Method for preparing Ha, Bi and Ca co-doped potassium-sodium niobate leadless piezoelectric ceramic by solid-phase sintering method

The invention relates to a method for preparing Ha, Bi and Ca co-doped potassium sodium niobate leadless piezoelectric ceramic by a solid-phase sintering method, the molecule of the leadless piezoelectric ceramic is (1-x) K0. 5Na0. 5Nb0. 95Sb0. 05O3-x (Bi0. 5Ca0. 5) HfO3, and x is more than or equal...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANG CHEN, ZHENG ZHANSHEN, CHEN JIAQIAO, XI KAIBIAO, WANG DIDI, LI DONGSHENG, LI YUANLIANG, ZENG KANGYU
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YANG CHEN
ZHENG ZHANSHEN
CHEN JIAQIAO
XI KAIBIAO
WANG DIDI
LI DONGSHENG
LI YUANLIANG
ZENG KANGYU
description The invention relates to a method for preparing Ha, Bi and Ca co-doped potassium sodium niobate leadless piezoelectric ceramic by a solid-phase sintering method, the molecule of the leadless piezoelectric ceramic is (1-x) K0. 5Na0. 5Nb0. 95Sb0. 05O3-x (Bi0. 5Ca0. 5) HfO3, and x is more than or equal to 0 and less than or equal to 0.05; the 0.97 KNNS-0. 03BCH ceramic has the advantages of remarkable piezoelectric and ferroelectric properties, higher Curie temperature, optimal piezoelectric thermal stability and the like, and specifically comprises 3367% of epsilon r, 0.023% of tan delta, 41715%of epsilon rPr, 43.8% of kp, 478.6 pm/V of d * 33, 392 pC/N of d33 and better Curie temperature Tc of 295 DEG C, and good thermostability Delta d33/d33 is less than 6%, therefore, the method has bright market prospect and development potential. 本发明涉及一种固相烧结法制备Ha、Bi、Ca共掺杂铌酸钾钠无铅压电陶瓷的方法,所述无铅压电陶瓷的分子是(1-x)K0.5Na0.5Nb0.95Sb0.05O3-x(Bi0.5Ca0.5)HfO3,其中0≤x≤0.05;本发明0.97KNNS-0.03BCH陶瓷表现出显著的压电和铁电性能、较高的居里温度及最佳的压电热稳定性等优点,具体包括εr为3367、ta
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN112266246A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN112266246A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN112266246A3</originalsourceid><addsrcrecordid>eNqNzbEKwjAURuEuDqK-w3W3g1W6a1G66OQut8mvDaS5ITcOuvriSvEBnL7lwJkW7xNyL5ZukigmRE4u3KnlFe0dcbDUMBkprURYipJZ1T2GUsV-oeCk4wzyYOuhStHhJfAwOTlDBomHr92TVLyzZexZQepCxvgZxvm8mNzYKxY_Z8XyeLg0bYkoV2hkg4B8bc7rdVXVdbWtd5t_mg-c00nY</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing Ha, Bi and Ca co-doped potassium-sodium niobate leadless piezoelectric ceramic by solid-phase sintering method</title><source>esp@cenet</source><creator>YANG CHEN ; ZHENG ZHANSHEN ; CHEN JIAQIAO ; XI KAIBIAO ; WANG DIDI ; LI DONGSHENG ; LI YUANLIANG ; ZENG KANGYU</creator><creatorcontrib>YANG CHEN ; ZHENG ZHANSHEN ; CHEN JIAQIAO ; XI KAIBIAO ; WANG DIDI ; LI DONGSHENG ; LI YUANLIANG ; ZENG KANGYU</creatorcontrib><description>The invention relates to a method for preparing Ha, Bi and Ca co-doped potassium sodium niobate leadless piezoelectric ceramic by a solid-phase sintering method, the molecule of the leadless piezoelectric ceramic is (1-x) K0. 5Na0. 5Nb0. 95Sb0. 05O3-x (Bi0. 5Ca0. 5) HfO3, and x is more than or equal to 0 and less than or equal to 0.05; the 0.97 KNNS-0. 03BCH ceramic has the advantages of remarkable piezoelectric and ferroelectric properties, higher Curie temperature, optimal piezoelectric thermal stability and the like, and specifically comprises 3367% of epsilon r, 0.023% of tan delta, 41715%of epsilon rPr, 43.8% of kp, 478.6 pm/V of d * 33, 392 pC/N of d33 and better Curie temperature Tc of 295 DEG C, and good thermostability Delta d33/d33 is less than 6%, therefore, the method has bright market prospect and development potential. 本发明涉及一种固相烧结法制备Ha、Bi、Ca共掺杂铌酸钾钠无铅压电陶瓷的方法,所述无铅压电陶瓷的分子是(1-x)K0.5Na0.5Nb0.95Sb0.05O3-x(Bi0.5Ca0.5)HfO3,其中0≤x≤0.05;本发明0.97KNNS-0.03BCH陶瓷表现出显著的压电和铁电性能、较高的居里温度及最佳的压电热稳定性等优点,具体包括εr为3367、ta</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210126&amp;DB=EPODOC&amp;CC=CN&amp;NR=112266246A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210126&amp;DB=EPODOC&amp;CC=CN&amp;NR=112266246A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YANG CHEN</creatorcontrib><creatorcontrib>ZHENG ZHANSHEN</creatorcontrib><creatorcontrib>CHEN JIAQIAO</creatorcontrib><creatorcontrib>XI KAIBIAO</creatorcontrib><creatorcontrib>WANG DIDI</creatorcontrib><creatorcontrib>LI DONGSHENG</creatorcontrib><creatorcontrib>LI YUANLIANG</creatorcontrib><creatorcontrib>ZENG KANGYU</creatorcontrib><title>Method for preparing Ha, Bi and Ca co-doped potassium-sodium niobate leadless piezoelectric ceramic by solid-phase sintering method</title><description>The invention relates to a method for preparing Ha, Bi and Ca co-doped potassium sodium niobate leadless piezoelectric ceramic by a solid-phase sintering method, the molecule of the leadless piezoelectric ceramic is (1-x) K0. 5Na0. 5Nb0. 95Sb0. 05O3-x (Bi0. 5Ca0. 5) HfO3, and x is more than or equal to 0 and less than or equal to 0.05; the 0.97 KNNS-0. 03BCH ceramic has the advantages of remarkable piezoelectric and ferroelectric properties, higher Curie temperature, optimal piezoelectric thermal stability and the like, and specifically comprises 3367% of epsilon r, 0.023% of tan delta, 41715%of epsilon rPr, 43.8% of kp, 478.6 pm/V of d * 33, 392 pC/N of d33 and better Curie temperature Tc of 295 DEG C, and good thermostability Delta d33/d33 is less than 6%, therefore, the method has bright market prospect and development potential. 本发明涉及一种固相烧结法制备Ha、Bi、Ca共掺杂铌酸钾钠无铅压电陶瓷的方法,所述无铅压电陶瓷的分子是(1-x)K0.5Na0.5Nb0.95Sb0.05O3-x(Bi0.5Ca0.5)HfO3,其中0≤x≤0.05;本发明0.97KNNS-0.03BCH陶瓷表现出显著的压电和铁电性能、较高的居里温度及最佳的压电热稳定性等优点,具体包括εr为3367、ta</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNzbEKwjAURuEuDqK-w3W3g1W6a1G66OQut8mvDaS5ITcOuvriSvEBnL7lwJkW7xNyL5ZukigmRE4u3KnlFe0dcbDUMBkprURYipJZ1T2GUsV-oeCk4wzyYOuhStHhJfAwOTlDBomHr92TVLyzZexZQepCxvgZxvm8mNzYKxY_Z8XyeLg0bYkoV2hkg4B8bc7rdVXVdbWtd5t_mg-c00nY</recordid><startdate>20210126</startdate><enddate>20210126</enddate><creator>YANG CHEN</creator><creator>ZHENG ZHANSHEN</creator><creator>CHEN JIAQIAO</creator><creator>XI KAIBIAO</creator><creator>WANG DIDI</creator><creator>LI DONGSHENG</creator><creator>LI YUANLIANG</creator><creator>ZENG KANGYU</creator><scope>EVB</scope></search><sort><creationdate>20210126</creationdate><title>Method for preparing Ha, Bi and Ca co-doped potassium-sodium niobate leadless piezoelectric ceramic by solid-phase sintering method</title><author>YANG CHEN ; ZHENG ZHANSHEN ; CHEN JIAQIAO ; XI KAIBIAO ; WANG DIDI ; LI DONGSHENG ; LI YUANLIANG ; ZENG KANGYU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN112266246A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>YANG CHEN</creatorcontrib><creatorcontrib>ZHENG ZHANSHEN</creatorcontrib><creatorcontrib>CHEN JIAQIAO</creatorcontrib><creatorcontrib>XI KAIBIAO</creatorcontrib><creatorcontrib>WANG DIDI</creatorcontrib><creatorcontrib>LI DONGSHENG</creatorcontrib><creatorcontrib>LI YUANLIANG</creatorcontrib><creatorcontrib>ZENG KANGYU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YANG CHEN</au><au>ZHENG ZHANSHEN</au><au>CHEN JIAQIAO</au><au>XI KAIBIAO</au><au>WANG DIDI</au><au>LI DONGSHENG</au><au>LI YUANLIANG</au><au>ZENG KANGYU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing Ha, Bi and Ca co-doped potassium-sodium niobate leadless piezoelectric ceramic by solid-phase sintering method</title><date>2021-01-26</date><risdate>2021</risdate><abstract>The invention relates to a method for preparing Ha, Bi and Ca co-doped potassium sodium niobate leadless piezoelectric ceramic by a solid-phase sintering method, the molecule of the leadless piezoelectric ceramic is (1-x) K0. 5Na0. 5Nb0. 95Sb0. 05O3-x (Bi0. 5Ca0. 5) HfO3, and x is more than or equal to 0 and less than or equal to 0.05; the 0.97 KNNS-0. 03BCH ceramic has the advantages of remarkable piezoelectric and ferroelectric properties, higher Curie temperature, optimal piezoelectric thermal stability and the like, and specifically comprises 3367% of epsilon r, 0.023% of tan delta, 41715%of epsilon rPr, 43.8% of kp, 478.6 pm/V of d * 33, 392 pC/N of d33 and better Curie temperature Tc of 295 DEG C, and good thermostability Delta d33/d33 is less than 6%, therefore, the method has bright market prospect and development potential. 本发明涉及一种固相烧结法制备Ha、Bi、Ca共掺杂铌酸钾钠无铅压电陶瓷的方法,所述无铅压电陶瓷的分子是(1-x)K0.5Na0.5Nb0.95Sb0.05O3-x(Bi0.5Ca0.5)HfO3,其中0≤x≤0.05;本发明0.97KNNS-0.03BCH陶瓷表现出显著的压电和铁电性能、较高的居里温度及最佳的压电热稳定性等优点,具体包括εr为3367、ta</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN112266246A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Method for preparing Ha, Bi and Ca co-doped potassium-sodium niobate leadless piezoelectric ceramic by solid-phase sintering method
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-13T10%3A13%3A31IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YANG%20CHEN&rft.date=2021-01-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN112266246A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true