High-strength high-temperature-resistant ethylene propylene diene monomer

The high-strength high-temperature-resistant ethylene propylene diene monomer is prepared from the following raw materials in parts by weight: 90-110 parts of ethylene propylene diene monomer, 8-11 parts of liquid ethylene propylene diene monomer, 55-65 parts of carbon black, 12-18 parts of paraffin...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: XI XIANGHUI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The high-strength high-temperature-resistant ethylene propylene diene monomer is prepared from the following raw materials in parts by weight: 90-110 parts of ethylene propylene diene monomer, 8-11 parts of liquid ethylene propylene diene monomer, 55-65 parts of carbon black, 12-18 parts of paraffin oil, 0.5-3 part of an anti-aging agent, 4.5-5.5 parts of zinc oxide, 0.8-1 part of stearic acid and 5.5-6 parts of a cross-linking agent. 一种高强度耐高温三元乙丙橡胶,包括以下重量份数的原料:三元乙丙橡胶90-110份、液体三元乙丙8-11份、碳黑55-65份,石蜡油12-18份、防老剂0.5-3份、氧化锌4.5-5.5份,硬脂酸0.8-1份,交联剂5.5-6份。