Friction material and preparation method thereof

The invention relates to a friction material and a preparation method thereof. The invention aims to provide a friction material and a preparation method thereof. A large amount of waste generated in the industry is effectively utilized, the aims of protecting the environment and protecting the body...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SI WANBAO, NIE DONGBIN, XU NANHAN, YANG PAN, ZHANG SULIAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SI WANBAO
NIE DONGBIN
XU NANHAN
YANG PAN
ZHANG SULIAN
description The invention relates to a friction material and a preparation method thereof. The invention aims to provide a friction material and a preparation method thereof. A large amount of waste generated in the industry is effectively utilized, the aims of protecting the environment and protecting the body health of people are achieved, the product quality is ensured, and the production efficiency and the automation rate are improved. According to the technical scheme, the friction material comprises the following components in parts by weight: 1) 5-25 parts of reinforced fibers, 10-40 parts of an adhesive, 0.5-8 part of a curing aid, 15-30 parts of a surface-modified friction performance regulator and 20-60 parts of surface-modified recycled waste. The surface-modified recycled waste is obtained by modifying the surfaces of recycled waste particles by adopting a powder coupling agent; and the weight ratio of the powder coupling agent is 0.5-2% of that of the recycled waste particles. The preparation method of the s
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN112694767A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN112694767A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN112694767A3</originalsourceid><addsrcrecordid>eNrjZDBwK8pMLsnMz1PITSxJLcpMzFFIzEtRKChKLUgsSoRIpJZk5KcolGSkFqXmp_EwsKYl5hSn8kJpbgZFN9cQZw_d1IL8-NTigsTk1LzUknhnP0NDIzNLE3Mzc0djYtQAAH1sK6A</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Friction material and preparation method thereof</title><source>esp@cenet</source><creator>SI WANBAO ; NIE DONGBIN ; XU NANHAN ; YANG PAN ; ZHANG SULIAN</creator><creatorcontrib>SI WANBAO ; NIE DONGBIN ; XU NANHAN ; YANG PAN ; ZHANG SULIAN</creatorcontrib><description>The invention relates to a friction material and a preparation method thereof. The invention aims to provide a friction material and a preparation method thereof. A large amount of waste generated in the industry is effectively utilized, the aims of protecting the environment and protecting the body health of people are achieved, the product quality is ensured, and the production efficiency and the automation rate are improved. According to the technical scheme, the friction material comprises the following components in parts by weight: 1) 5-25 parts of reinforced fibers, 10-40 parts of an adhesive, 0.5-8 part of a curing aid, 15-30 parts of a surface-modified friction performance regulator and 20-60 parts of surface-modified recycled waste. The surface-modified recycled waste is obtained by modifying the surfaces of recycled waste particles by adopting a powder coupling agent; and the weight ratio of the powder coupling agent is 0.5-2% of that of the recycled waste particles. The preparation method of the s</description><language>chi ; eng</language><subject>ADHESIVES ; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; DYES ; GENERAL PROCESSES OF COMPOUNDING ; MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; ORGANIC MACROMOLECULAR COMPOUNDS ; PAINTS ; POLISHES ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS ; WORKING-UP</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210423&amp;DB=EPODOC&amp;CC=CN&amp;NR=112694767A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210423&amp;DB=EPODOC&amp;CC=CN&amp;NR=112694767A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SI WANBAO</creatorcontrib><creatorcontrib>NIE DONGBIN</creatorcontrib><creatorcontrib>XU NANHAN</creatorcontrib><creatorcontrib>YANG PAN</creatorcontrib><creatorcontrib>ZHANG SULIAN</creatorcontrib><title>Friction material and preparation method thereof</title><description>The invention relates to a friction material and a preparation method thereof. The invention aims to provide a friction material and a preparation method thereof. A large amount of waste generated in the industry is effectively utilized, the aims of protecting the environment and protecting the body health of people are achieved, the product quality is ensured, and the production efficiency and the automation rate are improved. According to the technical scheme, the friction material comprises the following components in parts by weight: 1) 5-25 parts of reinforced fibers, 10-40 parts of an adhesive, 0.5-8 part of a curing aid, 15-30 parts of a surface-modified friction performance regulator and 20-60 parts of surface-modified recycled waste. The surface-modified recycled waste is obtained by modifying the surfaces of recycled waste particles by adopting a powder coupling agent; and the weight ratio of the powder coupling agent is 0.5-2% of that of the recycled waste particles. The preparation method of the s</description><subject>ADHESIVES</subject><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>DYES</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDBwK8pMLsnMz1PITSxJLcpMzFFIzEtRKChKLUgsSoRIpJZk5KcolGSkFqXmp_EwsKYl5hSn8kJpbgZFN9cQZw_d1IL8-NTigsTk1LzUknhnP0NDIzNLE3Mzc0djYtQAAH1sK6A</recordid><startdate>20210423</startdate><enddate>20210423</enddate><creator>SI WANBAO</creator><creator>NIE DONGBIN</creator><creator>XU NANHAN</creator><creator>YANG PAN</creator><creator>ZHANG SULIAN</creator><scope>EVB</scope></search><sort><creationdate>20210423</creationdate><title>Friction material and preparation method thereof</title><author>SI WANBAO ; NIE DONGBIN ; XU NANHAN ; YANG PAN ; ZHANG SULIAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN112694767A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>ADHESIVES</topic><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>DYES</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>SI WANBAO</creatorcontrib><creatorcontrib>NIE DONGBIN</creatorcontrib><creatorcontrib>XU NANHAN</creatorcontrib><creatorcontrib>YANG PAN</creatorcontrib><creatorcontrib>ZHANG SULIAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SI WANBAO</au><au>NIE DONGBIN</au><au>XU NANHAN</au><au>YANG PAN</au><au>ZHANG SULIAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Friction material and preparation method thereof</title><date>2021-04-23</date><risdate>2021</risdate><abstract>The invention relates to a friction material and a preparation method thereof. The invention aims to provide a friction material and a preparation method thereof. A large amount of waste generated in the industry is effectively utilized, the aims of protecting the environment and protecting the body health of people are achieved, the product quality is ensured, and the production efficiency and the automation rate are improved. According to the technical scheme, the friction material comprises the following components in parts by weight: 1) 5-25 parts of reinforced fibers, 10-40 parts of an adhesive, 0.5-8 part of a curing aid, 15-30 parts of a surface-modified friction performance regulator and 20-60 parts of surface-modified recycled waste. The surface-modified recycled waste is obtained by modifying the surfaces of recycled waste particles by adopting a powder coupling agent; and the weight ratio of the powder coupling agent is 0.5-2% of that of the recycled waste particles. The preparation method of the s</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN112694767A
source esp@cenet
subjects ADHESIVES
AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
DYES
GENERAL PROCESSES OF COMPOUNDING
MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
ORGANIC MACROMOLECULAR COMPOUNDS
PAINTS
POLISHES
THEIR PREPARATION OR CHEMICAL WORKING-UP
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS
WORKING-UP
title Friction material and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-31T05%3A42%3A51IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SI%20WANBAO&rft.date=2021-04-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN112694767A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true