Method for preparing Al2O3-SiC composite ceramic from coal slime

The coal slime is adopted as the raw material, the coal slime raw material is smashed through the ball mill, then the quartz sand is added for mixing, then dry pressing forming is conducted, sintering is conducted in the argon atmosphere, the Al2O3-SiC composite ceramic is obtained, the purpose of p...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HUANG RUI, HE TIANYING, BAI JIANGUANG, HUANG CHUANQING, LIANG LIDONG, WANG RUNXING, CHAI DELIANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HUANG RUI
HE TIANYING
BAI JIANGUANG
HUANG CHUANQING
LIANG LIDONG
WANG RUNXING
CHAI DELIANG
description The coal slime is adopted as the raw material, the coal slime raw material is smashed through the ball mill, then the quartz sand is added for mixing, then dry pressing forming is conducted, sintering is conducted in the argon atmosphere, the Al2O3-SiC composite ceramic is obtained, the purpose of preparing high-technology ceramic through the coal slime is achieved, the high-technology-content additional value of the coal slime is effectively improved, and the process is simple. The prepared composite ceramic has high strength, and the harm of the coal slime to the environment is reduced. 本发明采用煤泥作为原料,利用球磨机将煤泥原料进行粉碎后添加石英砂进行混料,随后干压成型氩气气氛下烧结得到Al2O3-SiC复相陶瓷,实现了利用煤泥制备高技术陶瓷目的,有效提升了煤泥高技术含量附加值,工艺简单,制备得到的复相陶瓷具有较高强度,减少了煤泥对环境危害。
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113233879A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113233879A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113233879A3</originalsourceid><addsrcrecordid>eNrjZHDwTS3JyE9RSMsvUigoSi1ILMrMS1dwzDHyN9YNznRWSM7PLcgvzixJVUhOLUrMzUxWSCvKzwUKJ-YoFOdk5qbyMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DQ2MjY2MLc0tHY2LUAABGLzBC</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing Al2O3-SiC composite ceramic from coal slime</title><source>esp@cenet</source><creator>HUANG RUI ; HE TIANYING ; BAI JIANGUANG ; HUANG CHUANQING ; LIANG LIDONG ; WANG RUNXING ; CHAI DELIANG</creator><creatorcontrib>HUANG RUI ; HE TIANYING ; BAI JIANGUANG ; HUANG CHUANQING ; LIANG LIDONG ; WANG RUNXING ; CHAI DELIANG</creatorcontrib><description>The coal slime is adopted as the raw material, the coal slime raw material is smashed through the ball mill, then the quartz sand is added for mixing, then dry pressing forming is conducted, sintering is conducted in the argon atmosphere, the Al2O3-SiC composite ceramic is obtained, the purpose of preparing high-technology ceramic through the coal slime is achieved, the high-technology-content additional value of the coal slime is effectively improved, and the process is simple. The prepared composite ceramic has high strength, and the harm of the coal slime to the environment is reduced. 本发明采用煤泥作为原料,利用球磨机将煤泥原料进行粉碎后添加石英砂进行混料,随后干压成型氩气气氛下烧结得到Al2O3-SiC复相陶瓷,实现了利用煤泥制备高技术陶瓷目的,有效提升了煤泥高技术含量附加值,工艺简单,制备得到的复相陶瓷具有较高强度,减少了煤泥对环境危害。</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210810&amp;DB=EPODOC&amp;CC=CN&amp;NR=113233879A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25544,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210810&amp;DB=EPODOC&amp;CC=CN&amp;NR=113233879A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HUANG RUI</creatorcontrib><creatorcontrib>HE TIANYING</creatorcontrib><creatorcontrib>BAI JIANGUANG</creatorcontrib><creatorcontrib>HUANG CHUANQING</creatorcontrib><creatorcontrib>LIANG LIDONG</creatorcontrib><creatorcontrib>WANG RUNXING</creatorcontrib><creatorcontrib>CHAI DELIANG</creatorcontrib><title>Method for preparing Al2O3-SiC composite ceramic from coal slime</title><description>The coal slime is adopted as the raw material, the coal slime raw material is smashed through the ball mill, then the quartz sand is added for mixing, then dry pressing forming is conducted, sintering is conducted in the argon atmosphere, the Al2O3-SiC composite ceramic is obtained, the purpose of preparing high-technology ceramic through the coal slime is achieved, the high-technology-content additional value of the coal slime is effectively improved, and the process is simple. The prepared composite ceramic has high strength, and the harm of the coal slime to the environment is reduced. 本发明采用煤泥作为原料,利用球磨机将煤泥原料进行粉碎后添加石英砂进行混料,随后干压成型氩气气氛下烧结得到Al2O3-SiC复相陶瓷,实现了利用煤泥制备高技术陶瓷目的,有效提升了煤泥高技术含量附加值,工艺简单,制备得到的复相陶瓷具有较高强度,减少了煤泥对环境危害。</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHDwTS3JyE9RSMsvUigoSi1ILMrMS1dwzDHyN9YNznRWSM7PLcgvzixJVUhOLUrMzUxWSCvKzwUKJ-YoFOdk5qbyMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DQ2MjY2MLc0tHY2LUAABGLzBC</recordid><startdate>20210810</startdate><enddate>20210810</enddate><creator>HUANG RUI</creator><creator>HE TIANYING</creator><creator>BAI JIANGUANG</creator><creator>HUANG CHUANQING</creator><creator>LIANG LIDONG</creator><creator>WANG RUNXING</creator><creator>CHAI DELIANG</creator><scope>EVB</scope></search><sort><creationdate>20210810</creationdate><title>Method for preparing Al2O3-SiC composite ceramic from coal slime</title><author>HUANG RUI ; HE TIANYING ; BAI JIANGUANG ; HUANG CHUANQING ; LIANG LIDONG ; WANG RUNXING ; CHAI DELIANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113233879A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>HUANG RUI</creatorcontrib><creatorcontrib>HE TIANYING</creatorcontrib><creatorcontrib>BAI JIANGUANG</creatorcontrib><creatorcontrib>HUANG CHUANQING</creatorcontrib><creatorcontrib>LIANG LIDONG</creatorcontrib><creatorcontrib>WANG RUNXING</creatorcontrib><creatorcontrib>CHAI DELIANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HUANG RUI</au><au>HE TIANYING</au><au>BAI JIANGUANG</au><au>HUANG CHUANQING</au><au>LIANG LIDONG</au><au>WANG RUNXING</au><au>CHAI DELIANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing Al2O3-SiC composite ceramic from coal slime</title><date>2021-08-10</date><risdate>2021</risdate><abstract>The coal slime is adopted as the raw material, the coal slime raw material is smashed through the ball mill, then the quartz sand is added for mixing, then dry pressing forming is conducted, sintering is conducted in the argon atmosphere, the Al2O3-SiC composite ceramic is obtained, the purpose of preparing high-technology ceramic through the coal slime is achieved, the high-technology-content additional value of the coal slime is effectively improved, and the process is simple. The prepared composite ceramic has high strength, and the harm of the coal slime to the environment is reduced. 本发明采用煤泥作为原料,利用球磨机将煤泥原料进行粉碎后添加石英砂进行混料,随后干压成型氩气气氛下烧结得到Al2O3-SiC复相陶瓷,实现了利用煤泥制备高技术陶瓷目的,有效提升了煤泥高技术含量附加值,工艺简单,制备得到的复相陶瓷具有较高强度,减少了煤泥对环境危害。</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN113233879A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Method for preparing Al2O3-SiC composite ceramic from coal slime
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-27T17%3A09%3A46IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HUANG%20RUI&rft.date=2021-08-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113233879A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true