Preparation method of anti-pollution membrane

The invention discloses a preparation method of an anti-pollution membrane. The preparation method comprises the following steps: (1) preparing an NPC-Ag composite material; and (2) blending the NPC-Ag composite material into a membrane material to form the anti-pollution membrane. The NPC-Ag is ble...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU JIN, ZHANG MANYING, HUAI YANJIN, WU JUAN, WANG YUJIE, GAO YONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIU JIN
ZHANG MANYING
HUAI YANJIN
WU JUAN
WANG YUJIE
GAO YONG
description The invention discloses a preparation method of an anti-pollution membrane. The preparation method comprises the following steps: (1) preparing an NPC-Ag composite material; and (2) blending the NPC-Ag composite material into a membrane material to form the anti-pollution membrane. The NPC-Ag is blended into the membrane material, so that the binding force of nano Ag in the membrane material can be improved, the nano Ag is prevented from falling off, meanwhile, the Ag can be uniformly distributed on the surface of the membrane material by using the NPC, the agglomeration phenomenon is prevented, and the anti-pollution performance of the membrane material is improved. According to the manufacturing method of the NPC-Ag mixture, Ag and NPC can be mixed more uniformly, meanwhile, Ag can be efficiently and stably reduced towards Ag through irradiation of a high-pressure mercury lamp, and particle size growth in the reduction process is effectively controlled. According to the preparation method disclosed by th
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113069940A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113069940A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113069940A3</originalsourceid><addsrcrecordid>eNrjZNANKEotSCxKLMnMz1PITS3JyE9RyE9TSMwrydQtyM_JKYVK5CYVJeal8jCwpiXmFKfyQmluBkU31xBnD93Ugvz41OKCxOTUvNSSeGc_Q0NjAzNLSxMDR2Ni1AAA6AQqdw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of anti-pollution membrane</title><source>esp@cenet</source><creator>LIU JIN ; ZHANG MANYING ; HUAI YANJIN ; WU JUAN ; WANG YUJIE ; GAO YONG</creator><creatorcontrib>LIU JIN ; ZHANG MANYING ; HUAI YANJIN ; WU JUAN ; WANG YUJIE ; GAO YONG</creatorcontrib><description>The invention discloses a preparation method of an anti-pollution membrane. The preparation method comprises the following steps: (1) preparing an NPC-Ag composite material; and (2) blending the NPC-Ag composite material into a membrane material to form the anti-pollution membrane. The NPC-Ag is blended into the membrane material, so that the binding force of nano Ag in the membrane material can be improved, the nano Ag is prevented from falling off, meanwhile, the Ag can be uniformly distributed on the surface of the membrane material by using the NPC, the agglomeration phenomenon is prevented, and the anti-pollution performance of the membrane material is improved. According to the manufacturing method of the NPC-Ag mixture, Ag and NPC can be mixed more uniformly, meanwhile, Ag&lt;+&gt; can be efficiently and stably reduced towards Ag through irradiation of a high-pressure mercury lamp, and particle size growth in the reduction process is effectively controlled. According to the preparation method disclosed by th</description><language>chi ; eng</language><subject>CHEMISTRY ; METALLURGY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; SEPARATION ; TRANSPORTING ; TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210706&amp;DB=EPODOC&amp;CC=CN&amp;NR=113069940A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210706&amp;DB=EPODOC&amp;CC=CN&amp;NR=113069940A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU JIN</creatorcontrib><creatorcontrib>ZHANG MANYING</creatorcontrib><creatorcontrib>HUAI YANJIN</creatorcontrib><creatorcontrib>WU JUAN</creatorcontrib><creatorcontrib>WANG YUJIE</creatorcontrib><creatorcontrib>GAO YONG</creatorcontrib><title>Preparation method of anti-pollution membrane</title><description>The invention discloses a preparation method of an anti-pollution membrane. The preparation method comprises the following steps: (1) preparing an NPC-Ag composite material; and (2) blending the NPC-Ag composite material into a membrane material to form the anti-pollution membrane. The NPC-Ag is blended into the membrane material, so that the binding force of nano Ag in the membrane material can be improved, the nano Ag is prevented from falling off, meanwhile, the Ag can be uniformly distributed on the surface of the membrane material by using the NPC, the agglomeration phenomenon is prevented, and the anti-pollution performance of the membrane material is improved. According to the manufacturing method of the NPC-Ag mixture, Ag and NPC can be mixed more uniformly, meanwhile, Ag&lt;+&gt; can be efficiently and stably reduced towards Ag through irradiation of a high-pressure mercury lamp, and particle size growth in the reduction process is effectively controlled. According to the preparation method disclosed by th</description><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>SEPARATION</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNANKEotSCxKLMnMz1PITS3JyE9RyE9TSMwrydQtyM_JKYVK5CYVJeal8jCwpiXmFKfyQmluBkU31xBnD93Ugvz41OKCxOTUvNSSeGc_Q0NjAzNLSxMDR2Ni1AAA6AQqdw</recordid><startdate>20210706</startdate><enddate>20210706</enddate><creator>LIU JIN</creator><creator>ZHANG MANYING</creator><creator>HUAI YANJIN</creator><creator>WU JUAN</creator><creator>WANG YUJIE</creator><creator>GAO YONG</creator><scope>EVB</scope></search><sort><creationdate>20210706</creationdate><title>Preparation method of anti-pollution membrane</title><author>LIU JIN ; ZHANG MANYING ; HUAI YANJIN ; WU JUAN ; WANG YUJIE ; GAO YONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113069940A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>SEPARATION</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU JIN</creatorcontrib><creatorcontrib>ZHANG MANYING</creatorcontrib><creatorcontrib>HUAI YANJIN</creatorcontrib><creatorcontrib>WU JUAN</creatorcontrib><creatorcontrib>WANG YUJIE</creatorcontrib><creatorcontrib>GAO YONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU JIN</au><au>ZHANG MANYING</au><au>HUAI YANJIN</au><au>WU JUAN</au><au>WANG YUJIE</au><au>GAO YONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of anti-pollution membrane</title><date>2021-07-06</date><risdate>2021</risdate><abstract>The invention discloses a preparation method of an anti-pollution membrane. The preparation method comprises the following steps: (1) preparing an NPC-Ag composite material; and (2) blending the NPC-Ag composite material into a membrane material to form the anti-pollution membrane. The NPC-Ag is blended into the membrane material, so that the binding force of nano Ag in the membrane material can be improved, the nano Ag is prevented from falling off, meanwhile, the Ag can be uniformly distributed on the surface of the membrane material by using the NPC, the agglomeration phenomenon is prevented, and the anti-pollution performance of the membrane material is improved. According to the manufacturing method of the NPC-Ag mixture, Ag and NPC can be mixed more uniformly, meanwhile, Ag&lt;+&gt; can be efficiently and stably reduced towards Ag through irradiation of a high-pressure mercury lamp, and particle size growth in the reduction process is effectively controlled. According to the preparation method disclosed by th</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN113069940A
source esp@cenet
subjects CHEMISTRY
METALLURGY
PERFORMING OPERATIONS
PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
SEPARATION
TRANSPORTING
TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE
title Preparation method of anti-pollution membrane
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-20T17%3A11%3A46IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20JIN&rft.date=2021-07-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113069940A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true