Quenching and tempering method for splines of bimetal cylinder bodies of hydraulic plunger pump and motor
The invention discloses a quenching and tempering method for splines of bimetal cylinder bodies of a hydraulic plunger pump and motor, and belongs to the technical field of machining. Residual heat isutilized to carry out hardening and tempering heat treatment in a bimetal casting process. Spline ha...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | YANG CHAOLIANG ZHOU WEI ZHOU BANGHUA |
description | The invention discloses a quenching and tempering method for splines of bimetal cylinder bodies of a hydraulic plunger pump and motor, and belongs to the technical field of machining. Residual heat isutilized to carry out hardening and tempering heat treatment in a bimetal casting process. Spline hardening and tempering are carried out in a cooling process. The method comprises the following specific operation steps that after heat preservation treatment of bimetal cylinder bodies, heated and molten according to a casting technology, of the hydraulic plunger pump and motor is finished, a steel base body and a molten copper alloy are conveyed to a cooling area device, and when the temperature is reduced to 840-880 DEG C, a hardening and tempering medium and compressed air are introduced into spline parts at the same time for cooling and hardening and tempering, wherein the hardening and tempering time is 5-10 min; the spline parts are conveyed to a designated position for air-cooling to normal temperature and |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN112593061A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN112593061A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN112593061A3</originalsourceid><addsrcrecordid>eNqNjMsKwjAQRbNxIeo_jB8gWItCl1IUV4LgvqTJpA0kmSGPRf_e-vgAV5d7zuUuhX0UDGq0YQAZNGT0jPHdPOaRNBiKkNjZgAnIQG9nLh2oaUYaI_Sk7VeNk46yOKuAXQnD7Lh4_rx6yhTXYmGkS7j55Upsr5dne9shU4eJpcKAuWvvVXU4NvX-VJ3rfzYvXMtAzg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Quenching and tempering method for splines of bimetal cylinder bodies of hydraulic plunger pump and motor</title><source>esp@cenet</source><creator>YANG CHAOLIANG ; ZHOU WEI ; ZHOU BANGHUA</creator><creatorcontrib>YANG CHAOLIANG ; ZHOU WEI ; ZHOU BANGHUA</creatorcontrib><description>The invention discloses a quenching and tempering method for splines of bimetal cylinder bodies of a hydraulic plunger pump and motor, and belongs to the technical field of machining. Residual heat isutilized to carry out hardening and tempering heat treatment in a bimetal casting process. Spline hardening and tempering are carried out in a cooling process. The method comprises the following specific operation steps that after heat preservation treatment of bimetal cylinder bodies, heated and molten according to a casting technology, of the hydraulic plunger pump and motor is finished, a steel base body and a molten copper alloy are conveyed to a cooling area device, and when the temperature is reduced to 840-880 DEG C, a hardening and tempering medium and compressed air are introduced into spline parts at the same time for cooling and hardening and tempering, wherein the hardening and tempering time is 5-10 min; the spline parts are conveyed to a designated position for air-cooling to normal temperature and</description><language>chi ; eng</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; CHEMISTRY ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20210402&DB=EPODOC&CC=CN&NR=112593061A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20210402&DB=EPODOC&CC=CN&NR=112593061A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YANG CHAOLIANG</creatorcontrib><creatorcontrib>ZHOU WEI</creatorcontrib><creatorcontrib>ZHOU BANGHUA</creatorcontrib><title>Quenching and tempering method for splines of bimetal cylinder bodies of hydraulic plunger pump and motor</title><description>The invention discloses a quenching and tempering method for splines of bimetal cylinder bodies of a hydraulic plunger pump and motor, and belongs to the technical field of machining. Residual heat isutilized to carry out hardening and tempering heat treatment in a bimetal casting process. Spline hardening and tempering are carried out in a cooling process. The method comprises the following specific operation steps that after heat preservation treatment of bimetal cylinder bodies, heated and molten according to a casting technology, of the hydraulic plunger pump and motor is finished, a steel base body and a molten copper alloy are conveyed to a cooling area device, and when the temperature is reduced to 840-880 DEG C, a hardening and tempering medium and compressed air are introduced into spline parts at the same time for cooling and hardening and tempering, wherein the hardening and tempering time is 5-10 min; the spline parts are conveyed to a designated position for air-cooling to normal temperature and</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>CHEMISTRY</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjMsKwjAQRbNxIeo_jB8gWItCl1IUV4LgvqTJpA0kmSGPRf_e-vgAV5d7zuUuhX0UDGq0YQAZNGT0jPHdPOaRNBiKkNjZgAnIQG9nLh2oaUYaI_Sk7VeNk46yOKuAXQnD7Lh4_rx6yhTXYmGkS7j55Upsr5dne9shU4eJpcKAuWvvVXU4NvX-VJ3rfzYvXMtAzg</recordid><startdate>20210402</startdate><enddate>20210402</enddate><creator>YANG CHAOLIANG</creator><creator>ZHOU WEI</creator><creator>ZHOU BANGHUA</creator><scope>EVB</scope></search><sort><creationdate>20210402</creationdate><title>Quenching and tempering method for splines of bimetal cylinder bodies of hydraulic plunger pump and motor</title><author>YANG CHAOLIANG ; ZHOU WEI ; ZHOU BANGHUA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN112593061A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>CHEMISTRY</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>YANG CHAOLIANG</creatorcontrib><creatorcontrib>ZHOU WEI</creatorcontrib><creatorcontrib>ZHOU BANGHUA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YANG CHAOLIANG</au><au>ZHOU WEI</au><au>ZHOU BANGHUA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Quenching and tempering method for splines of bimetal cylinder bodies of hydraulic plunger pump and motor</title><date>2021-04-02</date><risdate>2021</risdate><abstract>The invention discloses a quenching and tempering method for splines of bimetal cylinder bodies of a hydraulic plunger pump and motor, and belongs to the technical field of machining. Residual heat isutilized to carry out hardening and tempering heat treatment in a bimetal casting process. Spline hardening and tempering are carried out in a cooling process. The method comprises the following specific operation steps that after heat preservation treatment of bimetal cylinder bodies, heated and molten according to a casting technology, of the hydraulic plunger pump and motor is finished, a steel base body and a molten copper alloy are conveyed to a cooling area device, and when the temperature is reduced to 840-880 DEG C, a hardening and tempering medium and compressed air are introduced into spline parts at the same time for cooling and hardening and tempering, wherein the hardening and tempering time is 5-10 min; the spline parts are conveyed to a designated position for air-cooling to normal temperature and</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN112593061A |
source | esp@cenet |
subjects | CASTING CASTING OF METALS CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES CHEMISTRY GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS METALLURGY METALLURGY OF IRON MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS PERFORMING OPERATIONS POWDER METALLURGY TRANSPORTING |
title | Quenching and tempering method for splines of bimetal cylinder bodies of hydraulic plunger pump and motor |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T11%3A14%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YANG%20CHAOLIANG&rft.date=2021-04-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN112593061A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |