Method for preparing battery positive electrode material by leaching waste lithium batteries with sulfur dioxide gas

The invention discloses a method for preparing a battery positive electrode material by leaching waste lithium batteries with sulfur dioxide gas. The method comprises the steps: carrying out dischargedisassembly, sorting and grinding on the waste lithium batteries to obtain a positive electrode mixe...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: XU FEN, LIAO BING, DENG XUYING, YU YAHUI, LIU JING
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator XU FEN
LIAO BING
DENG XUYING
YU YAHUI
LIU JING
description The invention discloses a method for preparing a battery positive electrode material by leaching waste lithium batteries with sulfur dioxide gas. The method comprises the steps: carrying out dischargedisassembly, sorting and grinding on the waste lithium batteries to obtain a positive electrode mixed material, preparing a slurry from the positive electrode mixed material and water, feeding the slurry, sulfur dioxide and air mixed gas into a reactor, and adjusting the molar ratio of Li to Co to Ni to Mn in the obtained leachate by adding a proper amount of metal ion salt; and adding a mixed solution of citric acid and polyethylene glycol, adjusting the pH value of the solution, controlling the temperature of the solution to be 70-85 DEG C, continuously stirring to obtain gel, drying the gel, calcining, and uniformly grinding to obtain the ternary lithium battery positive electrode material. According to the method, the four metals of lithium, cobalt, nickel and manganesein the waste lithium batt
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN111807423A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN111807423A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN111807423A3</originalsourceid><addsrcrecordid>eNqNjDEOgkAURGksjHqH7wFMREy0NURjo5U9-cAAP1nYze5H5PZiwgGsJnnzZpaRPqCNLamynpyHYy9dTTmrwo_kbBCVNwgGhXpbglqeGmFD-UgGXDQ_f-CgICPaSN_Oa0GgYSIUelP1nkqxH5kOag7raFGxCdjMuYq2t-srve_gbIbguEAHzdJnHMfn_el4SC7JP84X-LxFjA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing battery positive electrode material by leaching waste lithium batteries with sulfur dioxide gas</title><source>esp@cenet</source><creator>XU FEN ; LIAO BING ; DENG XUYING ; YU YAHUI ; LIU JING</creator><creatorcontrib>XU FEN ; LIAO BING ; DENG XUYING ; YU YAHUI ; LIU JING</creatorcontrib><description>The invention discloses a method for preparing a battery positive electrode material by leaching waste lithium batteries with sulfur dioxide gas. The method comprises the steps: carrying out dischargedisassembly, sorting and grinding on the waste lithium batteries to obtain a positive electrode mixed material, preparing a slurry from the positive electrode mixed material and water, feeding the slurry, sulfur dioxide and air mixed gas into a reactor, and adjusting the molar ratio of Li&lt;+&gt; to Co&lt;2+&gt; to Ni&lt;2+&gt; to Mn&lt;2+&gt; in the obtained leachate by adding a proper amount of metal ion salt; and adding a mixed solution of citric acid and polyethylene glycol, adjusting the pH value of the solution, controlling the temperature of the solution to be 70-85 DEG C, continuously stirring to obtain gel, drying the gel, calcining, and uniformly grinding to obtain the ternary lithium battery positive electrode material. According to the method, the four metals of lithium, cobalt, nickel and manganesein the waste lithium batt</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; ELECTRICITY ; INORGANIC CHEMISTRY ; METALLURGY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201023&amp;DB=EPODOC&amp;CC=CN&amp;NR=111807423A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201023&amp;DB=EPODOC&amp;CC=CN&amp;NR=111807423A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>XU FEN</creatorcontrib><creatorcontrib>LIAO BING</creatorcontrib><creatorcontrib>DENG XUYING</creatorcontrib><creatorcontrib>YU YAHUI</creatorcontrib><creatorcontrib>LIU JING</creatorcontrib><title>Method for preparing battery positive electrode material by leaching waste lithium batteries with sulfur dioxide gas</title><description>The invention discloses a method for preparing a battery positive electrode material by leaching waste lithium batteries with sulfur dioxide gas. The method comprises the steps: carrying out dischargedisassembly, sorting and grinding on the waste lithium batteries to obtain a positive electrode mixed material, preparing a slurry from the positive electrode mixed material and water, feeding the slurry, sulfur dioxide and air mixed gas into a reactor, and adjusting the molar ratio of Li&lt;+&gt; to Co&lt;2+&gt; to Ni&lt;2+&gt; to Mn&lt;2+&gt; in the obtained leachate by adding a proper amount of metal ion salt; and adding a mixed solution of citric acid and polyethylene glycol, adjusting the pH value of the solution, controlling the temperature of the solution to be 70-85 DEG C, continuously stirring to obtain gel, drying the gel, calcining, and uniformly grinding to obtain the ternary lithium battery positive electrode material. According to the method, the four metals of lithium, cobalt, nickel and manganesein the waste lithium batt</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>ELECTRICITY</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjDEOgkAURGksjHqH7wFMREy0NURjo5U9-cAAP1nYze5H5PZiwgGsJnnzZpaRPqCNLamynpyHYy9dTTmrwo_kbBCVNwgGhXpbglqeGmFD-UgGXDQ_f-CgICPaSN_Oa0GgYSIUelP1nkqxH5kOag7raFGxCdjMuYq2t-srve_gbIbguEAHzdJnHMfn_el4SC7JP84X-LxFjA</recordid><startdate>20201023</startdate><enddate>20201023</enddate><creator>XU FEN</creator><creator>LIAO BING</creator><creator>DENG XUYING</creator><creator>YU YAHUI</creator><creator>LIU JING</creator><scope>EVB</scope></search><sort><creationdate>20201023</creationdate><title>Method for preparing battery positive electrode material by leaching waste lithium batteries with sulfur dioxide gas</title><author>XU FEN ; LIAO BING ; DENG XUYING ; YU YAHUI ; LIU JING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN111807423A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2020</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>ELECTRICITY</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>XU FEN</creatorcontrib><creatorcontrib>LIAO BING</creatorcontrib><creatorcontrib>DENG XUYING</creatorcontrib><creatorcontrib>YU YAHUI</creatorcontrib><creatorcontrib>LIU JING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>XU FEN</au><au>LIAO BING</au><au>DENG XUYING</au><au>YU YAHUI</au><au>LIU JING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing battery positive electrode material by leaching waste lithium batteries with sulfur dioxide gas</title><date>2020-10-23</date><risdate>2020</risdate><abstract>The invention discloses a method for preparing a battery positive electrode material by leaching waste lithium batteries with sulfur dioxide gas. The method comprises the steps: carrying out dischargedisassembly, sorting and grinding on the waste lithium batteries to obtain a positive electrode mixed material, preparing a slurry from the positive electrode mixed material and water, feeding the slurry, sulfur dioxide and air mixed gas into a reactor, and adjusting the molar ratio of Li&lt;+&gt; to Co&lt;2+&gt; to Ni&lt;2+&gt; to Mn&lt;2+&gt; in the obtained leachate by adding a proper amount of metal ion salt; and adding a mixed solution of citric acid and polyethylene glycol, adjusting the pH value of the solution, controlling the temperature of the solution to be 70-85 DEG C, continuously stirring to obtain gel, drying the gel, calcining, and uniformly grinding to obtain the ternary lithium battery positive electrode material. According to the method, the four metals of lithium, cobalt, nickel and manganesein the waste lithium batt</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN111807423A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
ELECTRICITY
INORGANIC CHEMISTRY
METALLURGY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title Method for preparing battery positive electrode material by leaching waste lithium batteries with sulfur dioxide gas
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-20T00%3A19%3A12IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=XU%20FEN&rft.date=2020-10-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN111807423A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true