Concrete crack repairing method
The invention discloses a concrete crack repairing method. The concrete crack repairing method comprises the following steps of cleaning a crack: detecting the depth and width of the crack by using equipment, then cleaning the ground near the crack, and when an opening in the top of the crack is sma...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | HUANG HENGJIN QI DAN |
description | The invention discloses a concrete crack repairing method. The concrete crack repairing method comprises the following steps of cleaning a crack: detecting the depth and width of the crack by using equipment, then cleaning the ground near the crack, and when an opening in the top of the crack is smaller than 5mm, digging a groove with the width of 0.5-1cm along the crack, cleaning the inner wall of the crack by using a high-pressure water gun and a high-pressure air gun; preparing slurry: mixing and preparing a filling material according to a proportion, wherein the filling material is prepared from 50 to 55 parts of cement, 25 to 28 parts of fly ash, 10 to 12 parts of quartz sand, 2 to 5 parts of epoxy resin glue, 1 to 1.2 parts of redispersible latex powder, 0.5 to 1.5 parts of a water reducing agent and 0.2 to 0.6 part of a retarder; cement, fly ash, silica fume, epoxy resin glue, redispersible latex powder, the water reducing agent, the retarder and the like are used for preparing a high-viscosity filling |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113293797A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113293797A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113293797A3</originalsourceid><addsrcrecordid>eNrjZJB3zs9LLkotSVVILkpMzlYoSi1IzCzKzEtXyE0tychP4WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hobGRpbG5pbmjsbEqAEAJnok8w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Concrete crack repairing method</title><source>esp@cenet</source><creator>HUANG HENGJIN ; QI DAN</creator><creatorcontrib>HUANG HENGJIN ; QI DAN</creatorcontrib><description>The invention discloses a concrete crack repairing method. The concrete crack repairing method comprises the following steps of cleaning a crack: detecting the depth and width of the crack by using equipment, then cleaning the ground near the crack, and when an opening in the top of the crack is smaller than 5mm, digging a groove with the width of 0.5-1cm along the crack, cleaning the inner wall of the crack by using a high-pressure water gun and a high-pressure air gun; preparing slurry: mixing and preparing a filling material according to a proportion, wherein the filling material is prepared from 50 to 55 parts of cement, 25 to 28 parts of fly ash, 10 to 12 parts of quartz sand, 2 to 5 parts of epoxy resin glue, 1 to 1.2 parts of redispersible latex powder, 0.5 to 1.5 parts of a water reducing agent and 0.2 to 0.6 part of a retarder; cement, fly ash, silica fume, epoxy resin glue, redispersible latex powder, the water reducing agent, the retarder and the like are used for preparing a high-viscosity filling</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; EMBANKMENTS ; EXCAVATIONS ; FIXED CONSTRUCTIONS ; FOUNDATIONS ; HYDRAULIC ENGINEERING ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; SOIL SHIFTING ; TREATMENT OF NATURAL STONE ; UNDERGROUND OR UNDERWATER STRUCTURES</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20210824&DB=EPODOC&CC=CN&NR=113293797A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25551,76302</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20210824&DB=EPODOC&CC=CN&NR=113293797A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HUANG HENGJIN</creatorcontrib><creatorcontrib>QI DAN</creatorcontrib><title>Concrete crack repairing method</title><description>The invention discloses a concrete crack repairing method. The concrete crack repairing method comprises the following steps of cleaning a crack: detecting the depth and width of the crack by using equipment, then cleaning the ground near the crack, and when an opening in the top of the crack is smaller than 5mm, digging a groove with the width of 0.5-1cm along the crack, cleaning the inner wall of the crack by using a high-pressure water gun and a high-pressure air gun; preparing slurry: mixing and preparing a filling material according to a proportion, wherein the filling material is prepared from 50 to 55 parts of cement, 25 to 28 parts of fly ash, 10 to 12 parts of quartz sand, 2 to 5 parts of epoxy resin glue, 1 to 1.2 parts of redispersible latex powder, 0.5 to 1.5 parts of a water reducing agent and 0.2 to 0.6 part of a retarder; cement, fly ash, silica fume, epoxy resin glue, redispersible latex powder, the water reducing agent, the retarder and the like are used for preparing a high-viscosity filling</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>EMBANKMENTS</subject><subject>EXCAVATIONS</subject><subject>FIXED CONSTRUCTIONS</subject><subject>FOUNDATIONS</subject><subject>HYDRAULIC ENGINEERING</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>SOIL SHIFTING</subject><subject>TREATMENT OF NATURAL STONE</subject><subject>UNDERGROUND OR UNDERWATER STRUCTURES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJB3zs9LLkotSVVILkpMzlYoSi1IzCzKzEtXyE0tychP4WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hobGRpbG5pbmjsbEqAEAJnok8w</recordid><startdate>20210824</startdate><enddate>20210824</enddate><creator>HUANG HENGJIN</creator><creator>QI DAN</creator><scope>EVB</scope></search><sort><creationdate>20210824</creationdate><title>Concrete crack repairing method</title><author>HUANG HENGJIN ; QI DAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113293797A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>EMBANKMENTS</topic><topic>EXCAVATIONS</topic><topic>FIXED CONSTRUCTIONS</topic><topic>FOUNDATIONS</topic><topic>HYDRAULIC ENGINEERING</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>SOIL SHIFTING</topic><topic>TREATMENT OF NATURAL STONE</topic><topic>UNDERGROUND OR UNDERWATER STRUCTURES</topic><toplevel>online_resources</toplevel><creatorcontrib>HUANG HENGJIN</creatorcontrib><creatorcontrib>QI DAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HUANG HENGJIN</au><au>QI DAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Concrete crack repairing method</title><date>2021-08-24</date><risdate>2021</risdate><abstract>The invention discloses a concrete crack repairing method. The concrete crack repairing method comprises the following steps of cleaning a crack: detecting the depth and width of the crack by using equipment, then cleaning the ground near the crack, and when an opening in the top of the crack is smaller than 5mm, digging a groove with the width of 0.5-1cm along the crack, cleaning the inner wall of the crack by using a high-pressure water gun and a high-pressure air gun; preparing slurry: mixing and preparing a filling material according to a proportion, wherein the filling material is prepared from 50 to 55 parts of cement, 25 to 28 parts of fly ash, 10 to 12 parts of quartz sand, 2 to 5 parts of epoxy resin glue, 1 to 1.2 parts of redispersible latex powder, 0.5 to 1.5 parts of a water reducing agent and 0.2 to 0.6 part of a retarder; cement, fly ash, silica fume, epoxy resin glue, redispersible latex powder, the water reducing agent, the retarder and the like are used for preparing a high-viscosity filling</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN113293797A |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE EMBANKMENTS EXCAVATIONS FIXED CONSTRUCTIONS FOUNDATIONS HYDRAULIC ENGINEERING LIME, MAGNESIA METALLURGY REFRACTORIES SLAG SOIL SHIFTING TREATMENT OF NATURAL STONE UNDERGROUND OR UNDERWATER STRUCTURES |
title | Concrete crack repairing method |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-16T05%3A45%3A53IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HUANG%20HENGJIN&rft.date=2021-08-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113293797A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |