Sodium yttrium tungstate film material as well as preparation method and application thereof

The invention belongs to the technical field of the preparation of inorganic photoelectric functional materials, and discloses a sodium yttrium tungstate film material as well as a preparation methodand application thereof. According to the invention, FTO conductive glass is used as a substrate, a t...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LI XUJIAO, LIANG GONGYING, TANG LIYONG, LI YANMEI, GUO KUNFENG, NAN ZONGLIANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LI XUJIAO
LIANG GONGYING
TANG LIYONG
LI YANMEI
GUO KUNFENG
NAN ZONGLIANG
description The invention belongs to the technical field of the preparation of inorganic photoelectric functional materials, and discloses a sodium yttrium tungstate film material as well as a preparation methodand application thereof. According to the invention, FTO conductive glass is used as a substrate, a tetragonal NaY(WO4)2 film material is prepared by using a layer-by-layer dip-coating method for alternate coating, and the density and crystal growth orientation of the film are effectively improved by the alternate coating of a surfactant and a precursor film layer. The sintering temperature of theprocess ranges from 350 DEG C to 550 DEG C, a good energy-saving effect is achieved, production energy consumption and production cost can be remarkably and greatly reduced, and the application fieldof the film is expanded. 本发明属于无机光电功能材料制备技术领域,公开了一种钨酸钇钠薄膜材料及其制备方法和应用。本发明以FTO导电玻璃为基底,利用层层浸渍提拉法交替镀膜制备了一种四方晶系的NaY(WO4)2薄膜材料,通过表面活性剂与前驱体膜层交替镀膜有效改善膜的致密度及晶体生长取向。本发明工艺烧结温度在350~550°之间,具有较好的节能效果,可以显著、大幅度降低生产能耗和生产成本、拓展薄膜的应用领域。
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN111864023A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN111864023A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN111864023A3</originalsourceid><addsrcrecordid>eNrjZIgJzk_JLM1VqCwpKQLRJaV56cUliSWpCmmZObkKuUBWUWZijkJisUJ5ag6YLihKLUgsSizJzM9TyE0tychPUUjMA-KCgpzMZIhwSUZqUWp-Gg8Da1piTnEqL5TmZlB0cw1x9tBNLciPTy0uSExOzUstiXf2MzQ0tDAzMTAydjQmRg0AAMM8Ug</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Sodium yttrium tungstate film material as well as preparation method and application thereof</title><source>esp@cenet</source><creator>LI XUJIAO ; LIANG GONGYING ; TANG LIYONG ; LI YANMEI ; GUO KUNFENG ; NAN ZONGLIANG</creator><creatorcontrib>LI XUJIAO ; LIANG GONGYING ; TANG LIYONG ; LI YANMEI ; GUO KUNFENG ; NAN ZONGLIANG</creatorcontrib><description>The invention belongs to the technical field of the preparation of inorganic photoelectric functional materials, and discloses a sodium yttrium tungstate film material as well as a preparation methodand application thereof. According to the invention, FTO conductive glass is used as a substrate, a tetragonal NaY(WO4)2 film material is prepared by using a layer-by-layer dip-coating method for alternate coating, and the density and crystal growth orientation of the film are effectively improved by the alternate coating of a surfactant and a precursor film layer. The sintering temperature of theprocess ranges from 350 DEG C to 550 DEG C, a good energy-saving effect is achieved, production energy consumption and production cost can be remarkably and greatly reduced, and the application fieldof the film is expanded. 本发明属于无机光电功能材料制备技术领域,公开了一种钨酸钇钠薄膜材料及其制备方法和应用。本发明以FTO导电玻璃为基底,利用层层浸渍提拉法交替镀膜制备了一种四方晶系的NaY(WO4)2薄膜材料,通过表面活性剂与前驱体膜层交替镀膜有效改善膜的致密度及晶体生长取向。本发明工艺烧结温度在350~550°之间,具有较好的节能效果,可以显著、大幅度降低生产能耗和生产成本、拓展薄膜的应用领域。</description><language>chi ; eng</language><subject>ADHESIVES ; BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; DEVICES USING STIMULATED EMISSION ; DYES ; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR ; ELECTRICITY ; MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; PAINTS ; POLISHES ; SEMICONDUCTOR DEVICES</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201030&amp;DB=EPODOC&amp;CC=CN&amp;NR=111864023A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201030&amp;DB=EPODOC&amp;CC=CN&amp;NR=111864023A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LI XUJIAO</creatorcontrib><creatorcontrib>LIANG GONGYING</creatorcontrib><creatorcontrib>TANG LIYONG</creatorcontrib><creatorcontrib>LI YANMEI</creatorcontrib><creatorcontrib>GUO KUNFENG</creatorcontrib><creatorcontrib>NAN ZONGLIANG</creatorcontrib><title>Sodium yttrium tungstate film material as well as preparation method and application thereof</title><description>The invention belongs to the technical field of the preparation of inorganic photoelectric functional materials, and discloses a sodium yttrium tungstate film material as well as a preparation methodand application thereof. According to the invention, FTO conductive glass is used as a substrate, a tetragonal NaY(WO4)2 film material is prepared by using a layer-by-layer dip-coating method for alternate coating, and the density and crystal growth orientation of the film are effectively improved by the alternate coating of a surfactant and a precursor film layer. The sintering temperature of theprocess ranges from 350 DEG C to 550 DEG C, a good energy-saving effect is achieved, production energy consumption and production cost can be remarkably and greatly reduced, and the application fieldof the film is expanded. 本发明属于无机光电功能材料制备技术领域,公开了一种钨酸钇钠薄膜材料及其制备方法和应用。本发明以FTO导电玻璃为基底,利用层层浸渍提拉法交替镀膜制备了一种四方晶系的NaY(WO4)2薄膜材料,通过表面活性剂与前驱体膜层交替镀膜有效改善膜的致密度及晶体生长取向。本发明工艺烧结温度在350~550°之间,具有较好的节能效果,可以显著、大幅度降低生产能耗和生产成本、拓展薄膜的应用领域。</description><subject>ADHESIVES</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>DEVICES USING STIMULATED EMISSION</subject><subject>DYES</subject><subject>ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR</subject><subject>ELECTRICITY</subject><subject>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>SEMICONDUCTOR DEVICES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZIgJzk_JLM1VqCwpKQLRJaV56cUliSWpCmmZObkKuUBWUWZijkJisUJ5ag6YLihKLUgsSizJzM9TyE0tychPUUjMA-KCgpzMZIhwSUZqUWp-Gg8Da1piTnEqL5TmZlB0cw1x9tBNLciPTy0uSExOzUstiXf2MzQ0tDAzMTAydjQmRg0AAMM8Ug</recordid><startdate>20201030</startdate><enddate>20201030</enddate><creator>LI XUJIAO</creator><creator>LIANG GONGYING</creator><creator>TANG LIYONG</creator><creator>LI YANMEI</creator><creator>GUO KUNFENG</creator><creator>NAN ZONGLIANG</creator><scope>EVB</scope></search><sort><creationdate>20201030</creationdate><title>Sodium yttrium tungstate film material as well as preparation method and application thereof</title><author>LI XUJIAO ; LIANG GONGYING ; TANG LIYONG ; LI YANMEI ; GUO KUNFENG ; NAN ZONGLIANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN111864023A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2020</creationdate><topic>ADHESIVES</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>DEVICES USING STIMULATED EMISSION</topic><topic>DYES</topic><topic>ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR</topic><topic>ELECTRICITY</topic><topic>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>SEMICONDUCTOR DEVICES</topic><toplevel>online_resources</toplevel><creatorcontrib>LI XUJIAO</creatorcontrib><creatorcontrib>LIANG GONGYING</creatorcontrib><creatorcontrib>TANG LIYONG</creatorcontrib><creatorcontrib>LI YANMEI</creatorcontrib><creatorcontrib>GUO KUNFENG</creatorcontrib><creatorcontrib>NAN ZONGLIANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LI XUJIAO</au><au>LIANG GONGYING</au><au>TANG LIYONG</au><au>LI YANMEI</au><au>GUO KUNFENG</au><au>NAN ZONGLIANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Sodium yttrium tungstate film material as well as preparation method and application thereof</title><date>2020-10-30</date><risdate>2020</risdate><abstract>The invention belongs to the technical field of the preparation of inorganic photoelectric functional materials, and discloses a sodium yttrium tungstate film material as well as a preparation methodand application thereof. According to the invention, FTO conductive glass is used as a substrate, a tetragonal NaY(WO4)2 film material is prepared by using a layer-by-layer dip-coating method for alternate coating, and the density and crystal growth orientation of the film are effectively improved by the alternate coating of a surfactant and a precursor film layer. The sintering temperature of theprocess ranges from 350 DEG C to 550 DEG C, a good energy-saving effect is achieved, production energy consumption and production cost can be remarkably and greatly reduced, and the application fieldof the film is expanded. 本发明属于无机光电功能材料制备技术领域,公开了一种钨酸钇钠薄膜材料及其制备方法和应用。本发明以FTO导电玻璃为基底,利用层层浸渍提拉法交替镀膜制备了一种四方晶系的NaY(WO4)2薄膜材料,通过表面活性剂与前驱体膜层交替镀膜有效改善膜的致密度及晶体生长取向。本发明工艺烧结温度在350~550°之间,具有较好的节能效果,可以显著、大幅度降低生产能耗和生产成本、拓展薄膜的应用领域。</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN111864023A
source esp@cenet
subjects ADHESIVES
BASIC ELECTRIC ELEMENTS
CHEMISTRY
DEVICES USING STIMULATED EMISSION
DYES
ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
ELECTRICITY
MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
PAINTS
POLISHES
SEMICONDUCTOR DEVICES
title Sodium yttrium tungstate film material as well as preparation method and application thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-09T04%3A20%3A38IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LI%20XUJIAO&rft.date=2020-10-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN111864023A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true