Immiscible metal molybdenum and copper diffusion bonding method adopting consumable intermediate layer
The invention discloses an immiscible metal molybdenum and copper diffusion bonding method adopting a consumable intermediate layer, which comprises the following steps: S1, pretreatment of molybdenum and copper base materials: carrying out mechanical or chemical treatment on to-be-welded surfaces o...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | LUAN BOYU LUO JIANYI WANG HONG DENG YONGQIANG GAN SHUDE GAN LINQIAO GAO HUANFANG |
description | The invention discloses an immiscible metal molybdenum and copper diffusion bonding method adopting a consumable intermediate layer, which comprises the following steps: S1, pretreatment of molybdenum and copper base materials: carrying out mechanical or chemical treatment on to-be-welded surfaces of the molybdenum and copper base materials to remove surface oil stains and oxide layers of the to-be-welded surfaces of the base materials so as to meet the requirements of a bonding process; S2, preparing a titanium intermediate layer between the to-be-welded surfaces of the molybdenum and copper base materials; and S3, performing diffusion bonding on the titanium middle layer and the base materials on the two sides, specifically, the assembled molybdenum-titanium middle layer-copper combined component is put into a vacuum furnace, certain pressure is applied to molybdenum or copper according to the technological requirements, heat preservation is conducted for a certain time at the temperature required by the te |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN112605518A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN112605518A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN112605518A3</originalsourceid><addsrcrecordid>eNqNjDEKwkAQANNYiPqH9QGCUSK2EhRtrOzD5nZPD253j9ylyO8l4AOshoFhlpV_iITsQh8ZhAtGEItTT6yjACqBs5R4AArejzmYQm9KQd9z_TECJEtldmeaR8F5FLTwIEwBC0PEiYd1tfAYM29-XFXb2_XV3necrOOc0LFy6dpnXR9O-6apz5fjP80X4exAcA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Immiscible metal molybdenum and copper diffusion bonding method adopting consumable intermediate layer</title><source>esp@cenet</source><creator>LUAN BOYU ; LUO JIANYI ; WANG HONG ; DENG YONGQIANG ; GAN SHUDE ; GAN LINQIAO ; GAO HUANFANG</creator><creatorcontrib>LUAN BOYU ; LUO JIANYI ; WANG HONG ; DENG YONGQIANG ; GAN SHUDE ; GAN LINQIAO ; GAO HUANFANG</creatorcontrib><description>The invention discloses an immiscible metal molybdenum and copper diffusion bonding method adopting a consumable intermediate layer, which comprises the following steps: S1, pretreatment of molybdenum and copper base materials: carrying out mechanical or chemical treatment on to-be-welded surfaces of the molybdenum and copper base materials to remove surface oil stains and oxide layers of the to-be-welded surfaces of the base materials so as to meet the requirements of a bonding process; S2, preparing a titanium intermediate layer between the to-be-welded surfaces of the molybdenum and copper base materials; and S3, performing diffusion bonding on the titanium middle layer and the base materials on the two sides, specifically, the assembled molybdenum-titanium middle layer-copper combined component is put into a vacuum furnace, certain pressure is applied to molybdenum or copper according to the technological requirements, heat preservation is conducted for a certain time at the temperature required by the te</description><language>chi ; eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20210406&DB=EPODOC&CC=CN&NR=112605518A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20210406&DB=EPODOC&CC=CN&NR=112605518A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LUAN BOYU</creatorcontrib><creatorcontrib>LUO JIANYI</creatorcontrib><creatorcontrib>WANG HONG</creatorcontrib><creatorcontrib>DENG YONGQIANG</creatorcontrib><creatorcontrib>GAN SHUDE</creatorcontrib><creatorcontrib>GAN LINQIAO</creatorcontrib><creatorcontrib>GAO HUANFANG</creatorcontrib><title>Immiscible metal molybdenum and copper diffusion bonding method adopting consumable intermediate layer</title><description>The invention discloses an immiscible metal molybdenum and copper diffusion bonding method adopting a consumable intermediate layer, which comprises the following steps: S1, pretreatment of molybdenum and copper base materials: carrying out mechanical or chemical treatment on to-be-welded surfaces of the molybdenum and copper base materials to remove surface oil stains and oxide layers of the to-be-welded surfaces of the base materials so as to meet the requirements of a bonding process; S2, preparing a titanium intermediate layer between the to-be-welded surfaces of the molybdenum and copper base materials; and S3, performing diffusion bonding on the titanium middle layer and the base materials on the two sides, specifically, the assembled molybdenum-titanium middle layer-copper combined component is put into a vacuum furnace, certain pressure is applied to molybdenum or copper according to the technological requirements, heat preservation is conducted for a certain time at the temperature required by the te</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjDEKwkAQANNYiPqH9QGCUSK2EhRtrOzD5nZPD253j9ylyO8l4AOshoFhlpV_iITsQh8ZhAtGEItTT6yjACqBs5R4AArejzmYQm9KQd9z_TECJEtldmeaR8F5FLTwIEwBC0PEiYd1tfAYM29-XFXb2_XV3necrOOc0LFy6dpnXR9O-6apz5fjP80X4exAcA</recordid><startdate>20210406</startdate><enddate>20210406</enddate><creator>LUAN BOYU</creator><creator>LUO JIANYI</creator><creator>WANG HONG</creator><creator>DENG YONGQIANG</creator><creator>GAN SHUDE</creator><creator>GAN LINQIAO</creator><creator>GAO HUANFANG</creator><scope>EVB</scope></search><sort><creationdate>20210406</creationdate><title>Immiscible metal molybdenum and copper diffusion bonding method adopting consumable intermediate layer</title><author>LUAN BOYU ; LUO JIANYI ; WANG HONG ; DENG YONGQIANG ; GAN SHUDE ; GAN LINQIAO ; GAO HUANFANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN112605518A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>LUAN BOYU</creatorcontrib><creatorcontrib>LUO JIANYI</creatorcontrib><creatorcontrib>WANG HONG</creatorcontrib><creatorcontrib>DENG YONGQIANG</creatorcontrib><creatorcontrib>GAN SHUDE</creatorcontrib><creatorcontrib>GAN LINQIAO</creatorcontrib><creatorcontrib>GAO HUANFANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LUAN BOYU</au><au>LUO JIANYI</au><au>WANG HONG</au><au>DENG YONGQIANG</au><au>GAN SHUDE</au><au>GAN LINQIAO</au><au>GAO HUANFANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Immiscible metal molybdenum and copper diffusion bonding method adopting consumable intermediate layer</title><date>2021-04-06</date><risdate>2021</risdate><abstract>The invention discloses an immiscible metal molybdenum and copper diffusion bonding method adopting a consumable intermediate layer, which comprises the following steps: S1, pretreatment of molybdenum and copper base materials: carrying out mechanical or chemical treatment on to-be-welded surfaces of the molybdenum and copper base materials to remove surface oil stains and oxide layers of the to-be-welded surfaces of the base materials so as to meet the requirements of a bonding process; S2, preparing a titanium intermediate layer between the to-be-welded surfaces of the molybdenum and copper base materials; and S3, performing diffusion bonding on the titanium middle layer and the base materials on the two sides, specifically, the assembled molybdenum-titanium middle layer-copper combined component is put into a vacuum furnace, certain pressure is applied to molybdenum or copper according to the technological requirements, heat preservation is conducted for a certain time at the temperature required by the te</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN112605518A |
source | esp@cenet |
subjects | CLADDING OR PLATING BY SOLDERING OR WELDING CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING MACHINE TOOLS METAL-WORKING NOT OTHERWISE PROVIDED FOR PERFORMING OPERATIONS SOLDERING OR UNSOLDERING TRANSPORTING WELDING WORKING BY LASER BEAM |
title | Immiscible metal molybdenum and copper diffusion bonding method adopting consumable intermediate layer |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T01%3A57%3A37IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LUAN%20BOYU&rft.date=2021-04-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN112605518A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |