topic><topic>FIXED CONSTRUCTIONS</topic><topic>LIME, MAGNESIA</topic><topic>MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>HUANG YONGSHENG</creatorcontrib><creatorcontrib>ZHANG QIYUE</creatorcontrib><creatorcontrib>PAN MINGJIANG</creatorcontrib><creatorcontrib>AILIKEMU AIZEZI</creatorcontrib><creatorcontrib>WANG SISI</creatorcontrib><creatorcontrib>WANG YONGXUE</creatorcontrib><creatorcontrib>YANG BILIANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HUANG YONGSHENG</au><au>ZHANG QIYUE</au><au>PAN MINGJIANG</au><au>AILIKEMU AIZEZI</au><au>WANG SISI</au><au>WANG YONGXUE</au><au>YANG BILIANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>High-modulus asphalt mixture as well as preparation method and application thereof</title><date>2021-12-10</date><risdate>2021</risdate><abstract>The invention discloses a high-modulus asphalt mixture as well as a preparation method and application thereof, and belongs to the technical field of pavement construction. The high-modulus asphalt mixture is prepared by mixing high-modulus asphalt, aggregate, machine-made sand and mineral powder according to a preset proportion, the high-modulus asphalt has the needle penetration of 15-40mm, the softening point of more than or equal to 60 DEG C, the ductility of more than or equal to 5cm, the flash point of more than or equal to 230 DEG C, the density of more than or equal to 1.1 g/cm < 3 >, the elastic recovery rate of more than or equal to 50%, the 48-hour softening point difference corresponding to storage stability segregation of less than or equal to 2.5 DEG C, the mass change of less than or equal to +/-0.5%, the residual needle penetration ratio of more than or equal to 70% and the residual ductility of more than or equal to 2cm. When the high-modulus asphalt, replacing SBS modified asphalt or asphalt</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN113772998A |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE FIXED CONSTRUCTIONS LIME, MAGNESIA MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR METALLURGY REFRACTORIES SLAG TREATMENT OF NATURAL STONE |
title | High-modulus asphalt mixture as well as preparation method and application thereof |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T05%3A59%3A03IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HUANG%20YONGSHENG&rft.date=2021-12-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113772998A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |