PROCESS FOR PREPARING COMPOSITE CATHODE FOR LITHIUM ION CELL

The present application provides a process for preparing a composite cathode for a lithium ion cell. The process comprises the steps of (i) forming a cathode slurry in a planetary mixing machine by mixing an active material, conducting diluent and binder; (ii) coating the slurry over an aluminum foi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MERCY TD, BIBIN JOHN, S ARAVAMUTHAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MERCY TD
BIBIN JOHN
S ARAVAMUTHAN
description The present application provides a process for preparing a composite cathode for a lithium ion cell. The process comprises the steps of (i) forming a cathode slurry in a planetary mixing machine by mixing an active material, conducting diluent and binder; (ii) coating the slurry over an aluminum foil substrate in a coating machine at a speed of 0.2-0.8 m/min; and (iii) calendering the cathode in a calendering machine at a temperature of 50-150 DEG C. The present invention also relates to a system for the process. The cathode has peel strength of greater than 200 gf/cm and moisture content less than 350 ppm. The lithium ion cell with the cathode disclosed in the invention and a graphite anode exhibits a capacity retention of >80% at 100% depth-of-discharge at C/2-1C charge-discharge rate when tested for 2000 cycles. 本申请提供了一种制备用于锂离子电池的复合正极的方法,包括以下步骤:(i)通过混合活性材料、导电稀释剂和粘合剂,在行星式混合机中形成正极浆料;(ii)在涂覆机中以0.2-0.8m/min的速度将浆料涂覆在铝箔基板上;(iii)在50-150℃温度下在压延机中压延正极。本申请还公开了一种用于此目的的系统。正极具有大于200gf/cm的剥离强度和小于350ppm的水分含量。具有本发明公开的正极和石
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113574711A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113574711A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113574711A3</originalsourceid><addsrcrecordid>eNrjZLAJCPJ3dg0OVnDzD1IICHINcAzy9HNXcPb3DfAP9gxxVXB2DPHwd3EFy_t4hnh4hvoqePr7KTi7-vjwMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DQ2NTcxNzQ0NHY2LUAAAHvSmB</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PROCESS FOR PREPARING COMPOSITE CATHODE FOR LITHIUM ION CELL</title><source>esp@cenet</source><creator>MERCY TD ; BIBIN JOHN ; S ARAVAMUTHAN</creator><creatorcontrib>MERCY TD ; BIBIN JOHN ; S ARAVAMUTHAN</creatorcontrib><description>The present application provides a process for preparing a composite cathode for a lithium ion cell. The process comprises the steps of (i) forming a cathode slurry in a planetary mixing machine by mixing an active material, conducting diluent and binder; (ii) coating the slurry over an aluminum foil substrate in a coating machine at a speed of 0.2-0.8 m/min; and (iii) calendering the cathode in a calendering machine at a temperature of 50-150 DEG C. The present invention also relates to a system for the process. The cathode has peel strength of greater than 200 gf/cm and moisture content less than 350 ppm. The lithium ion cell with the cathode disclosed in the invention and a graphite anode exhibits a capacity retention of &gt;80% at 100% depth-of-discharge at C/2-1C charge-discharge rate when tested for 2000 cycles. 本申请提供了一种制备用于锂离子电池的复合正极的方法,包括以下步骤:(i)通过混合活性材料、导电稀释剂和粘合剂,在行星式混合机中形成正极浆料;(ii)在涂覆机中以0.2-0.8m/min的速度将浆料涂覆在铝箔基板上;(iii)在50-150℃温度下在压延机中压延正极。本申请还公开了一种用于此目的的系统。正极具有大于200gf/cm的剥离强度和小于350ppm的水分含量。具有本发明公开的正极和石</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211029&amp;DB=EPODOC&amp;CC=CN&amp;NR=113574711A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25569,76552</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211029&amp;DB=EPODOC&amp;CC=CN&amp;NR=113574711A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MERCY TD</creatorcontrib><creatorcontrib>BIBIN JOHN</creatorcontrib><creatorcontrib>S ARAVAMUTHAN</creatorcontrib><title>PROCESS FOR PREPARING COMPOSITE CATHODE FOR LITHIUM ION CELL</title><description>The present application provides a process for preparing a composite cathode for a lithium ion cell. The process comprises the steps of (i) forming a cathode slurry in a planetary mixing machine by mixing an active material, conducting diluent and binder; (ii) coating the slurry over an aluminum foil substrate in a coating machine at a speed of 0.2-0.8 m/min; and (iii) calendering the cathode in a calendering machine at a temperature of 50-150 DEG C. The present invention also relates to a system for the process. The cathode has peel strength of greater than 200 gf/cm and moisture content less than 350 ppm. The lithium ion cell with the cathode disclosed in the invention and a graphite anode exhibits a capacity retention of &gt;80% at 100% depth-of-discharge at C/2-1C charge-discharge rate when tested for 2000 cycles. 本申请提供了一种制备用于锂离子电池的复合正极的方法,包括以下步骤:(i)通过混合活性材料、导电稀释剂和粘合剂,在行星式混合机中形成正极浆料;(ii)在涂覆机中以0.2-0.8m/min的速度将浆料涂覆在铝箔基板上;(iii)在50-150℃温度下在压延机中压延正极。本申请还公开了一种用于此目的的系统。正极具有大于200gf/cm的剥离强度和小于350ppm的水分含量。具有本发明公开的正极和石</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAJCPJ3dg0OVnDzD1IICHINcAzy9HNXcPb3DfAP9gxxVXB2DPHwd3EFy_t4hnh4hvoqePr7KTi7-vjwMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DQ2NTcxNzQ0NHY2LUAAAHvSmB</recordid><startdate>20211029</startdate><enddate>20211029</enddate><creator>MERCY TD</creator><creator>BIBIN JOHN</creator><creator>S ARAVAMUTHAN</creator><scope>EVB</scope></search><sort><creationdate>20211029</creationdate><title>PROCESS FOR PREPARING COMPOSITE CATHODE FOR LITHIUM ION CELL</title><author>MERCY TD ; BIBIN JOHN ; S ARAVAMUTHAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113574711A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>MERCY TD</creatorcontrib><creatorcontrib>BIBIN JOHN</creatorcontrib><creatorcontrib>S ARAVAMUTHAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MERCY TD</au><au>BIBIN JOHN</au><au>S ARAVAMUTHAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PROCESS FOR PREPARING COMPOSITE CATHODE FOR LITHIUM ION CELL</title><date>2021-10-29</date><risdate>2021</risdate><abstract>The present application provides a process for preparing a composite cathode for a lithium ion cell. The process comprises the steps of (i) forming a cathode slurry in a planetary mixing machine by mixing an active material, conducting diluent and binder; (ii) coating the slurry over an aluminum foil substrate in a coating machine at a speed of 0.2-0.8 m/min; and (iii) calendering the cathode in a calendering machine at a temperature of 50-150 DEG C. The present invention also relates to a system for the process. The cathode has peel strength of greater than 200 gf/cm and moisture content less than 350 ppm. The lithium ion cell with the cathode disclosed in the invention and a graphite anode exhibits a capacity retention of &gt;80% at 100% depth-of-discharge at C/2-1C charge-discharge rate when tested for 2000 cycles. 本申请提供了一种制备用于锂离子电池的复合正极的方法,包括以下步骤:(i)通过混合活性材料、导电稀释剂和粘合剂,在行星式混合机中形成正极浆料;(ii)在涂覆机中以0.2-0.8m/min的速度将浆料涂覆在铝箔基板上;(iii)在50-150℃温度下在压延机中压延正极。本申请还公开了一种用于此目的的系统。正极具有大于200gf/cm的剥离强度和小于350ppm的水分含量。具有本发明公开的正极和石</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN113574711A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRICITY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title PROCESS FOR PREPARING COMPOSITE CATHODE FOR LITHIUM ION CELL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-13T13%3A37%3A16IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MERCY%20TD&rft.date=2021-10-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113574711A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true