Preparation method of macromonomer for polymer polyol

The invention relates to a preparation method of a macromonomer for polymer polyol. The method comprises the following steps: adding a compound containing unsaturated double bonds, a catalyst and water into a reaction kettle, replacing air in the reaction kettle with nitrogen, and carrying out a sti...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GUAN SONGYUN, ZHOU GUOXIANG, ZHU SHU, YANG YUQIANG, HAO JINGYING, LI YUSONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GUAN SONGYUN
ZHOU GUOXIANG
ZHU SHU
YANG YUQIANG
HAO JINGYING
LI YUSONG
description The invention relates to a preparation method of a macromonomer for polymer polyol. The method comprises the following steps: adding a compound containing unsaturated double bonds, a catalyst and water into a reaction kettle, replacing air in the reaction kettle with nitrogen, and carrying out a stirring reaction at 10-30 DEG C for 2-3 hours; adding polyether polyol into the kettle, and reacting for 3-5 hours under the conditions that the temperature is 50-60 DEG C and the pressure is 0.02-0.5 MPa; heating to 100-130 DEG C, reacting for 5-8 hours under the pressure of 0.02-0.5 MPa, and vacuumizing to remove for 2-3 hours; keeping the reaction temperature at 100-130 DEG C, adding ethylene oxide into the kettle under micro-positive pressure of the system, and reacting for 3-5 hours; raising the temperature to 140 to 170 DEG C and reacting for 5 to 6 hours under the pressure of 0.02 to 0.5 MPa; and after the reaction is finished, cooling to below 80 DEG C to obtain the macromonomer product for the polymer polyol
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113480725A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113480725A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113480725A3</originalsourceid><addsrcrecordid>eNrjZDANKEotSCxKLMnMz1PITS3JyE9RyE9TyE1MLsrPzc_Lz00tUkjLL1IoyM-pBLFBdH4ODwNrWmJOcSovlOZmUHRzDXH20E0tyI9PLS5ITE7NSy2Jd_YzNDQ2sTAwNzJ1NCZGDQCi_y2y</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of macromonomer for polymer polyol</title><source>esp@cenet</source><creator>GUAN SONGYUN ; ZHOU GUOXIANG ; ZHU SHU ; YANG YUQIANG ; HAO JINGYING ; LI YUSONG</creator><creatorcontrib>GUAN SONGYUN ; ZHOU GUOXIANG ; ZHU SHU ; YANG YUQIANG ; HAO JINGYING ; LI YUSONG</creatorcontrib><description>The invention relates to a preparation method of a macromonomer for polymer polyol. The method comprises the following steps: adding a compound containing unsaturated double bonds, a catalyst and water into a reaction kettle, replacing air in the reaction kettle with nitrogen, and carrying out a stirring reaction at 10-30 DEG C for 2-3 hours; adding polyether polyol into the kettle, and reacting for 3-5 hours under the conditions that the temperature is 50-60 DEG C and the pressure is 0.02-0.5 MPa; heating to 100-130 DEG C, reacting for 5-8 hours under the pressure of 0.02-0.5 MPa, and vacuumizing to remove for 2-3 hours; keeping the reaction temperature at 100-130 DEG C, adding ethylene oxide into the kettle under micro-positive pressure of the system, and reacting for 3-5 hours; raising the temperature to 140 to 170 DEG C and reacting for 5 to 6 hours under the pressure of 0.02 to 0.5 MPa; and after the reaction is finished, cooling to below 80 DEG C to obtain the macromonomer product for the polymer polyol</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211008&amp;DB=EPODOC&amp;CC=CN&amp;NR=113480725A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211008&amp;DB=EPODOC&amp;CC=CN&amp;NR=113480725A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GUAN SONGYUN</creatorcontrib><creatorcontrib>ZHOU GUOXIANG</creatorcontrib><creatorcontrib>ZHU SHU</creatorcontrib><creatorcontrib>YANG YUQIANG</creatorcontrib><creatorcontrib>HAO JINGYING</creatorcontrib><creatorcontrib>LI YUSONG</creatorcontrib><title>Preparation method of macromonomer for polymer polyol</title><description>The invention relates to a preparation method of a macromonomer for polymer polyol. The method comprises the following steps: adding a compound containing unsaturated double bonds, a catalyst and water into a reaction kettle, replacing air in the reaction kettle with nitrogen, and carrying out a stirring reaction at 10-30 DEG C for 2-3 hours; adding polyether polyol into the kettle, and reacting for 3-5 hours under the conditions that the temperature is 50-60 DEG C and the pressure is 0.02-0.5 MPa; heating to 100-130 DEG C, reacting for 5-8 hours under the pressure of 0.02-0.5 MPa, and vacuumizing to remove for 2-3 hours; keeping the reaction temperature at 100-130 DEG C, adding ethylene oxide into the kettle under micro-positive pressure of the system, and reacting for 3-5 hours; raising the temperature to 140 to 170 DEG C and reacting for 5 to 6 hours under the pressure of 0.02 to 0.5 MPa; and after the reaction is finished, cooling to below 80 DEG C to obtain the macromonomer product for the polymer polyol</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDANKEotSCxKLMnMz1PITS3JyE9RyE9TyE1MLsrPzc_Lz00tUkjLL1IoyM-pBLFBdH4ODwNrWmJOcSovlOZmUHRzDXH20E0tyI9PLS5ITE7NSy2Jd_YzNDQ2sTAwNzJ1NCZGDQCi_y2y</recordid><startdate>20211008</startdate><enddate>20211008</enddate><creator>GUAN SONGYUN</creator><creator>ZHOU GUOXIANG</creator><creator>ZHU SHU</creator><creator>YANG YUQIANG</creator><creator>HAO JINGYING</creator><creator>LI YUSONG</creator><scope>EVB</scope></search><sort><creationdate>20211008</creationdate><title>Preparation method of macromonomer for polymer polyol</title><author>GUAN SONGYUN ; ZHOU GUOXIANG ; ZHU SHU ; YANG YUQIANG ; HAO JINGYING ; LI YUSONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113480725A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>GUAN SONGYUN</creatorcontrib><creatorcontrib>ZHOU GUOXIANG</creatorcontrib><creatorcontrib>ZHU SHU</creatorcontrib><creatorcontrib>YANG YUQIANG</creatorcontrib><creatorcontrib>HAO JINGYING</creatorcontrib><creatorcontrib>LI YUSONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GUAN SONGYUN</au><au>ZHOU GUOXIANG</au><au>ZHU SHU</au><au>YANG YUQIANG</au><au>HAO JINGYING</au><au>LI YUSONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of macromonomer for polymer polyol</title><date>2021-10-08</date><risdate>2021</risdate><abstract>The invention relates to a preparation method of a macromonomer for polymer polyol. The method comprises the following steps: adding a compound containing unsaturated double bonds, a catalyst and water into a reaction kettle, replacing air in the reaction kettle with nitrogen, and carrying out a stirring reaction at 10-30 DEG C for 2-3 hours; adding polyether polyol into the kettle, and reacting for 3-5 hours under the conditions that the temperature is 50-60 DEG C and the pressure is 0.02-0.5 MPa; heating to 100-130 DEG C, reacting for 5-8 hours under the pressure of 0.02-0.5 MPa, and vacuumizing to remove for 2-3 hours; keeping the reaction temperature at 100-130 DEG C, adding ethylene oxide into the kettle under micro-positive pressure of the system, and reacting for 3-5 hours; raising the temperature to 140 to 170 DEG C and reacting for 5 to 6 hours under the pressure of 0.02 to 0.5 MPa; and after the reaction is finished, cooling to below 80 DEG C to obtain the macromonomer product for the polymer polyol</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN113480725A
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title Preparation method of macromonomer for polymer polyol
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T02%3A02%3A14IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GUAN%20SONGYUN&rft.date=2021-10-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113480725A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true