HIGHLY EFFICIENT MOLTEN IRON ALLOY REFINING METHOD
This molten iron alloy refining method is for refining a molten iron alloy while blowing oxygen to a molten iron alloy bath in a converter, wherein when a direct current is supplied between a first electrode disposed above the molten iron alloy bath and a second electrode disposed in contact with th...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | POLYAKOV V F FUJI TAKEHIKO NAITO KENICHIRO MATSUO MITSUTAKA MORITA KOJI SEMYKIN S I HIRATA HIROSHI SASAKI NAOTO NIINO SOHICHI ONUKI KAZUO WAKAO MASAMITSU |
description | This molten iron alloy refining method is for refining a molten iron alloy while blowing oxygen to a molten iron alloy bath in a converter, wherein when a direct current is supplied between a first electrode disposed above the molten iron alloy bath and a second electrode disposed in contact with the molten iron alloy bath, at least one of formulas (1)-(4) is satisfied, where IP [A] represents the magnitude of the average of the direct current during a current passage period in which the current is passed, IP' [A] represents the magnitude of the average of the direct current during a current passage period within one minute immediately before the blowing of oxygen is stopped, Ws [t] represents the amount of molten steel in the converter, and As [m2] represents the area of the internal cross-section of the furnace at the belly thereof. (1): IP>=0.125*Ws. (2): IP>=1.5*As. (3): IP'>=0.125*Ws. (4): IP'>=1.5*As.
该熔融铁合金的精炼方法,是在向转炉内的熔融铁合金浴送氧的状态下精炼熔融铁合金的方法,在配置于所述熔融铁合金浴上方的第一电极与配置成与所述熔融铁合金浴接触的第二电极之间供给直流电流,在将流通所述直流电流的通电 |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113631729A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113631729A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113631729A3</originalsourceid><addsrcrecordid>eNrjZDDy8HT38IlUcHVz83T2dPULUfD19wlx9VPwDPL3U3D08fGPVAhydfP08_RzV_B1DfHwd-FhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfHOfoaGxmbGhuZGlo7GxKgBAHOqJsg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>HIGHLY EFFICIENT MOLTEN IRON ALLOY REFINING METHOD</title><source>esp@cenet</source><creator>POLYAKOV V F ; FUJI TAKEHIKO ; NAITO KENICHIRO ; MATSUO MITSUTAKA ; MORITA KOJI ; SEMYKIN S I ; HIRATA HIROSHI ; SASAKI NAOTO ; NIINO SOHICHI ; ONUKI KAZUO ; WAKAO MASAMITSU</creator><creatorcontrib>POLYAKOV V F ; FUJI TAKEHIKO ; NAITO KENICHIRO ; MATSUO MITSUTAKA ; MORITA KOJI ; SEMYKIN S I ; HIRATA HIROSHI ; SASAKI NAOTO ; NIINO SOHICHI ; ONUKI KAZUO ; WAKAO MASAMITSU</creatorcontrib><description>This molten iron alloy refining method is for refining a molten iron alloy while blowing oxygen to a molten iron alloy bath in a converter, wherein when a direct current is supplied between a first electrode disposed above the molten iron alloy bath and a second electrode disposed in contact with the molten iron alloy bath, at least one of formulas (1)-(4) is satisfied, where IP [A] represents the magnitude of the average of the direct current during a current passage period in which the current is passed, IP' [A] represents the magnitude of the average of the direct current during a current passage period within one minute immediately before the blowing of oxygen is stopped, Ws [t] represents the amount of molten steel in the converter, and As [m2] represents the area of the internal cross-section of the furnace at the belly thereof. (1): IP>=0.125*Ws. (2): IP>=1.5*As. (3): IP'>=0.125*Ws. (4): IP'>=1.5*As.
该熔融铁合金的精炼方法,是在向转炉内的熔融铁合金浴送氧的状态下精炼熔融铁合金的方法,在配置于所述熔融铁合金浴上方的第一电极与配置成与所述熔融铁合金浴接触的第二电极之间供给直流电流,在将流通所述直流电流的通电</description><language>chi ; eng</language><subject>BLASTING ; CHEMISTRY ; DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS, OR RETORTS,IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KINDOF FURNACE ; FURNACES ; HEATING ; KILNS ; LIGHTING ; MECHANICAL ENGINEERING ; METALLURGY ; METALLURGY OF IRON ; OVENS ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; RETORTS ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS ; WEAPONS</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20211109&DB=EPODOC&CC=CN&NR=113631729A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20211109&DB=EPODOC&CC=CN&NR=113631729A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>POLYAKOV V F</creatorcontrib><creatorcontrib>FUJI TAKEHIKO</creatorcontrib><creatorcontrib>NAITO KENICHIRO</creatorcontrib><creatorcontrib>MATSUO MITSUTAKA</creatorcontrib><creatorcontrib>MORITA KOJI</creatorcontrib><creatorcontrib>SEMYKIN S I</creatorcontrib><creatorcontrib>HIRATA HIROSHI</creatorcontrib><creatorcontrib>SASAKI NAOTO</creatorcontrib><creatorcontrib>NIINO SOHICHI</creatorcontrib><creatorcontrib>ONUKI KAZUO</creatorcontrib><creatorcontrib>WAKAO MASAMITSU</creatorcontrib><title>HIGHLY EFFICIENT MOLTEN IRON ALLOY REFINING METHOD</title><description>This molten iron alloy refining method is for refining a molten iron alloy while blowing oxygen to a molten iron alloy bath in a converter, wherein when a direct current is supplied between a first electrode disposed above the molten iron alloy bath and a second electrode disposed in contact with the molten iron alloy bath, at least one of formulas (1)-(4) is satisfied, where IP [A] represents the magnitude of the average of the direct current during a current passage period in which the current is passed, IP' [A] represents the magnitude of the average of the direct current during a current passage period within one minute immediately before the blowing of oxygen is stopped, Ws [t] represents the amount of molten steel in the converter, and As [m2] represents the area of the internal cross-section of the furnace at the belly thereof. (1): IP>=0.125*Ws. (2): IP>=1.5*As. (3): IP'>=0.125*Ws. (4): IP'>=1.5*As.
该熔融铁合金的精炼方法,是在向转炉内的熔融铁合金浴送氧的状态下精炼熔融铁合金的方法,在配置于所述熔融铁合金浴上方的第一电极与配置成与所述熔融铁合金浴接触的第二电极之间供给直流电流,在将流通所述直流电流的通电</description><subject>BLASTING</subject><subject>CHEMISTRY</subject><subject>DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS, OR RETORTS,IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KINDOF FURNACE</subject><subject>FURNACES</subject><subject>HEATING</subject><subject>KILNS</subject><subject>LIGHTING</subject><subject>MECHANICAL ENGINEERING</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>OVENS</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>RETORTS</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><subject>WEAPONS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDDy8HT38IlUcHVz83T2dPULUfD19wlx9VPwDPL3U3D08fGPVAhydfP08_RzV_B1DfHwd-FhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfHOfoaGxmbGhuZGlo7GxKgBAHOqJsg</recordid><startdate>20211109</startdate><enddate>20211109</enddate><creator>POLYAKOV V F</creator><creator>FUJI TAKEHIKO</creator><creator>NAITO KENICHIRO</creator><creator>MATSUO MITSUTAKA</creator><creator>MORITA KOJI</creator><creator>SEMYKIN S I</creator><creator>HIRATA HIROSHI</creator><creator>SASAKI NAOTO</creator><creator>NIINO SOHICHI</creator><creator>ONUKI KAZUO</creator><creator>WAKAO MASAMITSU</creator><scope>EVB</scope></search><sort><creationdate>20211109</creationdate><title>HIGHLY EFFICIENT MOLTEN IRON ALLOY REFINING METHOD</title><author>POLYAKOV V F ; FUJI TAKEHIKO ; NAITO KENICHIRO ; MATSUO MITSUTAKA ; MORITA KOJI ; SEMYKIN S I ; HIRATA HIROSHI ; SASAKI NAOTO ; NIINO SOHICHI ; ONUKI KAZUO ; WAKAO MASAMITSU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113631729A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>BLASTING</topic><topic>CHEMISTRY</topic><topic>DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS, OR RETORTS,IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KINDOF FURNACE</topic><topic>FURNACES</topic><topic>HEATING</topic><topic>KILNS</topic><topic>LIGHTING</topic><topic>MECHANICAL ENGINEERING</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>OVENS</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>RETORTS</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><topic>WEAPONS</topic><toplevel>online_resources</toplevel><creatorcontrib>POLYAKOV V F</creatorcontrib><creatorcontrib>FUJI TAKEHIKO</creatorcontrib><creatorcontrib>NAITO KENICHIRO</creatorcontrib><creatorcontrib>MATSUO MITSUTAKA</creatorcontrib><creatorcontrib>MORITA KOJI</creatorcontrib><creatorcontrib>SEMYKIN S I</creatorcontrib><creatorcontrib>HIRATA HIROSHI</creatorcontrib><creatorcontrib>SASAKI NAOTO</creatorcontrib><creatorcontrib>NIINO SOHICHI</creatorcontrib><creatorcontrib>ONUKI KAZUO</creatorcontrib><creatorcontrib>WAKAO MASAMITSU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>POLYAKOV V F</au><au>FUJI TAKEHIKO</au><au>NAITO KENICHIRO</au><au>MATSUO MITSUTAKA</au><au>MORITA KOJI</au><au>SEMYKIN S I</au><au>HIRATA HIROSHI</au><au>SASAKI NAOTO</au><au>NIINO SOHICHI</au><au>ONUKI KAZUO</au><au>WAKAO MASAMITSU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>HIGHLY EFFICIENT MOLTEN IRON ALLOY REFINING METHOD</title><date>2021-11-09</date><risdate>2021</risdate><abstract>This molten iron alloy refining method is for refining a molten iron alloy while blowing oxygen to a molten iron alloy bath in a converter, wherein when a direct current is supplied between a first electrode disposed above the molten iron alloy bath and a second electrode disposed in contact with the molten iron alloy bath, at least one of formulas (1)-(4) is satisfied, where IP [A] represents the magnitude of the average of the direct current during a current passage period in which the current is passed, IP' [A] represents the magnitude of the average of the direct current during a current passage period within one minute immediately before the blowing of oxygen is stopped, Ws [t] represents the amount of molten steel in the converter, and As [m2] represents the area of the internal cross-section of the furnace at the belly thereof. (1): IP>=0.125*Ws. (2): IP>=1.5*As. (3): IP'>=0.125*Ws. (4): IP'>=1.5*As.
该熔融铁合金的精炼方法,是在向转炉内的熔融铁合金浴送氧的状态下精炼熔融铁合金的方法,在配置于所述熔融铁合金浴上方的第一电极与配置成与所述熔融铁合金浴接触的第二电极之间供给直流电流,在将流通所述直流电流的通电</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN113631729A |
source | esp@cenet |
subjects | BLASTING CHEMISTRY DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS, OR RETORTS,IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KINDOF FURNACE FURNACES HEATING KILNS LIGHTING MECHANICAL ENGINEERING METALLURGY METALLURGY OF IRON OVENS PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL RETORTS TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS WEAPONS |
title | HIGHLY EFFICIENT MOLTEN IRON ALLOY REFINING METHOD |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-01T16%3A26%3A43IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=POLYAKOV%20V%20F&rft.date=2021-11-09&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113631729A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |