Solvent-free low-temperature ball-milling preparation method of solid polycarboxylic slump retaining agent

The invention relates to a solvent-free low-temperature ball-milling preparation method of a solid polycarboxylic slump retaining agent, which comprises the following steps: adding molten ethylene glycol vinyl polyoxyethylene ether, unsaturated carboxylic acid, acrylate, unsaturated amide and a chai...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHU YERAN, WEN JINBAO, DU ZHIQIN, TANG XIUSHENG, LU JIAN, CHEN GUOXIN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHU YERAN
WEN JINBAO
DU ZHIQIN
TANG XIUSHENG
LU JIAN
CHEN GUOXIN
description The invention relates to a solvent-free low-temperature ball-milling preparation method of a solid polycarboxylic slump retaining agent, which comprises the following steps: adding molten ethylene glycol vinyl polyoxyethylene ether, unsaturated carboxylic acid, acrylate, unsaturated amide and a chain transfer agent into a ball mill, closing a cover, opening an initiator feed valve, and adding halfof an initiator; opening a jacket chilled water valve of the ball mill while starting the ball mill for ball milling, and controlling the temperature to be 60+/-2 DEG C; adding the rest half of the initiator when ball milling is carried out for half of time, controlling the ball milling time to be 5-15 min, and after ball milling is finished, conveying a finished product to a cryogenic crusher through a discharging valve to crush and discharge the finished product. A solvent-free low-temperature ball milling method is adopted for bulk synthesis, the solid polycarboxylic acid slump retaining agent with the solid conte
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN112029049A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN112029049A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN112029049A3</originalsourceid><addsrcrecordid>eNqNjTEOwjAQBNNQIOAPxwMsJYEmJYpAVDTQRxfnEozOPst2gPyeIPEAqi1mRrvMHlfhJ7mk-kAELC-VyHoKmMZA0CKzsobZuAF8II8zMOLAUrpLB9JDFDYdeOFJY2jlPbHREHm0HgIlNO6b4jBfrLNFjxxp89tVtj0db_VZkZeGokdNjlJTX4qizMsq31eH3T_OBzHYQi8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Solvent-free low-temperature ball-milling preparation method of solid polycarboxylic slump retaining agent</title><source>esp@cenet</source><creator>ZHU YERAN ; WEN JINBAO ; DU ZHIQIN ; TANG XIUSHENG ; LU JIAN ; CHEN GUOXIN</creator><creatorcontrib>ZHU YERAN ; WEN JINBAO ; DU ZHIQIN ; TANG XIUSHENG ; LU JIAN ; CHEN GUOXIN</creatorcontrib><description>The invention relates to a solvent-free low-temperature ball-milling preparation method of a solid polycarboxylic slump retaining agent, which comprises the following steps: adding molten ethylene glycol vinyl polyoxyethylene ether, unsaturated carboxylic acid, acrylate, unsaturated amide and a chain transfer agent into a ball mill, closing a cover, opening an initiator feed valve, and adding halfof an initiator; opening a jacket chilled water valve of the ball mill while starting the ball mill for ball milling, and controlling the temperature to be 60+/-2 DEG C; adding the rest half of the initiator when ball milling is carried out for half of time, controlling the ball milling time to be 5-15 min, and after ball milling is finished, conveying a finished product to a cryogenic crusher through a discharging valve to crush and discharge the finished product. A solvent-free low-temperature ball milling method is adopted for bulk synthesis, the solid polycarboxylic acid slump retaining agent with the solid conte</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; REFRACTORIES ; SLAG ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TREATMENT OF NATURAL STONE</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201204&amp;DB=EPODOC&amp;CC=CN&amp;NR=112029049A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201204&amp;DB=EPODOC&amp;CC=CN&amp;NR=112029049A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHU YERAN</creatorcontrib><creatorcontrib>WEN JINBAO</creatorcontrib><creatorcontrib>DU ZHIQIN</creatorcontrib><creatorcontrib>TANG XIUSHENG</creatorcontrib><creatorcontrib>LU JIAN</creatorcontrib><creatorcontrib>CHEN GUOXIN</creatorcontrib><title>Solvent-free low-temperature ball-milling preparation method of solid polycarboxylic slump retaining agent</title><description>The invention relates to a solvent-free low-temperature ball-milling preparation method of a solid polycarboxylic slump retaining agent, which comprises the following steps: adding molten ethylene glycol vinyl polyoxyethylene ether, unsaturated carboxylic acid, acrylate, unsaturated amide and a chain transfer agent into a ball mill, closing a cover, opening an initiator feed valve, and adding halfof an initiator; opening a jacket chilled water valve of the ball mill while starting the ball mill for ball milling, and controlling the temperature to be 60+/-2 DEG C; adding the rest half of the initiator when ball milling is carried out for half of time, controlling the ball milling time to be 5-15 min, and after ball milling is finished, conveying a finished product to a cryogenic crusher through a discharging valve to crush and discharge the finished product. A solvent-free low-temperature ball milling method is adopted for bulk synthesis, the solid polycarboxylic acid slump retaining agent with the solid conte</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjTEOwjAQBNNQIOAPxwMsJYEmJYpAVDTQRxfnEozOPst2gPyeIPEAqi1mRrvMHlfhJ7mk-kAELC-VyHoKmMZA0CKzsobZuAF8II8zMOLAUrpLB9JDFDYdeOFJY2jlPbHREHm0HgIlNO6b4jBfrLNFjxxp89tVtj0db_VZkZeGokdNjlJTX4qizMsq31eH3T_OBzHYQi8</recordid><startdate>20201204</startdate><enddate>20201204</enddate><creator>ZHU YERAN</creator><creator>WEN JINBAO</creator><creator>DU ZHIQIN</creator><creator>TANG XIUSHENG</creator><creator>LU JIAN</creator><creator>CHEN GUOXIN</creator><scope>EVB</scope></search><sort><creationdate>20201204</creationdate><title>Solvent-free low-temperature ball-milling preparation method of solid polycarboxylic slump retaining agent</title><author>ZHU YERAN ; WEN JINBAO ; DU ZHIQIN ; TANG XIUSHENG ; LU JIAN ; CHEN GUOXIN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN112029049A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2020</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHU YERAN</creatorcontrib><creatorcontrib>WEN JINBAO</creatorcontrib><creatorcontrib>DU ZHIQIN</creatorcontrib><creatorcontrib>TANG XIUSHENG</creatorcontrib><creatorcontrib>LU JIAN</creatorcontrib><creatorcontrib>CHEN GUOXIN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHU YERAN</au><au>WEN JINBAO</au><au>DU ZHIQIN</au><au>TANG XIUSHENG</au><au>LU JIAN</au><au>CHEN GUOXIN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Solvent-free low-temperature ball-milling preparation method of solid polycarboxylic slump retaining agent</title><date>2020-12-04</date><risdate>2020</risdate><abstract>The invention relates to a solvent-free low-temperature ball-milling preparation method of a solid polycarboxylic slump retaining agent, which comprises the following steps: adding molten ethylene glycol vinyl polyoxyethylene ether, unsaturated carboxylic acid, acrylate, unsaturated amide and a chain transfer agent into a ball mill, closing a cover, opening an initiator feed valve, and adding halfof an initiator; opening a jacket chilled water valve of the ball mill while starting the ball mill for ball milling, and controlling the temperature to be 60+/-2 DEG C; adding the rest half of the initiator when ball milling is carried out for half of time, controlling the ball milling time to be 5-15 min, and after ball milling is finished, conveying a finished product to a cryogenic crusher through a discharging valve to crush and discharge the finished product. A solvent-free low-temperature ball milling method is adopted for bulk synthesis, the solid polycarboxylic acid slump retaining agent with the solid conte</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN112029049A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
REFRACTORIES
SLAG
THEIR PREPARATION OR CHEMICAL WORKING-UP
TREATMENT OF NATURAL STONE
title Solvent-free low-temperature ball-milling preparation method of solid polycarboxylic slump retaining agent
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T19%3A16%3A08IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHU%20YERAN&rft.date=2020-12-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN112029049A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true