Preparation method of C40 inorganic coating anti-freezing concrete and surface spraying process of C40 inorganic coating anti-freezing concrete

The invention discloses a preparation method of C40 inorganic coating anti-freezing concrete and a surface spraying process of the C40 inorganic coating anti-freezing concrete, and belongs to the technical field of concrete. The method comprises the following steps: pre-homogenizing sand and the sto...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG LANMIN, ZHU ZHAOXIA, NIU FUHANG, WANG PING, XU SHIYANG, WANG HUIJUAN, ZHENG HAIZHONG, YAN WUJIAN, GUO HAITAO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG LANMIN
ZHU ZHAOXIA
NIU FUHANG
WANG PING
XU SHIYANG
WANG HUIJUAN
ZHENG HAIZHONG
YAN WUJIAN
GUO HAITAO
description The invention discloses a preparation method of C40 inorganic coating anti-freezing concrete and a surface spraying process of the C40 inorganic coating anti-freezing concrete, and belongs to the technical field of concrete. The method comprises the following steps: pre-homogenizing sand and the stones in respective raw material bins; stirring the pre-homogenized sand and stones in a forced stirrer for 2 minutes; adding the cement and the water reducing agent into a forced stirrer, stirring for 5 minutes, adding the additive and the water, stirring for 2 minutes, and solidifying to obtain a concrete test piece; and maintaining the concrete test piece for 28 days, and spraying a coating to obtain the C40 inorganic coating anti-freezing concrete. The weight part ratio of the cement to the sand to the stones to the admixture to the water is (400-450): (750-800): (950-1000): (4-5): (150-200). The anti-freezing agent is simple in formula, good in anti-freezing durability and suitable for various engineering projec
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN112028561A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN112028561A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN112028561A3</originalsourceid><addsrcrecordid>eNqVjb0KwkAQhK-xEPUd1gcIJPEHWwmKlVjYh-Wylxzo7rF3FvoSvrIX8AG0Gma-YWZq3helgIrJC8Od0iAdiINmXYJn0R7ZW7CSOfeAnHzhlOg1OitslRLluIP4UIeWIAbF50iDiqUY_x2bm4nDW6TFV2dmeTxcm1NBQVqKIX8wpbY5V1Vd1rvNttqvful8AM-STlo</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of C40 inorganic coating anti-freezing concrete and surface spraying process of C40 inorganic coating anti-freezing concrete</title><source>esp@cenet</source><creator>WANG LANMIN ; ZHU ZHAOXIA ; NIU FUHANG ; WANG PING ; XU SHIYANG ; WANG HUIJUAN ; ZHENG HAIZHONG ; YAN WUJIAN ; GUO HAITAO</creator><creatorcontrib>WANG LANMIN ; ZHU ZHAOXIA ; NIU FUHANG ; WANG PING ; XU SHIYANG ; WANG HUIJUAN ; ZHENG HAIZHONG ; YAN WUJIAN ; GUO HAITAO</creatorcontrib><description>The invention discloses a preparation method of C40 inorganic coating anti-freezing concrete and a surface spraying process of the C40 inorganic coating anti-freezing concrete, and belongs to the technical field of concrete. The method comprises the following steps: pre-homogenizing sand and the stones in respective raw material bins; stirring the pre-homogenized sand and stones in a forced stirrer for 2 minutes; adding the cement and the water reducing agent into a forced stirrer, stirring for 5 minutes, adding the additive and the water, stirring for 2 minutes, and solidifying to obtain a concrete test piece; and maintaining the concrete test piece for 28 days, and spraying a coating to obtain the C40 inorganic coating anti-freezing concrete. The weight part ratio of the cement to the sand to the stones to the admixture to the water is (400-450): (750-800): (950-1000): (4-5): (150-200). The anti-freezing agent is simple in formula, good in anti-freezing durability and suitable for various engineering projec</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201204&amp;DB=EPODOC&amp;CC=CN&amp;NR=112028561A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201204&amp;DB=EPODOC&amp;CC=CN&amp;NR=112028561A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG LANMIN</creatorcontrib><creatorcontrib>ZHU ZHAOXIA</creatorcontrib><creatorcontrib>NIU FUHANG</creatorcontrib><creatorcontrib>WANG PING</creatorcontrib><creatorcontrib>XU SHIYANG</creatorcontrib><creatorcontrib>WANG HUIJUAN</creatorcontrib><creatorcontrib>ZHENG HAIZHONG</creatorcontrib><creatorcontrib>YAN WUJIAN</creatorcontrib><creatorcontrib>GUO HAITAO</creatorcontrib><title>Preparation method of C40 inorganic coating anti-freezing concrete and surface spraying process of C40 inorganic coating anti-freezing concrete</title><description>The invention discloses a preparation method of C40 inorganic coating anti-freezing concrete and a surface spraying process of the C40 inorganic coating anti-freezing concrete, and belongs to the technical field of concrete. The method comprises the following steps: pre-homogenizing sand and the stones in respective raw material bins; stirring the pre-homogenized sand and stones in a forced stirrer for 2 minutes; adding the cement and the water reducing agent into a forced stirrer, stirring for 5 minutes, adding the additive and the water, stirring for 2 minutes, and solidifying to obtain a concrete test piece; and maintaining the concrete test piece for 28 days, and spraying a coating to obtain the C40 inorganic coating anti-freezing concrete. The weight part ratio of the cement to the sand to the stones to the admixture to the water is (400-450): (750-800): (950-1000): (4-5): (150-200). The anti-freezing agent is simple in formula, good in anti-freezing durability and suitable for various engineering projec</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqVjb0KwkAQhK-xEPUd1gcIJPEHWwmKlVjYh-Wylxzo7rF3FvoSvrIX8AG0Gma-YWZq3helgIrJC8Od0iAdiINmXYJn0R7ZW7CSOfeAnHzhlOg1OitslRLluIP4UIeWIAbF50iDiqUY_x2bm4nDW6TFV2dmeTxcm1NBQVqKIX8wpbY5V1Vd1rvNttqvful8AM-STlo</recordid><startdate>20201204</startdate><enddate>20201204</enddate><creator>WANG LANMIN</creator><creator>ZHU ZHAOXIA</creator><creator>NIU FUHANG</creator><creator>WANG PING</creator><creator>XU SHIYANG</creator><creator>WANG HUIJUAN</creator><creator>ZHENG HAIZHONG</creator><creator>YAN WUJIAN</creator><creator>GUO HAITAO</creator><scope>EVB</scope></search><sort><creationdate>20201204</creationdate><title>Preparation method of C40 inorganic coating anti-freezing concrete and surface spraying process of C40 inorganic coating anti-freezing concrete</title><author>WANG LANMIN ; ZHU ZHAOXIA ; NIU FUHANG ; WANG PING ; XU SHIYANG ; WANG HUIJUAN ; ZHENG HAIZHONG ; YAN WUJIAN ; GUO HAITAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN112028561A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2020</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG LANMIN</creatorcontrib><creatorcontrib>ZHU ZHAOXIA</creatorcontrib><creatorcontrib>NIU FUHANG</creatorcontrib><creatorcontrib>WANG PING</creatorcontrib><creatorcontrib>XU SHIYANG</creatorcontrib><creatorcontrib>WANG HUIJUAN</creatorcontrib><creatorcontrib>ZHENG HAIZHONG</creatorcontrib><creatorcontrib>YAN WUJIAN</creatorcontrib><creatorcontrib>GUO HAITAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG LANMIN</au><au>ZHU ZHAOXIA</au><au>NIU FUHANG</au><au>WANG PING</au><au>XU SHIYANG</au><au>WANG HUIJUAN</au><au>ZHENG HAIZHONG</au><au>YAN WUJIAN</au><au>GUO HAITAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of C40 inorganic coating anti-freezing concrete and surface spraying process of C40 inorganic coating anti-freezing concrete</title><date>2020-12-04</date><risdate>2020</risdate><abstract>The invention discloses a preparation method of C40 inorganic coating anti-freezing concrete and a surface spraying process of the C40 inorganic coating anti-freezing concrete, and belongs to the technical field of concrete. The method comprises the following steps: pre-homogenizing sand and the stones in respective raw material bins; stirring the pre-homogenized sand and stones in a forced stirrer for 2 minutes; adding the cement and the water reducing agent into a forced stirrer, stirring for 5 minutes, adding the additive and the water, stirring for 2 minutes, and solidifying to obtain a concrete test piece; and maintaining the concrete test piece for 28 days, and spraying a coating to obtain the C40 inorganic coating anti-freezing concrete. The weight part ratio of the cement to the sand to the stones to the admixture to the water is (400-450): (750-800): (950-1000): (4-5): (150-200). The anti-freezing agent is simple in formula, good in anti-freezing durability and suitable for various engineering projec</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN112028561A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Preparation method of C40 inorganic coating anti-freezing concrete and surface spraying process of C40 inorganic coating anti-freezing concrete
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-20T04%3A33%3A10IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20LANMIN&rft.date=2020-12-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN112028561A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true